Abstract:
PROBLEM TO BE SOLVED: To provide an aqueous primer that exerts good adhesion to a polyolefin resin without incorporating a chlorine-containing resin. SOLUTION: This aqueous primer comprises an acid modified polyolefin resin (A) and/or its salt that is prepared by graft polymerizing at least one selected from the group consisting of an unsaturated dicarboxylic acid, its anhydride and its ester derivative to a polyolefin resin, and has a mass average molecular weight more than 20,000 and an acid value of 4 mg KOH/g or more. COPYRIGHT: (C)2007,JPO&INPIT
Abstract:
PROBLEM TO BE SOLVED: To provide a thermoplastic resin composition having excellent moldability and giving a molded article having excellent scratch resistance, impact resistance and coloring property and provide a molded article having excellent scratch resistance, impact resistance and coloring property (color-developing property). SOLUTION: The thermoplastic resin composition contains (A) 1-99 pts.mass of a graft copolymer produced by grafting at least one kind of monomer selected from aromatic vinyl monomers, (meth)acrylic acid esters and vinyl cyanide monomers to an olefin rubber polymer G and (B) 1-99 pts.mass of a vinyl polymer provided that the grafting ratio of the graft copolymer is 65-90 mass% and the reduced viscosity (ηsp/C) of the acetone-soluble fraction of the graft copolymer A is 0.35-0.60 dl/g. COPYRIGHT: (C)2007,JPO&INPIT
Abstract:
PROBLEM TO BE SOLVED: To provide a polymer composite material with improved characteristics, specifically mechanical characteristics, heat resistance, impact strength and flame retardancy without determent to molding properties and the appearance inherent in the polymer, and also to provide a method for manufacturing the same and a molded product of the same. SOLUTION: The polymer composite material comprises a styrene based resin (A), a polycarbonate resin (B) and a lamellar silicate (C). The manufacturing method for the polymer composite material comprises the steps of: manufacturing a latex of the styrene based resin (A) by emulsification polymerization using an organic onium salt (D); preparing a resin component (E), where the lamellar silicate (C) and the organic onium salt (D) are dispersed in the styrene based resin (A), by mixing the latex of the thermoplastic resin (A) and the aqueous dispersion of the lamellar silicate (C); and mixing the resin component (E) with the polycarbonate resin (B). COPYRIGHT: (C)2006,JPO&NCIPI
Abstract:
PROBLEM TO BE SOLVED: To provide a thermoplastic resin composition which has excellent production stability and low temperature impact resistance, and to provide a molded article. SOLUTION: This thermoplastic resin composition comprises 15 to 44 pts.mass of a graft polymer (C) prepared by emulsion graft-polymerizing 55 to 25 mass% of a monomer mixture (B) comprising an aromatic vinylic monomer and a vinyl cyanide-based monomer to 45 to 75 mass% of a rubbery polymer (A) comprising an ethylene-propylene-non-conjugated diene copolymer and a low mol. wt. modified α-olefin copolymer and having a cross-linking rate of 15 to 55 mass%, and 85 to 56 pts.mass of copolymer (D) prepared by copolymerizing an aromatic vinyic monomer with a vinyl cyanide-based monomer (the total amount of the graft polymer (C) and the copolymer (D) is 100 pts.mass). COPYRIGHT: (C)2006,JPO&NCIPI
Abstract:
PROBLEM TO BE SOLVED: To provide a thermoplastic resin composition for laser welding improving appearance trouble such as occurrence of flashes and voids caused when synthetic resin parts are joined by the laser welding and to provide the synthetic resin parts using the thermoplastic resin composition for the laser welding. SOLUTION: The thermoplastic resin composition for the laser welding comprises a graft copolymer (A) and an infrared absorber exhibiting absorbency at 750-850 nm wavelength. The graft copolymer (A) is obtained by further carrying out graft polymerization of at least one kind of monomer (a2) selected from the group consisting of an aromatic vinyl monomer, a vinyl cyanide monomer, an acrylic or a methacrylic ester monomer and other vinyl monomers with a cross-linked acrylic rubber (a1) prepared by polymerizing a mixture (a1-2) of an acrylic ester with a monomer having ≥2 (meth)acryloyl groups or vinyl groups in the molecule and a monomer having an allyl group in the molecule in the presence of cross-linked polymer particles (a1-1). COPYRIGHT: (C)2006,JPO&NCIPI
