Abstract:
A process for the preparation of propylene polymer compositions carried out in the presence of a catalyst system comprising (a) a solid catalyst component having average particle size ranging from 15 to 80 μm comprising a magnesium halide, a titanium compound having at least a Ti-halogen bond and at least two electron donor compounds one of which being present in an amount from 50 to 90% by mol with respect to the total amount of donors and selected from succinates and the other being selected from 1,3 diethers, (b) an aluminum alkyl and optionally (c) an external electron donor compound, and comprising the following steps: (i) contacting the catalyst components (a), (b) and optionally (c); (ii) pre-polymerizing up to forming amounts of polymer from about 0.1 up to about 1000 g per gram of solid catalyst component (a); (iii) polymerizing propylene producing a propylene (co)polymer being for at least 85% by weight of insoluble in xylene at 25° C. and (iv) in a successive step, carried out in gas-phase, polymerizing mixtures of ethylene with α-olefins CH2═CHR in which R is a hydrocarbon radical having 1-10 carbon atoms, to produce the said ethylene copolymer.
Abstract:
A propylene composition comprising (percent by weight): A) 60%-90%, of a crystalline propylene copolymer containing from 3.5% to 10% of ethylene derived units and having a melting temperature Tm (measured by DSC on the as-reactor polymer) ranging from 146° to 160°C; B) 10%-40%, of a copolymer of propylene containing from 15% to 30%, of ethylene derived units.
Abstract:
A propylene composition comprising (percent by weight): A) 60%-90%, of a crystalline propylene copolymer containing from 3.5% to 10% of ethylene derived units; B) 10%-40%, of a copolymer of propylene containing from 18.5% to 23.5%, of ethylene derived units.
Abstract:
A masterbatch composition comprising: 70-90 %wt of a component (A) being a propylene homopolymer or copolymer of propylene with ethylene or C 4 -C 10 alpha olefins, having a MFR A according to ISO 1133 (230°C/2.16 Kg) ranging from 15 to 70 g/10 min; and 10-30 %wt of a component B) being a propylene-ethylene copolymer comprising 25-45 %wt of ethylene derived units and having a value of the intrinsic viscosity [η] of the fraction soluble in xylene at room temperature ranging from 5 to 9 dl/g, said masterbatch composition having a total MFR higher than 4 g/10 min, and a value of the fiexural modulus measured according to ISO method 178 ranging from 950 to 2000 MPa.
Abstract:
The present invention provides polyolefin composition comprising a 50-80 wt% of propylene omopolymer or copolymer and a first and a second ethylene/alpha-olefin copolymer, said composition having good stress whitening resistance and gloss, in combination with a good balance of mechanical properties.
Abstract:
Polyolefin composition, comprising in percent by weight: 1) 75-85% of a copolymer of propylene, said copolymer containing up to 15% by weight, of ethylene and/or C 4 -C 10 α-olefin(s) and having a fraction soluble in Xilene at room temperature lower than 6% by weight, and 2) 15-25% of a copolymer of ethylene with one or more C 4 -C 10 α-olefin(s) containing from 10 to 25% by weight of said C 4 -C 10 α-olefin(s); said composition having the value of MFR, measured at 230 °C, 2.16 kg, of less than 2.5 g/10 min, the total content of ethylene of from 14 to 22 % by weight, the total content Of C 4 -C 10 α-olefin(s) of less than 4.5% by weight, the ratio of the total content of ethylene to the total content of C 4 -C 10 α-olefin(s) equal to or higher than 4, the value of the intrinsic viscosity of the total fraction soluble in xylene at room temperature equal to or less than 1.5 dl/g, and the ratio of the amount of component 2) and the amount Of C 4 -C 10 α-olefin(s) in component 2) equal to or higher than 0.80.
Abstract:
Polyolefin compositions, comprising (percent by weight): 1) 55-80% of a homopolymer or copolymer of propylene, said copolymer containing up to 15% of ethylene and/or C4-C10 -olefin(s). 2) 20-45% of a copolymer of ethylene with one or more C4-C10 -olefin(s) containing from 10 to 40% of said C4-C10 -olefin(s); said compositions having values of MFR (230 °C, 2.16 kg) up to 20 g/10 min, a total content of ethylene of 20% or more, a total content of C4-C10 -olefin(s) of 4.5% or more, a ratio of the total content of ethylene to the total content of C4-C10 -olefin(s) of 2.3 or more, a total fract ion soluble in xylene at room temperature of 18 wt% or higher and flexural modulus, referred to the composition as a reactor grade, of more than 700 MPa.