Abstract:
A propylene-1-hexene copolymer having: i) a content of 1-hexene derived units ranging from 0.6 wt% to 3.0 wt%; ii) melt flow rate (MFR) measured according to the method ISO 1133 (230° C, 5 kg) ranging from 0.5 g/10 min to 5.0 g/10 min iii) the polydispersity (PI) ranges from 4.5 to 10 and the distribution of molecular weight is of multimodal type; iv) the melting point ranges from 160°C to 145°C; v) the DSC curve (temperature/heat of fusion) shows at least two peaks.
Abstract:
A polyolefin composition comprising: A) from 85.0 wt% to 99.5 wt%; A terpolymer containing propylene, ethylene and 1- hexene wherein: (i) the content of 1-hexene derived units ranges from 1.0 wt% to 5.0%; (ii) the content of ethylene derived units is comprised between 0.5 wt% and 10.0 wt% (iii) the melting temperature ranges from 130° C to 145° C; B) from 0.5 wt% to 10.0 wt%; of a propylene, ethylene copolymer composition comprising: b1) from 12 wt% to 52 wt%; of a propylene homopolymer or a propylene/ethylene copolymer having a content of ethylene derived units ranging from 0.1 wt% to 4.5 wt%; and having a xylene soluble content measured at 25°C lower than 10 wt%; b2) from 48 wt% to 88 wt% of a propylene ethylene copolymer having a content of ethylene derived units ranging from 15.0 wt% to wt% to 42.0 wt%; wherein the resulting polyolefin composition has an melt flow rate (230°C/5 kg..ISO 133) ranging from 0.2 g/10min to 4.0 g/10min; the sum A+B being 100 and the sum b1+b2 being 100.
Abstract:
Polyolefin compositions suitable for injection moulded items e.g. for impact bumpers and car interiors comprising from 30% to 90% by weight of an heterophasic propylene polymer composition (A) ; and from 10% to 70% by weight of a multimodal ethylene/C6-C12 alpha olefin copolymer (B); having density from 0.850 to 0.920 g/cm 3 , total comonomer content from 6% to 30% by weight, Mw/Mn from 4 to 20; intrinsic viscosity in decalin at 135°C from 1.0 to 4.0 dL/g, and comprising an HDPE fraction (HDPE %wt) up to 30%wt; further comprising up to 50 % by weight of a filler (C) and optionally, in amount up to 10% by weight with respect to the overall composition, an impact modifier masterbatch component (D) consisting of a ultra-soft heterophasic copolymer component.
Abstract:
A copolymer of propylene with hexene-1 containing from 5 to 9% by weight of recurring units derived from hexene-1, having a melting temperature from 125° C. to 140° C. and Melt Flow Rate (ASTM D1238, 230° C./2.16 Kg) from 0.1 to 3 g/10 min., is used to produce blown films having valuable mechanical and optical properties.
Abstract translation:丙烯与己烯-1的共聚物,其含有5至9重量%的衍生自己烯-1的重复单元,其熔点为125-140℃,熔体流动速率(ASTM D1238,230 / 2.16Kg)为0.1至3 g / 10分钟,用于生产具有有价值的机械和光学性能的吹塑薄膜。
Abstract:
A masterbatch composition comprising, all percent amounts being by weight: A) 10-45 % of a homopolymer or a copolymer of propylene; B) 10-30 % of a copolymer of propylene with ethylene, containing from 18 to 45 % of ethylene; C) 42-60 % of a copolymer of propylene with ethylene, containing from 55 to 85 % of ethylene; said composition having a MFR L value from 0.01 to 10 g/10 min., a value of the intrinsic viscosity [η] sol of the fraction soluble in xylene at room temperature from 1.5 to 2.5 dl/g and a value of the ratio [η] sol /MFR L equal to or lower than 6.
Abstract:
1 -butene/ethylene/propylene terpolymer containing: c) from 4 to 10 wt% of ethylene derived units, and d) from 2 tol0wt% of propylene derived units; the said terpolymer having the following properties: - distribution of molecular weights (Mw/Mn) measured by GPC lower than 3; - no melting point detectable at the DSC; - melting enthalpy, measured after 10 days of aging at room temperature, from 12 to 20 J/g
Abstract:
A polyolefin composition comprising, in percent by weight: A) 10-25% of a propylene homopolymer or copolymer with up to 8% of comonomer(s); B) 75-90% of a copolymer of ethylene and (i) propylene or (ii) CH2=CHR alpha- olefins, where R is a 2-8 carbon alkyl radical, or (iii) a combination thereof, optionally with minor amounts of a diene, containing from 54 to 65% of ethylene; wherein the weight ratio B/XS of the content B of copolymer component (B) to the fraction XS soluble in xylene at room temperature, both referred to the total weight of (A) + (B), is of 1.50 or less.
Abstract:
A polyolefin composition having unusually low values of flexural modulus and shore hardness andcomprising, in percent by weight: A) 15-40% of a copolymer of propylene with hexene-1 containing from 2.5 to 10% of hexene-1 and having Melt Flow Rate (MFR, measured according to ISO 1133, 230°C/2.16 Kg) from 0.5 to 100g/10 min.; and B) 60-85% of an ethylene copolymer containing ethylene in a quantity equal to or lower than 40%, and having solubility in xylene at room temperature greater than 70%.
Abstract:
Polyolefin composition comprising, in percent by weight: A) 50-75% of a blend of polymers (PP) and (ECI), wherein (PP) is selected from the group consisting of: (i) propylene homopolymers; (ii) copolymers of propylene; (iii) combinations of said homopolymers (i) and copolymers (ii); (EC1) is a copolymer of ethylene and propylene or CH2=CHR alpha-olefin(s), where R is a 2-8 carbon alkyl radical, or a copolymer of ethylene, propylene and the said CH2=CHR alpha-olefin(s), containing from 20 to 35%, of ethylene; and B) 25-50% of a copolymer (ECII) of ethylene and propylene or CH2=CHR alpha-olefin(s), where R is a 2-8 carbon alkyl radical,or a copolymer of ethylene, propylene and the said CH2=CHR alpha-olefin(s), containing from 40 to 60% of ethylene; in which composition the copolymer component (ECI) is present in amounts from 23 to 45% with respect to the total weight of (A),and the intrinsic viscosity [ηtot] of the fraction XS soluble in xylene at room temperature, referred to the total weight of (A) + (B), is of 3.5 dl/g or more.
Abstract:
A polyolefin composition comprising, in percent by weight: A) 10-25% of a propylene homopolymer or copolymer with up to 8% of comonomer(s); B) 75-90% of a copolymer of ethylene and (i) propylene or (ii) CH2=CHR alpha- olefins, where R is a 2-8 carbon alkyl radical, or (iii) a combination thereof, optionally with minor amounts of a diene, containing from 54 to 65% of ethylene; wherein the weight ratio B/XS of the content B of copolymer component (B) to the fraction XS soluble in xylene at room temperature, both referred to the total weight of (A) + (B), is of 1.50 or less.