Invention Grant
- Patent Title: Scandium recovery method
-
Application No.: US15115030Application Date: 2015-01-21
-
Publication No.: US09963762B2Publication Date: 2018-05-08
- Inventor: Tatsuya Higaki , Yoshitomo Ozaki , Shin-ya Matsumoto , Itsumi Matsuoka , Hidemasa Nagai , Toshihiko Nagakura , Keiji Kudo
- Applicant: SUMITOMO METAL MINING CO., LTD.
- Applicant Address: JP Tokyo
- Assignee: SUMITOMO METAL MINING CO., LTD.
- Current Assignee: SUMITOMO METAL MINING CO., LTD.
- Current Assignee Address: JP Tokyo
- Agency: Locke Lord LLP
- Priority: JP2014-016901 20140131; JP2014-065879 20140327
- International Application: PCT/JP2015/051501 WO 20150121
- International Announcement: WO2015/115269 WO 20150608
- Main IPC: C22B59/00
- IPC: C22B59/00 ; C22B3/44 ; C22B3/26 ; C22B3/08 ; C22B3/42 ; C22B21/00 ; C22B34/32

Abstract:
In order to recover high-quality scandium from nickel oxide ores efficiently, this method comprises: a step (S1) for feeding Ni oxide ores and sulfuric acid into a pressure vessel, and subjecting the mixture to solid-liquid separation to form a leachate and a leach residue; a step (S2) for adding a neutralizing agent to the leachate, and thus forming a neutralization sediment and a post-neutralization fluid; a step (S3) for adding a sulfurizing agent to the post-neutralization fluid, and separating the obtained mixture into Ni sulfide and a post-sulfurization fluid; a step (S4) for bringing the post-sulfurization fluid into contact with a chelating resin, making Sc adsorbed on the chelating resin, and forming an Sc eluent; a step (S6) for bringing the Sc eluent into contact with an extracting agent, adding a back-extraction agent to the extract, and forming back-extracted matter; and a step (S8) for roasting the back-extracted matter, and forming Sc oxide.
Public/Granted literature
- US20160340757A1 SCANDIUM RECOVERY METHOD Public/Granted day:2016-11-24
Information query