Method for the production of calcium sulfate dihydrate based paper substrates and/or coating colours
    91.
    发明公开
    Method for the production of calcium sulfate dihydrate based paper substrates and/or coating colours 审中-公开
    维尔法赫尔·祖尔·赫斯特隆·冯·硫酸钙 - 二氢氯化钠底漆和/或Beschichtungsfarben

    公开(公告)号:EP2460935A1

    公开(公告)日:2012-06-06

    申请号:EP10193228.3

    申请日:2010-12-01

    Abstract: The present invention relates to a method for making a fibre-based substrate such as paper of board, which as filler particles or as a coating colour pigment constituent comprises calcium sulfate dihydrate pigment. According to the method, the calcium sulfate dihydrate pigment is introduced into the papermaking/coating process as a calcium sulfate dihydrate pigment slurry for the formation of the paper web and/or its coating formulation. In order to avoid losses due to dissolution of the pigment, it is proposed for the preparation of said calcium sulfate dihydrate pigment slurry to use a powdery calcium sulfate dihydrate pigment or a calcium sulfate dihydrate pigment starting slurry and to dilute it with water which is essentially presaturated in calcium sulfate dihydrate.

    Abstract translation: 本发明涉及一种制备作为填料颗粒或作为涂料颜料的组分包括硫酸钙二水合物颜料的基板的纤维基底的方法。 根据该方法,将硫酸钙二水合物颜料作为用于形成纸幅和/或其涂层制剂的硫酸钙二水合物颜料浆料被引入造纸/涂布方法。 为了避免颜料溶解造成的损失,提出制备所述硫酸钙二水合物颜料浆料以使用粉状硫酸钙二水合物颜料或硫酸钙二水合物颜料起始浆料,并用基本上用水稀释的水 以硫酸钙二水合物预饱和。

    COATING FORMULATION FOR AN OFFSET PAPER AND PAPER COATED THEREWITH
    92.
    发明公开
    COATING FORMULATION FOR AN OFFSET PAPER AND PAPER COATED THEREWITH 审中-公开
    胶版纸涂布配制剂,因此涂布纸

    公开(公告)号:EP2279299A1

    公开(公告)日:2011-02-02

    申请号:EP09732389.3

    申请日:2009-04-09

    Abstract: A coated paper for offset printing comprising at least on one side a top coating layer, is described, said top coating layer comprising a pigment part, the 100 parts in dry weight thereof consisting of a) in the range of 50 -100 parts in dry weight of a fine particulate pigment with a particle size distribution such that at least 50% of the particles have a size of below or equal to 1 μm and/or that at least 80% of the particles have a size of below or equal to 2 μm, b) in the range of 0 - 50 parts in dry weight of a fine particulate pigment with a particle size distribution such that at least 50% of the particles have a size of below or equal to 3 μm and/or that at least 40% of the particles have a size of below or equal to 2 μm, as well as c) in the range of 0 - 50 parts in dry weight of a further fine particulate pigment, the parts a), b) and c) supplementing to 100 parts in dry weight a binder part with in the range of 2 - 20 parts in dry weight of binder, an additive part with in the range of 0 - 8 parts in dry weight of additive(s), wherein the binder part comprises a synthetic auto-oxidative resinous binder or at least partly (modified) natural resinous binder with auto-oxidative drying functionality as well as optionally at least one further non-resinous binder.

    COATED PAPER FOR OFFSET PRINTING
    93.
    发明授权
    COATED PAPER FOR OFFSET PRINTING 有权
    涂布纸胶印

    公开(公告)号:EP1907626B1

    公开(公告)日:2010-11-03

    申请号:EP06777722.7

    申请日:2006-07-12

    Abstract: The specification pertains to a single or multiple coated printing sheet in particular but not exclusively for sheet-fed offset printing with an image receptive coating layer on a paper substrate. Unexpectedly short converting times and times until reprinting can be achieved by choosing a coating, in which the image receptive coating layer comprises a top layer and/or at least one second layer below said top layer, said top and/or second layer comprising a pigment part, wherein this pigment part is composed of 1-95 preferably of 80-95 parts in dry weight of a fine particulate carbonate and/or of a fine particulate kaolin or clay and 1-100, preferably 6 to 25 parts in dry weight of a fine particulate silica, and a binder part, wherein this binder part is composed of 5-20 parts in dry weight of binder and less than 4 parts in dry weight of additives. Furthermore methods for making such a printing sheet and uses of such a printing sheet are disclosed.

