Method of manufacturing negative electrode for nonaqueous electrolyte secondary battery
Abstract:
A method of manufacturing a negative electrode for a nonaqueous electrolyte secondary battery includes: preparing a copper foil having a first main surface and a second main surface that are opposite sides of the copper foil; obtaining a granulated body by mixing a negative electrode active material, a thickener, a binder, and a solvent with each other to obtain a mixture and by granulating the mixture; obtaining a first negative electrode mixture layer by pressing the granulated body; arranging the first negative electrode mixture layer on the first main surface; and softening the copper foil by bringing the second main surface into contact with a heated roller in a state where the first negative electrode mixture layer is arranged on the first main surface. A temperature of the heated roller is a recrystallization temperature of the copper foil or higher.