91.DIENE RUBBER COMPOSITION CONFIGURED TO BE VULCANIZED AT LOWER TEMPERATURE; AND MANUFACTURING PROCESS OF RUBBER ARTICLE 审中-公开
Title translation: DIENE橡胶组合物被配置为在较低温度下成型; 和橡胶制品的制造工艺公开(公告)号:WO2016160781A1
公开(公告)日:2016-10-06
申请号:PCT/US2016/024667
申请日:2016-03-29
Applicant: KRATON POLYMERS U.S. LLC
Inventor: NAITO, Fumio , NAKAZAWA, Yoshikatsu
CPC classification number: C08J3/247 , C08J5/18 , C08J2307/00 , C08J2309/00 , C08K5/14 , C08K2201/019 , C08L7/00 , C08L9/00 , C08L9/06 , C08L23/16 , C08L2205/025 , C08K5/09
Abstract: The present invention provides a process for forming an article from a diene rubber, comprising: providing a raw diene rubber substance comprising 1,2-polybutadiene rubber component; adding to the raw diene rubber substance a peroxide as a vulcanizing agent; softening the raw diene rubber at a first temperature of not more than 200°C; vulcanizing the diene rubber at a second temperature of not more than 200°C, with contacting the diene rubber to an ambient atmosphere; and forming from the vulcanized diene rubber an article.
Abstract translation: 本发明提供了一种由二烯橡胶形成物品的方法,包括:提供包含1,2-聚丁二烯橡胶组分的原料二烯橡胶物质; 向原料二烯橡胶物质中加入作为硫化剂的过氧化物; 在不高于200℃的第一温度下软化原料二烯橡胶; 在不高于200℃的第二温度下硫化二烯橡胶,使二烯橡胶与环境气氛接触; 并从硫化二烯橡胶成型制品。
-
92.
公开(公告)号:WO2016124400A1
公开(公告)日:2016-08-11
申请号:PCT/EP2016/051111
申请日:2016-01-20
Applicant: BASF COATINGS GMBH
Inventor: STEINMETZ, Bernhard , JANKOWSKI, Peggy , LUHMANN, Nadia , MATURA, Michael , WOHLFAHRT, Michael
IPC: C09D7/00
CPC classification number: C09D7/63 , C08K5/52 , C08K5/521 , C08K2003/329 , C08K2201/019 , C09D5/002 , C09D7/61
Abstract: Die Erfindung betrifft die Verwendung von Phosphorsäure und/oder von Mono- und/oder Diestern der Phosphorsäure in wässrigen Basislacken zur Verbesserung der Haftung dieser Lacke auf überbrannten Klarlacken, die Borverbindungen enthalten.
Abstract translation: 本发明涉及在水基涂料中的使用磷酸和/或甘油单酯和/或磷酸二酯,以提高这些涂料在含有硼化合物烘焙清漆的粘合性。
-
93.A PROCESS FOR PREPARING A CONDUCTIVE COMPOSITION USING A MASTERBATCH. 审中-公开
Title translation: 使用主板来制备导电组合物的方法。公开(公告)号:WO2013107876A1
公开(公告)日:2013-07-25
申请号:PCT/EP2013/050964
申请日:2013-01-18
Applicant: TOTAL RESEARCH & TECHNOLOGY FELUY
Inventor: ROUSSEAUX, Dimitri , DUC, Michel , LODEFIER, Philippe , LHOST, Olivier
CPC classification number: H01B1/24 , C08J3/22 , C08J3/226 , C08J2325/04 , C08J2423/08 , C08J2425/04 , C08K3/04 , C08K3/041 , C08K7/24 , C08K2201/011 , C08K2201/019 , C08L23/06 , C08L25/06 , C08L51/04 , H01B3/441 , H01B3/442
Abstract: The present invention relates to a composition comprising polystyrene or modified-polystyrene or a mixture thereof, said polystyrene or modified-polystyrene or mixture thereof further comprising carbon nanotubes; wherein the composition comprises a polyolefin; and wherein the composition comprises at most 1.90 % by weight of carbon nanotubes, based on the total weight of the composition. The present invention also relates to a method for the preparation of the composition, wherein the carbon nanotubes are provided in polyolefin or styrenic copolymer masterbatch.