Abstract:
PROBLEM TO BE SOLVED: To provide a polylactic acid-based thermoplastic resin composition excellent in mechanical properties such as impact resistance, heat resistance or the like by imparting mechanical strength such as practically sufficient impact resistance to a polylactic acid resin. SOLUTION: The polylactic acid-based thermoplastic resin composition comprises (A) 10-95 pts.wt. polylactic acid resin and (B) 5-90 pts.wt. rubber-containing graft copolymer obtained by carrying out graft polymerization of a rubber-like polymer having 50-90 wt.% gel content with a vinyl cyanide-based monomer and an aromatic vinyl-based monomer so that total content of components A and B becomes 100 pts.wt. In the resin composition, (C) a rigid copolymer obtained by copolymerizing the vinyl cyanide-based monomer with an aromatic vinyl-based monomer may further be contained and further, (D) other resin such as polyester-based resin may be formulated. The rubber content in the rubber-containing graft copolymer (B) or the rubber content in total of the rubber-containing graft copolymer (B) and the rigid copolymer (C) is 40-80 wt.%. COPYRIGHT: (C)2006,JPO&NCIPI
Abstract:
PROBLEM TO BE SOLVED: To provide a thermoplastic resin composition which is highly flowable and prevented from generation of silver streaks while retaining impact resistance and coatability. SOLUTION: The thermoplastic resin composition comprises 20-40 pts.mass of a rubber-containing graft copolymer (A) comprised of a rubbery polymer (a) having a gel content of 70-85% and, grafted thereonto, an aromatic vinyl monomer unit and a vinyl cyanide monomer unit with a graft density within the range of 3-15%, and 80-60 pts.mass of a matrix resin (B) comprising the aromatic vinyl monomer unit and the vinyl cyanide monomer unit (the total of the rubber-containing graft copolymer (A) and the matrix resin (B) being 100 pts.mass), where the matrix resin (B) has a mass-average molecular weight (Mw) of 55,000-80,000 and contains at least 50 mass% of a vinyl copolymer having a vinyl cyanide monomer unit content of 20-30 mass%. COPYRIGHT: (C)2006,JPO&NCIPI
Abstract:
PROBLEM TO BE SOLVED: To provide a thermoplastic resin composition having a high sliding property, excellent in surface appearances and mechanical strengths and exhibiting high manufacturing stability, and a molded article thereof. SOLUTION: The thermoplastic resin composition comprises a graft polymer (C), obtained by emulsion graft polymerization of a monomer mixture (B) comprising an aromatic vinyl monomer and a vinyl cyanide monomer onto a rubbery polymer (A) comprising an ethylene-propylene-non-conjugated diene copolymer having an ethylene content of 75-90 mass% and a low-molecular weight modified α-olefin copolymer, and a copolymer (D) obtained by copolymerization of the aromatic vinyl monomer with the vinyl cyanide monomer. COPYRIGHT: (C)2006,JPO&NCIPI
Abstract:
PROBLEM TO BE SOLVED: To provide a thermoplastic resin composition capable of obtaining a molded article excellent in flowability and moldability, as well as excellent in balance between impact resistance and rigidity, and to provide the molded article thereof. SOLUTION: The thermoplastic resin composition comprises 30-50 parts mass of a rubber-containing graft copolymer (A) and 50-70 parts mass of a hard polymer (B), wherein (A)+(B)=100 parts mass. The rubber-containing graft copolymer (A) is prepared by allowing a rubbery polymer (a), which has a gel content of 50-70 mass%, an amount of swelling of 10-50 times and a mass average particle size of 100-600 nm, to occlude an aromatic vinyl monomer and a vinyl cyanide monomer and by graft polymerization of the monomers in the range of a graft density of 6-15%. The hard polymer (B) has aromatic vinyl monomer units and vinyl cyanide monomer units, has a ratio (Mw/Mn) of mass average molecular weight Mw to number average molecular weight Mn of acetone solubles of 4.0 or more, and has a proportion of the polymer having a molecular weight of 50,000 or more of 35-65 mass%. COPYRIGHT: (C)2006,JPO&NCIPI