Abstract:
The present invention pertains to a UHMWPE film having a tensile strength of at least 2.0 GPa, a tensile energy to break of at least 30 J/g, an Mw of at least 500 000 gram/mole, and a Mw/Mn ratio of at most 6. The film may be manufactured via a process which comprises subjecting a starting UHMWPE with a weight average molecular weight of at least 500 000 gram/mole, an elastic shear modulus determined directly after melting at 160° C. of at most 0.9 MPa, and a Mw/Mn ratio of at most 6 to a compacting step and a stretching step under such conditions that at no point during the processing of the polymer its temperature is raised to a value above its melting point. The film may be used as starting material in any applications where high tensile strength and high energy to break are important. Suitable applications include ballistic applications, ropes, cables, nets, fabrics, and protective applications.
Abstract:
A mooring loop is provided for use with connecting a mooring line to a bollard. The mooring loop may stretch and function as a time delay fuse when excessive loads are applied to the mooring line. The mooring loop is comprised of a reactive fiber component in the shape of a continuous loop that includes a plurality of at least one of: an undrawn hydrophobic polymer fiber or a substantially undrawn hydrophobic polymer fiber. At least two jackets are in surrounding relation to portions of the reactive fiber component. The at least two jackets include respective end portions which overlap. As the mooring loop stretches, a visual indicator on an end portion of one of the jackets pulls out of and away from the end portion of the other one of the jackets. The visual indicator serves as a warning that excessive loads are being applied to the mooring line.
Abstract:
A process for manufacturing high molecular weight polyethylene fibers, including subjecting a polyethylene tape with a weight average molecular weight of at least 500,000 grams/mole, a Mw/Mn ratio of at most 6, and a 200/110 uniplanar orientation parameter of at least 3 to a force in the direction of the thickness of the tape over the entire width of the tape. A polyethylene fiber having a Mw of at least 500 000 gram/mole, a Mw/Mn ratio of at most 6, and a 020 uniplanar orientation value of at most 55°.
Abstract:
A system and method for actively damping tension members modulates the natural frequency of shape memory alloys incorporated into tension members, such as suspension ropes or cables. The frequency of the tension member can be modulated by heating the shape memory alloy, such modulation preventing potentially destructive resonance with natural exciting forces.
Abstract:
A securing device is provided comprised of a reactive fiber component and at least one of a terminating fiber component and an initiating fiber component. The reactive fiber component includes at least one of the following: an undrawn polymer fiber and a substantially undrawn polymer fiber, wherein the first reactive fiber component is operative to stretch responsive to a load. The terminating fiber component is in a compressed state and is operative to elongate to a length at which the terminating fiber component is operative to prevent further stretching of the first reactive fiber component responsive to the load. The initiating fiber component is operative to break responsive to a predetermined force and permit the first reactive fiber component to stretch responsive to the load.
Abstract:
Rope (4) having an eye (2). The rope (4) comprises a first rope portion (8) and a second rope portion (10). The first rope portion (8) and the second rope portion (10) are spliced into each other for forming a spliced connection for obtaining the eye (2). The first rope portion (8) and the second rope portion (10) are formed from an end portion of the rope (4).
Abstract:
An elastic link for adjusting the distance between two members, at least one of which is mobile, is characterised in that it includes at least two elastic yarns each attached through one of the opposite ends thereof to two points distant from each other of an intermediate portion of a strap located between the extreme portions of the latter, under conditions such that when a tensile force is applied on said strap, the first elastic yarn is stretched first, the second elastic yarn being then stretched based on the magnitude of the applied tensile force.
Abstract:
The invention relates to a wire cable (12) which is produced by producing the wires already in the cable configuration by layer construction. Preferably, the wires are already formed onto terminal couplings. The wire cable (12) so produced is suitable for specific purposes only. It is advantageous in that it is not influenced by variations in quality of the starting product or by variations in manufacturing parameters. The inventive wire cable (12) is used for applications where short cables are required and where their absolute regularity can be made use of. An important field of application of the inventive method is the production of samples for obtaining background data required for optimizing wire cable construction. According to the inventive method, samples of identical basic cable structure but different wire diameters and/or lay lengths of strands, a core wire and/or the cable are produced and the characteristic features of interest are determined. In the tests, different absolute values are found. However, the values in relation to each other show influences of geometry, i.e. wire diameters and lay length modifications. A comparison with samples produced according to conventional manufacturing methods can be used to find correctional variables which can be taken into consideration when required.
Abstract:
A large-sized compound polyurethane elastomer submarine anchor cable to hold steady a offshore platform within a specific range defined by the anchors is comprised of outer layer made of polyurethane elastomer and carbon fiber mixed at a certain ratio, compressed and wrapping around aramid fiber or kelvar fiber or ultra-high-molecular-weight polyethylene (UHMWPE) fiber and a core of synthetic fiber rope with molecular malleability; the rope exposed from both ends of the cable each in a loop; and each loop having one or multiple layers of sheath to wrap around the rope at where closer to a tie on each end.
Abstract:
High strength polyethylene fibers and their applications, for example, chopped fibers, ropes, nets, ballistic materials or items, protective gloves, fiber reinforced concrete products, helmets, and other products obtained therefrom, in which the fiber is characterized in that: it contains a high molecular weight polyethylene consisting essentially of a repeating unit of ethylene; it has an intrinsic viscosity number of 5 or larger and an average strength of 22 cN/dtex or higher; and the measurement of the fiber by differential scanning calorimetry (DSC) exhibits a temperature-increasing DCS curve having at least one endothermic peak over a temperature region of 140° C. to 148° C. (on the low temperature side) and at least one endothermic peak over a temperature region of 148° C. or higher (on the high temperature side) or the number of frictions until the fiber is broken in an abrasion test according to method B for measuring abrasion resistance in the Testing Methods for Spun Yarn (JIS L 1095) is 100,000 or larger.