Method for producing a low alloy steel for oil country tubular goods having excellent sulfide stress cracking resistance
Abstract:
The low alloy steel for oil country tubular goods according to the present invention has a chemical composition containing, by mass percent, C: 0.56 to 1.00%, Si: 0.05 to 0.50%, Mn: 0.05 to 1.00%, P: at most 0.025%, S: at most 0.010%, Al: 0.005 to 0.100%, Mo: 0.40 to 1.00%, V: 0.05 to 0.30%, and O: at most 0.010%, the balance being Fe and impurities, wherein the yield stress thereof is at least 862 MPa, and the half-value width of a [211] crystal surface obtained by X-ray diffraction is at most 0.50°.