대면적 매그넬리상 타이타늄 산화물 및 그 제조방법
    91.
    发明公开
    대면적 매그넬리상 타이타늄 산화물 및 그 제조방법 有权
    具有高特异性表面积的MAGNELI相氧化钛及其制造方法

    公开(公告)号:KR1020130046479A

    公开(公告)日:2013-05-08

    申请号:KR1020110110897

    申请日:2011-10-28

    Abstract: PURPOSE: A magneli phase titanium oxide with a high specific surface area is provided to secure 35 wt% or more of a metal loading amount due to the high specific surface area and have excellent electric conductivity, high-voltage durability, and a high corrosive resistance under an oxygen atmosphere. CONSTITUTION: A magneli phase titanium oxide has a specific surface area in the range of 3-50m^2/g. The titanium oxide contains 80 wt% or more of Ti4O7 and Ti5O9. The titanium oxide further contains non-stoichiometric titanium oxide of TikO2k-(1+2l)(k is a natural number, wherein 4

    Abstract translation: 目的:提供比表面积高的镁硅相氧化钛,由于比表面积高,确保了35重量%以上的金属负载量,具有优异的导电性,高耐久性和高耐腐蚀性 在氧气氛下。 构成:镁橄榄相氧化钛的比表面积在3-50m ^ 2 / g范围内。 氧化钛含有80重量%以上的Ti 4 O 7和Ti 5 O 9。 氧化钛还含有非化学计量的TikO2k-(1 + 21)的氧化钛(k是自然数,其中4≤k≤10,l是自然数,其中1≤l≤=(k -1))。 在氧化钛中形成纳米孔,纳米孔的平均直径在10〜20nm的范围内。 氧化钛具有多孔分布的表面积。 基于氧化钛粒子的半径(R),表面积的厚度在10-40%的范围内。 氧化钛的金属负载量为35重量%以上。 用于燃料电池的催化剂含有镁铝相二氧化钛。 (附图标记)(AA,CC)MPTO; (BB,DD)现有MPTO

Patent Agency Ranking