Invention Grant
- Patent Title: Cerium-zirconium-based composite oxide and method for producing same
-
Application No.: US15125430Application Date: 2014-04-25
-
Publication No.: US09962684B2Publication Date: 2018-05-08
- Inventor: Hiroyuki Hayashida , Akiko Tatsumi
- Applicant: DAIICHI KIGENSO KAGAKU KOGYO CO., LTD.
- Applicant Address: JP Osaka
- Assignee: DAIICHI KIGENSO KAGAKU KOGYO CO., LTD.
- Current Assignee: DAIICHI KIGENSO KAGAKU KOGYO CO., LTD.
- Current Assignee Address: JP Osaka
- Agency: Westerman, Hattori, Daniels & Adrian, LLP
- Priority: JP2014-062327 20140325; JP2014-062334 20140325
- International Application: PCT/JP2014/061662 WO 20140425
- International Announcement: WO2015/145788 WO 20151001
- Main IPC: B01J21/06
- IPC: B01J21/06 ; B01J23/02 ; B01J23/04 ; B01J23/10 ; B01J23/34 ; B01J23/72 ; B01J23/745 ; B01J23/75 ; B01J23/755 ; B01J23/83 ; B01J37/08 ; B01J37/00 ; C01G25/00 ; C01G45/12 ; C01G49/00 ; C01G51/00 ; C01G53/00 ; C04B35/486 ; C04B35/50 ; C04B35/653 ; C01G45/00

Abstract:
Provided is a cerium-zirconium-based composite oxide having an excellent OSC, high catalytic activity, and excellent heat resistance, and also provided is a method for producing the same. The cerium-zirconium-based composite oxide comprises cerium, zirconium, and a third element other than these elements. The third element is (a) a transition metal element or (b) at least one or more elements selected from the group consisting of rare earth elements and alkaline earth metal elements. After a heat treatment at 1,000° C. to 1,100° C. for 3 hours, (1) the composite oxide has a crystal structure containing a pyrochlore phase, (2) a value of {I111/(I111+I222)}×100 is 1 or more, and (3) the composite oxide has an oxygen storage capacity at 600° C. of 0.05 mmol/g or more, and an oxygen storage capacity at 750° C. of 0.3 mmol/g or more.