Manufacturing method for non-aqueous secondary battery
Abstract:
A manufacturing method for a non-aqueous secondary battery includes the following steps. (a) Preparing an electrode body including a positive electrode having a positive electrode active material layer and a negative electrode having a negative electrode active material layer. (b) Constructing a battery assembly using the electrode body and a non-aqueous electrolyte. (c) Initially charging the battery assembly. (d) Aging the battery assembly at a temperature of 60° C. or higher. (e) Forcibly starting to discharge the battery assembly in said temperature region after lowering the temperature of the battery assembly down to a temperature region of 35° C. or higher and 55° C. or lower. (f) Adjusting the SOC of the battery assembly. (g) Measuring a voltage drop amount by self-discharging the battery assembly. And (h) determining whether or not the battery assembly is qualified based on the voltage drop amount.