公开(公告)号:WO2015026448A2
公开(公告)日:2015-02-26
申请号:PCT/US2014/045945
申请日:2014-07-09
Applicant: UNITED TECHNOLOGIES CORPORATION
Inventor: KLING, Colin J. , PARKOS, Joseph , LOMASNEY, Gary M. , BOGUE, William
CPC classification number: G06K19/07749 , B29C37/0025 , B29C64/124 , B29C64/153 , B29C67/0062 , B29C67/0077 , B29C70/42 , B29C70/54 , B29K2079/08 , B29K2105/0058 , B29K2105/12 , B29K2105/251 , B29K2105/253 , B29K2307/04 , B29K2309/08 , B29L2009/008 , B29L2031/082 , B32B27/08 , B32B27/281 , B32B2250/02 , B32B2255/10 , B32B2255/205 , B32B2262/101 , B32B2262/106 , B32B2603/00 , B33Y10/00 , B33Y70/00 , B33Y80/00 , C23C18/1641 , C23C18/1653 , C23C18/1657 , C23C18/166 , C23C18/22 , C23C18/30 , C23C18/32 , C23C28/021 , C23C28/023 , C25D1/003 , C25D1/02 , C25D1/20 , C25D3/02 , C25D5/06 , C25D5/54 , C25D5/56 , C25D7/00 , C25D7/04 , C25D9/02 , C25D17/12 , G01B7/16 , G01D5/12 , G01N3/08 , G01N2203/026 , G01N2203/0268 , G01N2203/0298
Abstract: A method for balancing a rotatable component is disclosed This method comprises and then plating the component to deposit a metal layer onto the component until the component is balanced. In addition, and alternative method for balancing a rotatable component is disclosed. This method comprises attaching a balancing weight to the rotatable component and rotating the component. This is followed by plating the component and the balancing weight to deposit a metal layer onto the balancing weight and the component until the component is balanced.
Abstract translation: 公开了一种用于平衡可旋转部件的方法。该方法包括然后电镀该部件以将金属层沉积到部件上直到部件平衡。 另外,公开了用于平衡可旋转部件的替代方法。 该方法包括将平衡配重附接到可旋转部件并旋转部件。 接着是电镀组件和平衡重量,以在平衡重和组件上沉积金属层,直到组件平衡为止。 p>
-
2.
公开(公告)号:EP3358143A1
公开(公告)日:2018-08-08
申请号:EP18154771.2
申请日:2018-02-01
Applicant: United Technologies Corporation
Inventor: MARTEL, Nathan T. , LOMASNEY, Gary M.
CPC classification number: F01D5/288 , C25D3/12 , C25D15/00 , F01D11/122 , F01D21/045 , F05D2230/31 , F05D2240/307 , F05D2300/611 , Y02T50/672
Abstract: An abrasive coating (116) for a substrate (114) comprises a strike layer (130) formed on a substrate top surface (132); a base layer (134) coupled to the strike layer; a tack layer (136) coupled to the base layer (134), wherein the tack layer (136) is configured to adhere first grit particles (118) to the base layer (134); a plurality of first grit particles (118) are adapted to be coupled to the tack layer (136), a plurality of second grit particles (122) are placed between each of the plurality of first grit particles (118), the second grit particles (122) having a nominal size smaller than the first grit particles (118); and an overplate layer (138) comprising a matrix material (120) is bonded to the tack layer (136); the matrix material (120) envelops the second grit particles (122) and bonds and partially surrounds the first grit particles (118), wherein the first grit particles (118) extend above the overplate layer (138).
-