유전체 세라믹 조성물 및 그 제조방법
    1.
    发明授权
    유전체 세라믹 조성물 및 그 제조방법 失效
    电介质陶瓷组合物及其制造方法

    公开(公告)号:KR100808472B1

    公开(公告)日:2008-03-03

    申请号:KR1020060120341

    申请日:2006-12-01

    Applicant: (주)써모텍

    Abstract: A dielectric ceramic composition is provided to satisfy high permittivity, low dielectric loss, and low-temperature sintering characteristics of a dielectric substance containing Ba6Ti2Nb8O30 as a main component. A method for preparing a dielectric ceramic composition includes the steps of: calcining a base composition of Ba6Ti2Nb8O30; adding a sintering aid selected from the group consisting of ZnO-B2O3-based glass having a composition of ZnB2O4 or Zn3B2O6, an oxide mixture selected from a mixture of B2O3 and CuO and a mixture B2O3 and ZnO, and mixtures thereof, to the calcined base composition, and then mixing the admixture; grinding the mixture and molding the ground mixture into a predetermined shape; and sintering the molded material at 1000 ‹C or below.

    Abstract translation: 提供了一种电介质陶瓷组合物,以满足包含Ba6Ti2Nb8O30作为主要成分的电介质的高介电常数,低介电损耗和低温烧结特性。 制备电介质陶瓷组合物的方法包括以下步骤:煅烧Ba6Ti2Nb8O30的基础组合物; 添加选自组成为ZnB 2 O 4或Zn 3 B 2 O 6的ZnO-B 2 O 3类玻璃,选自B 2 O 3和CuO的混合物的氧化物混合物和B 2 O 3和ZnO混合物及其混合物的烧结助剂, 组合,然后混合混合物; 研磨混合物并将研磨的混合物模制成预定的形状; 并在1000℃以下烧结成型材料。

Patent Agency Ranking