Abstract translation: 本发明涉及包含聚苯乙烯或改性聚苯乙烯或其混合物的组合物,所述聚苯乙烯或改性聚苯乙烯或其混合物还包含碳纳米管; 其中所述组合物包含聚烯烃; 并且其中所述组合物包含至少1.90重量%的碳纳米管,基于组合物的总重量。 本发明还涉及制备组合物的方法,其中碳纳米管设置在聚烯烃或苯乙烯共聚物母料中。
-
公开(公告)号:WO2013046804A1
公开(公告)日:2013-04-04
申请号:PCT/JP2012/063909
申请日:2012-05-30
Applicant: 住友ゴム工業株式会社 , 宮崎 達也
Inventor: 宮崎 達也
CPC classification number: B60C1/0025 , B60C19/086 , B60C2200/06 , C08K3/04 , C08K3/36 , C08K2201/019 , C08L7/00 , C08L9/00 , C08L9/02
Abstract: 本発明は、通電性、耐スピュー切れ性および押出し加工性においてバランスよく優れ、さらに作製コストにおいても優れたサイドウォール用ゴム組成物を提供することを目的とし、ジエン系ゴム成分100質量部に対して、BET比表面積が70~250m 2 /gの湿式シリカを2~15質量部、BET比表面積が37~125m 2 /gのカーボンブラックを40~62質量部含有し、シランカップリング剤を含有せず、体積固有抵抗が1×10 8 Ω・cm以下であるサイドウォール用ゴム組成物を提供する。
Abstract translation: 本发明的目的是提供一种侧导电橡胶组合物,其具有良好的导电性能,耐冲击破裂和挤出加工性能的平衡,以及低制造成本。 本发明提供一种体积电阻率为1×10 8Ω·cm以下的侧壁橡胶组合物,相对于100质量份二烯类橡胶成分,含有2〜15质量份具有BET的湿法二氧化硅 比表面积为70-250m 2 / g,40-62质量份BET比表面积为37-125m 2 / g的炭黑,不含硅烷偶联剂。
-
95.POLYMERIC FILM ASSEMBLIES WITH IMPROVED RESISTANCE TO SMUDGES, RELATED ARTICLES AND METHODS 审中-公开
Title translation: 具有改善电阻的聚合物薄膜组件,相关文章和方法公开(公告)号:WO2012106386A1
公开(公告)日:2012-08-09
申请号:PCT/US2012/023415
申请日:2012-02-01
Applicant: ENTROTECH, INC. , MCGUIRE, James, E., Jr.
Inventor: MCGUIRE, James, E., Jr.
IPC: B32B27/00
CPC classification number: C08K3/346 , B32B7/12 , B32B27/20 , C08K2201/011 , C08K2201/019 , C09J7/22 , C09J7/29 , C09J2201/162 , C09J2203/318 , C09J2205/106 , C09J2475/006 , G02B1/14 , Y10T156/10 , Y10T428/1476 , Y10T428/259 , Y10T428/28 , Y10T428/31598 , C08L75/04
Abstract: A polymeric film assembly for application to at least one surface of an article comprises a polymeric film comprising an exterior surface, wherein the polymeric film comprises at least one clay in an anti-smudge effective amount, and wherein the polymeric film is essentially free of low surface energy components. A method for application of a polymeric film to at least one surface of an electronic device is also disclosed.
Abstract translation: 用于应用于制品的至少一个表面的聚合物膜组件包括包含外表面的聚合物膜,其中所述聚合物膜包含至少一种具有防污染有效量的粘土,并且其中所述聚合物膜基本上不含低 表面能组分。 还公开了一种将聚合物膜应用于电子器件的至少一个表面的方法。
-
公开(公告)号:WO2011118827A1
公开(公告)日:2011-09-29
申请号:PCT/JP2011/057508
申请日:2011-03-22
Applicant: 日本フッソ工業株式会社 , 三井・デュポンフロロケミカル株式会社 , 福村 直己 , 竹山 昌宏 , 中澤 亮
IPC: C09D127/12 , B05D7/24 , C09D5/00 , C09D7/12 , C09D143/02
CPC classification number: C09D129/10 , C08K5/0091 , C08K5/057 , C08K5/098 , C08K2201/019 , C09D5/002 , C09D5/08 , C09D127/12 , C09D127/18 , Y10T428/24967 , Y10T428/269 , C08L27/12 , C08L27/18
