Abstract:
An article that includes: an inorganic oxide substrate having opposing major surfaces; and an optical film structure disposed on a first major surface of the substrate, the optical film structure comprising one or more of a silicon-containing oxide, a silicon-containing nitride and a silicon-containing oxynitride and a physical thickness from about 50 nm to less than 500 nm. The article exhibits a hardness of 8 GPa or greater measured at an indentation depth of about 100 nm or a maximum hardness of 9 GPa or greater measured over an indentation depth range from about 100 nm to about 500 nm, the hardness and the maximum hardness measured by a Berkovich Indenter Hardness Test. Further, the article exhibits a single-side photopic average reflectance that is less than 1%.
Abstract:
Embodiments of this disclosure pertain to articles that exhibit scratch-resistance and improved optical properties. In some examples, the article exhibits a color shift of about 2 or less, when viewed at an incident illumination angle in the range from about 0 degrees to about 60 degrees from normal under an illuminant. In one or more embodiments, the articles include a substrate, and an optical film disposed on the substrate. The optical film includes a scratch-resistant layer and an optical interference layer. The optical interference layer may include one or more sub-layers that exhibit different refractive indices. In one example, the optical interference layer includes a first low refractive index sub-layer and a second a second high refractive index sub-layer. In some instances, the optical interference layer may include a third sub-layer.
Abstract:
A flexible substrate are disclosed comprising an amorphous inorganic composition, wherein the substrate has a thickness of less than about 250 μm and has at least one of: a) a brittleness ratio less than about 9.5 (μm)−1/2, or b) a fracture toughness of at least about 0.75 MPa·(m)1/2. Electronic devices comprising such flexible devices are also disclosed. Also disclosed is a method for making a flexible substrate comprising selecting an amorphous inorganic material capable of forming a substrate having a thickness of less than about 250 μm and having at least one of: a) a brittleness ratio of less than about 9.5 (μm)−1/2, or b) a fracture toughness of at least about 0.75 MPa·(m)1/2; and then forming a substrate from the selected inorganic material.
Abstract:
A flexible substrate are disclosed comprising an amorphous inorganic composition, wherein the substrate has a thickness of less than about 250 μm and has at least one of: a) a brittleness ratio less than about 9.5 (μm)−1/2, or b) a fracture toughness of at least about 0.75 MPa.(m)1/2. Electronic devices comprising such flexible devices are also disclosed. Also disclosed is a method for making a flexible substrate comprising selecting an amorphous inorganic material capable of forming a substrate having a thickness of less than about 250 μm and having at least one of: a) a brittleness ratio of less than about 9.5 (μm)−1/2, or b) a fracture toughness of at least about 0.75 MPa.(m)1/2; and then forming a substrate from the selected inorganic material.
Abstract:
A coated article may comprise a substrate and an optical coating. The substrate may have a major surface comprising a first portion and a second portion. A first direction that is normal to the first portion of the major surface may not be equal to a second direction that is normal to the second portion of the major surface. The optical coating may be disposed on at least the first portion and the second portion of the major surface. The coated article may exhibit at the first portion of the substrate and at the second portion of the substrate hardness of about 8 GPa or greater at an indentation depth of about 50 nm or greater as measured on the anti-reflective surface by a Berkovich Indenter Hardness Test.
Abstract:
Embodiments of durable, anti-reflective articles are described. In one or more embodiments, the article includes a substrate and an optical coating disposed on the major surface. The optical coating includes an anti-reflective coating and a scratch-resistant coating forming an anti-reflective surface. The article exhibits a maximum hardness of 12 GPa or greater, as measured on the anti-reflective surface by a a Berkovich Indenter Hardness Test along an indentation depth of about 100 nm or greater. The articles of some embodiments exhibit a single side average light reflectance measured at the anti-reflective surface of about 8% or less over an optical wavelength regime in the range from about 400 nm to about 800 nm and a reference point color shift in transmittance or reflectance of less than about 2. In some embodiments, the article exhibits an angular color shift of about 5 or less at all angles from normal incidence to an incident illumination angle that is 20 degrees or greater.
Abstract:
Embodiments of durable, anti-reflective articles are described. In one or more embodiments, the article includes a substrate and an optical coating disposed on the major surface. The optical coating includes an anti-reflective coating and a scratch-resistant coating forming an anti-reflective surface. The article exhibits a maximum hardness of 12 GPa or greater, as measured on the anti-reflective surface by a Berkovich Indenter Hardness Test along an indentation depth of about 100 nm or greater. The articles of some embodiments exhibit a single side average light reflectance measured at the anti-reflective surface of about 8% or less over an optical wavelength regime in the range from about 400 nm to about 800 nm and a reference point color shift in transmittance or reflectance of less than about 2. In some embodiments, the article exhibits an angular color shift of about 5 or less at all angles from normal incidence to an incident illumination angle that is 20 degrees or greater.
Abstract:
Embodiments of this disclosure pertain to a coating material comprising silicon and/or aluminum, hydrogen and any two or more of oxygen, nitrogen, carbon, and fluorine. The coating material exhibits a hardness of about 17 GPa or greater and an optical band gap of about 3.5 eV or greater. In some embodiments, the coating material includes, in atomic %, silicon and/or aluminum in an amount of about 40 or greater, hydrogen in an amount in the range from about 1 to about 25, nitrogen in an amount of about 30 or greater, oxygen in an amount in the range from about 0 to about 7.5, and carbon in an amount in the range from about 0 to about 10. The coating material may optionally include fluorine and/or boron. Articles including the coating material are also described and exhibit an average transmittance of about 85% or greater over an optical wavelength regime in the range from about 380 nm to about 720 nm and colorlessness.
Abstract:
A strengthened glass article having a central tension that is below a threshold value above which the glass exhibits frangible behavior. The central tension varies non-linearly with the thickness of the glass. The glass article may be used as cover plates or windows for portable or mobile electronic devices such as cellular phones, music players, information terminal (IT) devices, including laptop computers, and the like.
Abstract:
Embodiments of a layered-substrate comprising a substrate and a layer disposed thereon, wherein the layered-substrate is able to withstand fracture when assembled with a device that is dropped from a height of at least 100 cm onto a drop surface, are disclosed. The layered-substrate may exhibit a hardness of at least about 10 GPa or at least about 20 GPa. The substrate may include an amorphous substrate or a crystalline substrate. Examples of amorphous substrates include glass, which is optionally chemically strengthened. Examples of crystalline substrates include single crystal substrates (e.g. sapphire) and glass ceramics. Articles and/or devices including such layered-substrate and methods for making such devices are also disclosed.