Propylene copolymer for blow molded articles
Abstract:
Propylene copolymer having a melt flow rate MFR2 (230° C.) in the range of more than 0.5 to below 2.5 g/10 min, a xylene cold soluble content (XCS) in the range of 30.0 to 40.0 wt-%, a comonomer content in the range of more than 7.5 to 12.0 wt.-%, wherein further the comonomer content of xylene cold soluble (XCS) fraction of the propylene copolymer is in the range of 16.0 to 28.0 wt.-%.