公开(公告)号:SG10201704148SA
公开(公告)日:2017-06-29
申请号:SG10201704148S
申请日:2013-10-23
Applicant: CORNING INC
Inventor: CHANG THERESA , DEMARTINO STEVEN EDWARD , FADEEV ANDREI GENNADYEVICH , PEANASKY JOHN STEPHEN , SCHAUT ROBERT ANTHONY , TIMMONS CHRISTOPHER LEE , BOOKBINDER DANA CRAIG
Abstract: The glass containers described herein have at least two performance attributes selected from resistance to delamination, improved strength, and increased damage resistance. In one embodiment, a glass container may include a body having an inner surface, an outer surface and a wall thickness extending between the outer surface and the inner surface. At least the inner surface of the body may have a delamination factor less than or equal to 10. A tenacious inorganic coating may be positioned around at least a portion of the outer surface of the body. The outer surface of the body with the tenacious inorganic coating may have a coefficient of friction less than or equal to 0.7.
-
公开(公告)号:AU2013352517C1
公开(公告)日:2017-04-20
申请号:AU2013352517
申请日:2013-11-22
Applicant: CORNING INC
Inventor: CHANG THERESA , DANIELSON PAUL STEPHEN , DEMARTINO STEVEN EDWARD , FADEEV ANDREI GENNADYEVICH , MORENA ROBERT MICHAEL , PAL SANTONA , PEANASKY JOHN STEPHEN , SCHAUT ROBERT ANTHONY , TIMMONS CHRISTOPHER LEE , VENKATARAMAN NATESAN , VERKLEEREN RONALD LUCE
Abstract: The glass containers described herein are resistant to delamination, have improved strength, and increased damage resistance. In one embodiment, a glass container may include a body having an inner surface, an outer surface and a wall thickness extending between the outer surface and the inner surface. At least the inner surface of the body may have a delamination factor less than or equal to 10. The body may also have a compressively stressed layer extending from the outer surface of the body into the wall thickness. The compressively stressed layer may have a surface compressive stress greater than or equal to 150 MPa. A lubricous coating may be positioned around at least a portion of the outer surface of the body, such that the outer surface of the body with the lubricous coating has a coefficient of friction less than or equal to 0.7.
-
公开(公告)号:AU2013352512B2
公开(公告)日:2017-03-30
申请号:AU2013352512
申请日:2013-11-22
Applicant: CORNING INC
Inventor: CHANG THERESA , DANIELSON PAUL STEPHEN , DEMARTINO STEVEN EDWARD , FADEEV ANDREI GENNADYEVICH , MORENA ROBERT MICHAEL , PAL SANTONA , PEANASKY JOHN STEPHEN , SCHAUT ROBERT ANTHONY , TIMMONS CHRISTOPHER LEE , VENKATARAMAN NATESAN , VERKLEEREN RONALD LUCE
IPC: C03C17/00 , B32B17/06 , B65D1/40 , B65D25/14 , C03C17/30 , C03C17/32 , C03C17/42 , C03C21/00 , C09D179/08
Abstract: The glass containers described herein have at least two performance attributes selected from resistance to delamination, improved strength, and increased damage resistance. In one embodiment, a glass container may include a body having an inner surface, an outer surface and a wall thickness extending between the outer surface and the inner surface. A compressively stressed layer may extend from the outer surface of the body into the wall thickness. The compressively stressed layer may have a surface compressive stress greater than or equal to 150 MPa. A lubricous coating may be positioned around at least a portion of the outer surface of the body. The outer surface of the body with the lubricous coating may have a coefficient of friction less than or equal to 0.7.
-
公开(公告)号:AU2013226031B2
公开(公告)日:2016-11-17
申请号:AU2013226031
申请日:2013-02-28
Applicant: CORNING INC
Inventor: DEMARTINO STEVEN EDWARD , SCHAUT ROBERT ANTHONY
Abstract: A strengthened glass container or vessel such as, but not limited to, vials for holding pharmaceutical products or vaccines in a hermetic and/or sterile state. The strengthened glass container undergoes a strengthening process that produces compression at the surface and tension within the container wall. The strengthening process is designed such that the tension within the wall is great enough to ensure catastrophic failure of the container, thus rendering the product unusable, should sterility be compromised by a through-wall crack. The tension is greater than a threshold central tension, above which catastrophic failure of the container is guaranteed, thus eliminating any potential for violation of pharmaceutical integrity.
