Method for depositing aluminum on a permanent Nd—Fe—B magnet
Abstract:
The present invention provides a method for depositing aluminum on a permanent Nd—Fe—B magnet including a step of cooling the chamber and the arc source by feeding a fluid of water at a cooling temperature of between 0° C. and 5° C. through the chamber and the arc source. The method also includes a step of adjusting a target source and a control magnet of the arc source in the chamber of the multi-arc ion plating apparatus to define a predetermined distance of between 1 cm and 10 cm. The step of depositing the film of aluminum further including steps of applying a current of between 50 A and 70 A and an electrical potential of between 100V and 200V to the target source of aluminum and directing the ions of aluminum using the arc source to the purified permanent Nd—Fe—B magnet for a time period of between 0.5 hours and 5 hours.