폴리(트리메틸렌 테레프탈레이트) 카페트의 제조방법
    119.
    发明公开
    폴리(트리메틸렌 테레프탈레이트) 카페트의 제조방법 失效
    聚(三甲苯三烯酸)地毯的制造方法

    公开(公告)号:KR1020020087159A

    公开(公告)日:2002-11-22

    申请号:KR1020010026144

    申请日:2001-05-14

    Abstract: PURPOSE: Provided is a manufacturing method of a poly(trimethylene terephthalate) carpet having beautiful appearance, excellent touch, abrasion resistance, elastic recovering ratio, excellent anti-fouling property, excellent antistatic property, excellent exfoliating strength, excellent pulling strength and excellent shape stability. CONSTITUTION: The poly(trimethylene terephthalate) carpet is obtained by a process containing the steps of: (s1) cabling; (s2) heat-setting with a superba at 120-160deg.C of temperature on a main tunnel at 4-9m/min of band speed on 200-240g/m of density; (s3) tufting to make 5-15/inch of stitch; (s4) beck-dyeing the tufted carpet with disperse dyes at normal pressure at 90-100deg.C of temperature without carrier; (s5) backing the dyed carpet; and then (s6) shearing.

    Abstract translation: 目的:提供具有美观,触感,耐磨性,弹性回复率,优异的抗结垢性,优异的抗静电性,优异的剥离强度,优异的拉伸强度和优异的形状稳定性的聚(对苯二甲酸丙二醇酯)地毯的制造方法 。 构成:通过包括以下步骤的方法获得聚(对苯二甲酸丙二醇酯)地毯:(s1)布线; (s2)以200-240g / m密度,以​​主干隧道的温度为120-160℃,以4-9m / min的速度进行热定型; (s3)簇绒制作5-15英寸针迹; (s4)使用分散染料在90-100℃的温度下在常压下对簇绒地毯进行染色,无载体; (s5)支持染色地毯; 然后(s6)剪切。

Patent Agency Ranking