-
公开(公告)号:MX343430B
公开(公告)日:2016-11-03
申请号:MX2014004972
申请日:2012-10-25
Applicant: CORNING INC
Inventor: DRAKE MELINDA ANN , MORENA ROBERT MICHAEL , DANIELSON PAUL STEPHEN , DEMARTINO STEVEN EDWARD , PAL SANTONA , SCHAUT ROBERT ANTHONY
Abstract: Las modalidades descritas en la presente se refieren a composiciones de vidrio química y mecánicamente durables, y artículos de vidrio formados de las mismas; en otra modalidad, una composición de vidrio puede incluir de aproximadamente 70% molar a aproximadamente 80% molar de SiO2; de aproximadamente 3% molar a aproximadamente 13% molar de óxido alcalinotérreo; X% molar de Al2O3; y Y% molar de óxido de álcali; el óxido de álcali puede incluir Na2O en una cantidad mayor de aproximadamente 8% molar; la razón Y:X puede ser mayor de 1, y la composición de vidrio puede estar libre de boro y compuestos de boro; el algunas modalidades, la composición de vidrio también puede estar libre de fósforo y compuestos de fósforo; los artículos de vidrio formados de la composición de vidrio pueden tener una resistencia al ácido de por lo menos clase S3 de acuerdo con DIN 12116, una resistencia a la base de por lo menos clase A2 de acuerdo con ISO 695, y una resistencia hidrolítica de tipo HGA1 de acuerdo con ISO 720.
-
公开(公告)号:AU2013226034C1
公开(公告)日:2016-10-27
申请号:AU2013226034
申请日:2013-02-28
Applicant: CORNING INC
Inventor: FADEEV ANDREI GENNADYEVICH , CHANG THERESA , BOOKBINDER DANA CRAIG , PAL SANTONA , SAHA CHANDAN KUMAR , DEMARTINO STEVEN EDWARD , TIMMONS CHRISTOPHER LEE , PEANASKY JOHN STEPHEN
Abstract: Low-friction coatings and glass articles with low-friction coatings are disclosed. According to one embodiment, a coated glass article may include a glass body comprising a first surface and a low-friction coating positioned on at least a portion of the first surface of the glass body. The low-friction coating may include a polymer chemical composition. The coated glass article may be thermally stable at a temperature of at least about 260°C for 30 minutes. A light transmission through the coated glass article may be greater than or equal to about 55% of a light transmission through an uncoated glass article for wavelengths from about 400 nm to about 700 nm. The low- friction coating may have a mass loss of less than about 5% of its mass when heated from a temperature of 150°C to 350°C at a ramp rate of about 10°C/minute.
-
公开(公告)号:CA2959666A1
公开(公告)日:2016-03-10
申请号:CA2959666
申请日:2015-09-04
Applicant: CORNING INC
Inventor: DEMARTINO STEVEN EDWARD , ELLISON ADAM JAMES , HOFF KYLE CHISTOPHER
IPC: C03C15/00
Abstract: According to one embodiment, a glass article may include a glass body having a first surface and a second surface opposite the first surface. The first surface and the second surface each have a radius of curvature. The first surface of the glass body comprises a flaw population extending from the first surface into a thickness of the glass body with a maximum initial flaw depth Ai. The first surface of the glass body may be etched to a depth less than or equal to about 25% of the maximum initial flaw depth Ai of the flaw population present in the first surface. When the glass article is under uniaxial compressive loading, at least a portion of the first surface is in tension and a uniaxial compressive strength of the glass article is greater than or equal to 90% of a uniaxial compressive strength of a flaw-free glass article.