Abstract: 本発明は、フッ素樹脂被膜と、金属、ガラス、セラミック、耐熱性プラスチック等の基材表面にフッ素樹脂被膜との充分な接着力を有するプライマー層を設けることにより、より高い耐食性の優れる被膜体を得ることができるクロムレスのフッ素樹脂含有プライマー組成物、それを用いた被膜製造方法および被膜体を提供する。 本発明により、反応性官能基含有フッ素樹脂およびASTM D1238に準拠して、荷重5kg、372℃で測定したメルトフローレート(MFR)が、10~100g/10分であるフッ素樹脂から選ばれる少なくとも1種のフッソ樹脂成分と、有機チタネートを含有し、フッ素樹脂成分に対する有機チタネートに含まれるチタン含有量が1~40重量%であることを特徴とする塗料組成物が提供される。
Abstract translation: 提供一种含有无铬氟树脂的底漆组合物,其可以通过将氟树脂膜和氟树脂膜一起具有足够的粘合强度的底漆层提供到基材的表面,从而提供具有优异的高抗腐蚀性的涂布体, 金属,玻璃,陶瓷和耐热塑料。 此外,提供了使用底漆组合物制造膜的方法和使用底漆组合物的涂布体。 提供一种涂料组合物,其基于ASTM D1238和含有反应性官能团的氟树脂,含有有机钛酸酯和至少一种选自氟树脂的氟树脂组分,其熔体流动速率(MFR)在372℃下测定 5kg的载荷为10〜100g / 10分钟,有机钛酸酯相对于氟树脂成分的钛含量为1〜40重量%。
-
公开(公告)号:CZ9801330A3
公开(公告)日:1998-11-11
申请号:CZ133098
申请日:1998-04-29
Applicant: MONTELL NORTH AMERICA INC
Inventor: BECKER RONALD F , STARSINIC MICHAEL E
IPC: C08J5/18 , C08K3/22 , C08K3/34 , C08K5/098 , C08K5/13 , C08K5/1535 , C08K5/17 , C08K5/32 , C08K5/523 , C08K5/526 , C08K5/5353 , C08L23/00 , C08L23/26 , D01F6/46
CPC classification number: C08K5/526 , C08K3/22 , C08K3/34 , C08K5/1535 , C08K5/32 , C08K5/5353 , C08K2201/019 , C08L23/02
-
公开(公告)号:NO981917A
公开(公告)日:1998-11-03
申请号:NO981917
申请日:1998-04-28
Applicant: MONTELL NORTH AMERICA INC
Inventor: BECKER RONALD F , STARSINIC MICHAEL E
IPC: C08J5/18 , C08K3/22 , C08K3/34 , C08K5/098 , C08K5/13 , C08K5/1535 , C08K5/17 , C08K5/32 , C08K5/523 , C08K5/526 , C08K5/5353 , C08L23/00 , C08L23/26 , D01F6/46 , C08L23/02 , D01F6/04
CPC classification number: C08K5/526 , C08K3/22 , C08K3/34 , C08K5/1535 , C08K5/32 , C08K5/5353 , C08K2201/019 , C08L23/02
-
公开(公告)号:JP6391812B2
公开(公告)日:2018-09-19
申请号:JP2017511655
申请日:2016-01-18
Applicant: ワッカー ケミー アクチエンゲゼルシャフト , Wacker Chemie AG
Inventor: トルステン、ジクスト , フランツ、ノイハウザー
CPC classification number: C08L83/06 , C08G77/08 , C08G77/16 , C08G77/18 , C08K3/30 , C08K3/36 , C08K5/5419 , C08K2003/3045 , C08K2201/006 , C08K2201/019 , C08L83/04 , C08L83/00
-
公开(公告)号:JP2018514493A
公开(公告)日:2018-06-07
申请号:JP2017551056
申请日:2016-03-30
Applicant: サビック グローバル テクノロジーズ ビー.ブイ.
Inventor: ベラ レダ , フレスカス ヘスース アルフォンソ カラヴェオ , アル‐ホワイシュ イブラヒム , ジェームズ ニジェシュ ケイ. , ヴァン デル ズワーグ シブランド , カリク ジブラン , フルン ヴィルヘルム エイ.
IPC: C04B35/495 , H01L41/09 , H01L41/113 , H01L41/18 , H01L41/187 , H01L41/43
CPC classification number: H01L41/1873 , C01G33/006 , C01P2002/34 , C01P2002/54 , C01P2002/72 , C01P2004/03 , C01P2004/38 , C01P2004/51 , C01P2004/62 , C01P2006/40 , C04B35/495 , C04B2235/3201 , C04B2235/3203 , C04B2235/786 , C04B2235/81 , C08K3/22 , C08K7/00 , C08K2201/001 , C08K2201/005 , C08K2201/019 , H01L41/183 , H01L41/37
Abstract: 粉末形態でありかつ単結晶相を有する、リチウム添加ニオブ酸カリウムナトリウム無鉛圧電セラミック材料、およびその使用方法を記載する。該圧電セラミック材料の製造方法も記載する。
-
-
-
-
-
-
-
-
-