Abstract:
A dispersion having from one to sixty percent by weight of total dispersion of a solids component dispersed in an organic continuous phase is useful as a coating for substrates. The solids component contains 40-95 weight-percent of a polyolefin containing only carbon and hydrogen and that has a number average molecular weight that is greater than 400 gram per mole, 5-40 weight-percent of an amine salt of a functionalized polyolefin; and 0-20 weight-percent of optional additives, wherein weight-percent is based on total weight of solids and wherein the dispersed particles have an average particle size of less than 35 micrometers and the organic phase is a dispersion support medium for the polyolefin and amine salt of a functionalized polyolefin.
Abstract:
The purpose of the present invention is to provide an additive for a solvent-based coating material which has high coating material product stability when added to a solvent-based coating material and whereby the resulting coating film has excellent abrasion resistance. Specifically, the present invention provides a silica composition containing silica coated with a cationic surfactant represented by a specific structure, and also provides a solvent-based coating material composition comprising the silica composition.
Abstract:
Water-borne cross-linking polymeric compositions and related embodiments, such as methods of making and using the compositions, as well as products formed with said compositions are described. For example, the water-borne composition may comprise polymers incorporating cross-linking functionality such as, but not limited to, carbonyl or epoxy functionality, and a blocked cross-linking agent, for example, a hydrazone. The cross-linking functionality does not react with the blocked cross-linking agent; however, the blocked cross-linking agent is capable of reacting with the alternative form cross-linking agent such as, but not limited to, a hydrazide, to yield a cross-linked polymer. The alternative form cross-linking agent may be formed in an equilibrium reaction including the blocked cross-linking agent.
Abstract:
A fire-retardant material comprising from 25 to 50 wt % base oil, from 0.5 to 2.5 wt % polymer, from 0.1 to 1.0 wt % antioxidant, and from 50 to 75 wt % flame retardant.
Abstract:
There is provided a method of producing a polymerizable composition that includes a first polymerizable monomer; and a second polymerizable monomer, a polymer of the second polymerizable monomer, or both, the second polymerizable monomer, the polymer of the second polymerizable monomer, or the both being dispersed in the first polymerizable monomer, the method of producing a polymerizable composition includes dissolving the first polymerizable monomer; the second polymerizable monomer, the polymer of the second polymerizable monomer, or the both in a solvent to obtain a solution in a first step; and evaporating the solvent from the solution in a second step, wherein the first polymerizable monomer is a liquid, and wherein the second polymerizable monomer is a solid.
Abstract:
Disclosed is a eutectic mixture containing a first component and a second component as main components. The first component is a quaternary ammonium salt, and the second component is an aminocarboxylic acid and/or a derivative thereof, the aminocarboxylic acid having a —COOH group and an —NH— group in the same molecule. The eutectic mixture has a melting point, Tm, which is lower than the melting point of the first component, T1, and which is lower than the melting point of the second component, T2. The eutectic mixture is in a homogeneous liquid state at a temperature higher than the melting point, Tm. Disclosed is a liquid composition containing a third component dissolving in the eutectic mixture. The third component contains one or two or more selected from cellulose, hemicellulose, and lignin.
Abstract:
Provided are a binder solution, an electrode mixture, an electrode, and an all-solid-state battery, which use an organic solvent having low reactivity with a solid electrolyte and in which a binder easily dissolves. The binder solution for an all-solid-state battery contains: a binder made of a vinylidene fluoride polymer; and an organic solvent. The organic solvent is at least one selected from the group consisting of a cyclic ether, a ketone, and an ester. The organic solvent has a boiling point of 60° C. or higher and 160° C. or lower. A residual moisture content of the organic solvent is 300 ppm or less.