-
公开(公告)号:MX2015006890A
公开(公告)日:2015-09-16
申请号:MX2015006890
申请日:2013-11-22
Applicant: CORNING INC
Inventor: MORENA ROBERT MICHAEL , DANIELSON PAUL STEPHEN , DEMARTINO STEVEN EDWARD , SCHAUT ROBERT ANTHONY , FADEEV ANDREI GENNADYEVICH , CHANG THERESA , TIMMONS CHRISTOPHER LEE , PEANASKY JOHN STEPHEN , PAL SANTONA , VENKATARAMAN NATESAN , VERKLEEREN RONALD LUCE
IPC: C03C17/00 , B32B17/06 , B65D1/40 , B65D25/14 , C03C17/30 , C03C17/32 , C03C17/42 , C03C21/00 , C09D179/08
Abstract: Los contenedores de vidrio descritos en la presente tienen por lo menos dos atributos de rendimiento seleccionados de resistencia a la deslaminación, resistencia mejorada y mayor resistencia al daño; en una modalidad, un contenedor de vidrio puede incluir un cuerpo que tiene una superficie interna, una superficie externa y un grosor de pared que se extiende entre la superficie externa y la superficie interna; una capa tensada compresivamente que se extiende desde la superficie externa del cuerpo hacia el grosor de pared; la capa tensada compresivamente puede tener un esfuerzo de compresión de superficie mayor o igual que 150 MPa; se puede colocar un revestimiento lúbrico sobre por lo menos una porción de la superficie externa del cuerpo; la superficie externa del cuerpo con el revestimiento lúbrico puede tener un coeficiente de fricción menor o igual que 0.7.
-
公开(公告)号:MX2015006899A
公开(公告)日:2015-09-08
申请号:MX2015006899
申请日:2013-11-22
Applicant: CORNING INC
Inventor: MORENA ROBERT MICHAEL , DANIELSON PAUL STEPHEN , DEMARTINO STEVEN EDWARD , SCHAUT ROBERT ANTHONY , FADEEV ANDREI GENNADYEVICH , CHANG THERESA , TIMMONS CHRISTOPHER LEE , PEANASKY JOHN STEPHEN , PAL SANTONA , VENKATARAMAN NATESAN , VERKLEEREN RONALD LUCE
Abstract: Los contenedores de vidrio descritos en la presente son resistentes a la deslaminación, tienen fuerza mejorada y mayor resistencia al daño; en una modalidad, un contenedor de vidrio puede incluir un cuerpo que tiene una superficie interior, una superficie exterior y un grosor de pared que se extiende entre la superficie exterior y la superficie interior; por lo menos la superficie interior del cuerpo puede tener un factor de deslaminación menor o igual que 10; el cuerpo también puede tener una capa tensada compresivamente que se extiende desde la superficie exterior del cuerpo en el grosor de pared; la capa tensada compresivamente puede tener una tensión de compresión de superficie mayor o igual que 150 MPa; se puede poner un revestimiento lúbrico alrededor de por lo menos una porción de la superficie exterior del cuerpo, de modo que la superficie exterior del cuerpo con el revestimiento lúbrico tenga un coeficiente de fricción menor o igual que 0.7.
-
公开(公告)号:SG11201504070PA
公开(公告)日:2015-06-29
申请号:SG11201504070P
申请日:2013-11-22
Applicant: CORNING INC
Inventor: CHANG THERESA , DANIELSON PAUL STEPHEN , DEMARTINO STEVEN EDWARD , FADEEV ANDREI GENNADYEVICH , MORENA ROBERT MICHAEL , PAL SANTONA , PEANASKY JOHN STEPHEN , SCHAUT ROBERT ANTHONY , TIMMONS CHRISTOPHER LEE , VENKATARAMAN NATESAN , VERKLEEREN RONALD LUCE
IPC: C03C17/00 , B32B17/06 , B65D1/40 , B65D23/08 , B65D25/14 , C03C17/30 , C03C17/32 , C03C17/42 , C03C21/00 , C09D179/08
Abstract: The glass containers described herein have at least two performance attributes selected from resistance to delamination, improved strength, and increased damage resistance. In one embodiment, a glass container may include a body having an inner surface, an outer surface and a wall thickness extending between the outer surface and the inner surface. At least the inner surface of the body may have a delamination factor less than or equal to 10. A tenacious inorganic coating may be positioned around at least a portion of the outer surface of the body. The outer surface of the body with the tenacious inorganic coating may have a coefficient of friction less than or equal to 0.7.
-
-
-
-
-
-
-
-
-