公开(公告)号:CA2698577C
公开(公告)日:2013-08-20
申请号:CA2698577
申请日:2008-08-28
Applicant: CABOT CORP
Inventor: ZHANG XUAN , MORRIS MICHAEL D
Abstract: An elastomer composite includes the coagulated product of a mixture of a particulate slurry and a latex blend comprising skim latex and at least one of field latex and latex concentrate.
-
公开(公告)号:CA2811004A1
公开(公告)日:2013-03-22
申请号:CA2811004
申请日:2011-09-14
Applicant: CABOT CORP
Inventor: MORRIS MICHAEL D , PRAKASH ANAND , RUMPF FREDERICK H
Abstract: An elastomer composite with silica-containing filler is described, along with methods to make the same. The advantages achieved with the elastomer composite and methods are further described.
-
93.
公开(公告)号:ITTO20110827A1
公开(公告)日:2012-03-16
申请号:ITTO20110827
申请日:2011-09-15
Applicant: CABOT CORP
Inventor: MORRIS MICHAEL D , PRAKASH ANAND , RUMPF FREDERICK H
IPC: B29C48/395
-
94.
公开(公告)号:FR2964661A1
公开(公告)日:2012-03-16
申请号:FR1158209
申请日:2011-09-15
Applicant: CABOT CORP
Inventor: MORRIS MICHAEL D , PRAKASH ANAND , RUMPF FREDERICK H
IPC: C08J3/215 , B29C48/395 , C08J3/22 , C08K3/04 , C08K3/36 , C08K5/18 , C08K5/372 , C08L7/02 , C08L21/02
Abstract: On décrit un composite d élastomère avec une charge contenant de la silice, conjointement avec des procédés pour sa préparation. On décrit en outre les avantages obtenus avec le composite d'élastomère et les procédés. FIGURE 1
-
公开(公告)号:ZA201005671B
公开(公告)日:2011-04-28
申请号:ZA201005671
申请日:2010-08-06
Applicant: CABOT CORP
Inventor: TIRUMALA VIJAY R , GREEN MARTIN C , ZHANG XUAN , MORRIS MICHAEL D , WANG TING , WANG MENG-JIAO
Abstract: A method of producing an elastomer composite. The method includes A) combining a first fluid comprising elastomer latex with a second fluid comprising particulate filler; B) causing the elastomer latex to coagulate, thereby forming masterbatch crumb; C) bringing the masterbatch crumb to a water content of about 1 weight percent to about 20 weight percent, thereby forming a de-watered coagulum; D) removing water from the de-watered coagulum by subjecting the dewatered coagulum to mechanical energy, thereby causing the dewatered coagulum to heat as a result of friction, while allowing the dewatered coagulum to achieve a temperature of about 130° C. to about 190° C., wherein water content is reduced to about 0.5% to about 3% and wherein substantially all of the decrease in water content is accomplished by evaporation, thereby producing a masticated masterbatch; and E) subjecting the masticated masterbatch to at least an additional 0.3 MJ/kg of mechanical energy while further reducing the water content.
-
公开(公告)号:CA2714461A1
公开(公告)日:2009-08-13
申请号:CA2714461
申请日:2009-02-05
Applicant: CABOT CORP
Inventor: WANG MENG-JIAO , WANG TING , MORRIS MICHAEL D , ZHANG XUAN , GREEN MARTIN C , TIRUMALA VIJAY R
IPC: C08J3/22
Abstract: A method of producing an elastomer composite. The method includes A) combining a first fluid comprising elastomer latex with a second fluid comprising particulate filler; B) causing the elastomer latex to coagulate, thereby forming masterbatch crumb; C) bringing the masterbatch crumb to a water content of about 1 weight percent to about 20 weight percent, thereby forming a dewatered coagulum; D) removing water from the dewatered coagulum by subjecting the dewatered coagulum to mechanical energy, thereby causing the dewatered coagulum to heat as a result of friction, while allowing the dewatered coagulum to achieve a temperature of about 130°C to about 19O°C, wherein water content is reduced to about 0.5 % to about 3 % and wherein substantially all of the decrease in water content is accomplished by evaporation, thereby producing a masticated masterbatch; and E) subjecting the masticated masterbatch to at least an additional 0.3 MJ/kg of mechanical energy while further reducing the water content.
-
公开(公告)号:AU2008296995A1
公开(公告)日:2009-03-12
申请号:AU2008296995
申请日:2008-08-28
Applicant: CABOT CORP
Inventor: ZHANG XUAN , MORRIS MICHAEL D
Abstract: The present invention is a vulcanized elastomer composite including at least 70 phr carbon black, for example, N234 carbon black, and exhibiting a ratio of T300/T100 of at least 4.5.
-
-
-
-
-
-