    Coating formulation for an offset paper and paper coated therewith
    94.
    发明公开
    Coating formulation for an offset paper and paper coated therewith 审中-公开
    胶版纸涂布配方及其涂布的纸张

    公开(公告)号:EP2053162A1

    公开(公告)日:2009-04-29

    申请号:EP07119350.2

    申请日:2007-10-26

    Abstract: The document describes a coated paper for offset printing e.g. with a TAPPI 75° gloss value of below 35% or with high gloss properties, comprising at least on one side a top coating layer, said top coating layer comprising a pigment part, the 100 parts in dry weight thereof comprising in the range of 5 - 40 parts in dry weight of a fine particulate ground calcium carbonate with surface and internal structure modification as a result of treatment with one or more medium to strong H 3 O + providers and eventually additional treatment with gaseous carbon dioxide, a binder part of 2 - 20 parts in dry weight of binder and (regular) additives in the range of 0 - 8 parts in dry weight.

    Abstract translation: 该文件描述了用于胶版印刷的涂布纸,例如 具有低于35%的TAPPI 75°光泽度值或具有高光泽度特性,其至少在一侧上包括顶部涂层,所述顶部涂层包含颜料部分,其100重量份干重包含5 - 40份干重量的细颗粒重质碳酸钙,由于用一种或多种中等强度的H 3 O +提供者处理并且最终用气态二氧化碳进行额外处理,其中粘合剂部分为2-20份 干重量的粘合剂和(常规)添加剂,干重范围为0-8份。

    COATED PAPER FOR OFFSET PRINTING
    95.
    发明公开
    COATED PAPER FOR OFFSET PRINTING 有权
    涂布纸胶印

    公开(公告)号:EP1907626A1

    公开(公告)日:2008-04-09

    申请号:EP06777722.7

    申请日:2006-07-12

    Abstract: The specification pertains to a single or multiple coated printing sheet in particular but not exclusively for sheet-fed offset printing with an image receptive coating layer on a paper substrate. Unexpectedly short converting times and times until reprinting can be achieved by choosing a coating, in which the image receptive coating layer comprises a top layer and/or at least one second layer below said top layer, said top and/or second layer comprising a pigment part, wherein this pigment part is composed of 1-95 preferably of 80-95 parts in dry weight of a fine particulate carbonate and/or of a fine particulate kaolin or clay and 1-100, preferably 6 to 25 parts in dry weight of a fine particulate silica, and a binder part, wherein this binder part is composed of 5-20 parts in dry weight of binder and less than 4 parts in dry weight of additives. Furthermore methods for making such a printing sheet and uses of such a printing sheet are disclosed.

    BARRIER PAPER OR BOARD
    96.
    发明公开

    公开(公告)号:EP4481113A2

    公开(公告)日:2024-12-25

    申请号:EP24211595.4

    申请日:2021-06-23

    Abstract: A process for improving the barrier properties of a barrier layer in a pulp-based substrate layer having a barrier layer, comprising the steps of providing a pulp-based substrate layer having a layer of an aqueous barrier composition applied to it, and then drying the pulp-based substrate layer having a layer of aqueous barrier composition applied to it to form a pulp-based substrate layer having a barrier layer, such that the moisture content of the pulp-based substrate layer having a barrier layer is below 2.5 % by weight, preferably below 2 % by weight, based on the weight of the pulp-based substrate layer having a barrier layer.

    Cellulosic fibres or filaments reinforced with inorganic particles and method for the production thereof
    99.
    发明公开
    Cellulosic fibres or filaments reinforced with inorganic particles and method for the production thereof 审中-公开
    无机颗粒增强的纤维素纤维或长丝和它们的制备方法

    公开(公告)号:EP2889400A1

    公开(公告)日:2015-07-01

    申请号:EP13199519.3

    申请日:2013-12-24

    CPC classification number: D01F2/00 D01F1/10

    Abstract: The present invention provides for a method for spinning a reinforced cellulosic fibre or filament, comprising the steps of: a. forming a composite spinning solution comprising inorganic reinforcing particles, a cellulosic base material and a process solvent, b. extruding the composite spinning solution through an orifice into a regeneration fluid such as to form the reinforced cellulosic fibre or filament, wherein the composite spinning solution is formed by dissolving the cellulosic base material in the process solvent and distributively dispersing the inorganic reinforcing particles in the process solvent and wherein the inorganic reinforcing particles have an aspect ratio of 1.25:1 or more, preferably of 1.5 or more and more preferably of 10:1 or more.

    Abstract translation: 本发明提供了一种用于纺制纤维素增强纤维或长丝,包括以下步骤的方法:一个。 形成复合纺丝溶液包括无机增强颗粒,纤维素基体材料和处理溶剂,B。 挤压成检测作为再生流体通过向孔的复合纺丝溶液以形成增强的纤维素纤维或长丝,worin复合纺丝溶液通过在该过程中的纤维素基材料溶解的溶剂和分布式无机增强颗粒分散在工艺形成 溶剂和worin无机增强颗粒具有1.25的长宽比:1或更大,优选为1.5以上,更优选为10:1或更高。