Method of manufacturing hollow glass product

    公开(公告)号:JP2004238242A

    公开(公告)日:2004-08-26

    申请号:JP2003028395

    申请日:2003-02-05

    Inventor: HASEGAWA TOSHIKI

    CPC classification number: C03B9/32

    Abstract: PROBLEM TO BE SOLVED: To provide a method of manufacturing a hollow glass product free from seam, showing excellent surface gloss and having a recessed part formed on the outside surface by a turn mold blowing method.
    SOLUTION: In the method of blow-molding the hollow product while rotating by introducing parison into a mold on which exhaust holes are formed with a ceratin interval, a non-exhaust part is provided on the mold and the recessed part is formed on the outside surface of the molded product corresponding to the non-exhaust part. The rotation of the parison may be stopped directly before the mold is opened. A carbon mold is desirably used as the mold.
    COPYRIGHT: (C)2004,JPO&NCIPI

    Surface treatment film superior in corrosion-preventive property and lubricity, solution for forming it, and metallic material coated with surface treatment film
    142.
    发明专利
    Surface treatment film superior in corrosion-preventive property and lubricity, solution for forming it, and metallic material coated with surface treatment film 审中-公开
    表面处理膜在腐蚀性物质和润滑剂中的形成及其表面处理溶液和用表面处理膜涂覆的金属材料

    公开(公告)号:JP2004084002A

    公开(公告)日:2004-03-18

    申请号:JP2002247010

    申请日:2002-08-27

    Abstract: PROBLEM TO BE SOLVED: To provide a surface treatment film containing no chromium or lead superior in corrosion-preventive properties and lubricity, and to provide a solution for forming it and a metallic material coated with the surface treatment film.
    SOLUTION: The provided surface treatment film superior in corrosion-preventive properties and lubricity contains a filler with an aspect ratio of 30-17,000, metallic microparticles and a resin as main components, wherein the filler forms a multilayer. The provided solution for forming the surface treatment film with superior corrosion-preventive properties and lubricity, contains each main component dispersed in an organic solvent, and has a viscosity controlled to 10 pa S or lower at ordinary temperature and atmospheric pressure. The provided metallic material has the surface treatment film superior in corrosion-preventive properties and lubricity formed thereon.
    COPYRIGHT: (C)2004,JPO

    Abstract translation: 要解决的问题:提供一种不具有优异的耐腐蚀性和润滑性的铬或铅的表面处理膜,并提供其形成用溶液和涂覆有表面处理膜的金属材料。 解决方案:所提供的耐腐蚀性和润滑性优异的表面处理膜包含纵横比为30-17,000,金属微粒和树脂为主要成分的填料,其中填料形成多层。 用于形成具有优异的防腐性和润滑性的表面处理膜的所提供的溶液包含分散在有机溶剂中的每个主要组分,并且在常温和大气压下具有粘度控制在10paS或更低。 所提供的金属材料具有在其上形成的耐腐蚀性和润滑性优异的表面处理膜。 版权所有(C)2004,JPO

    Method and apparatus for forming glass tumbler with drawn leg

    公开(公告)号:JP2004075473A

    公开(公告)日:2004-03-11

    申请号:JP2002239479

    申请日:2002-08-20

    Inventor: SENOUE MASAKADO

    CPC classification number: C03B9/42 C03B23/0006

    Abstract: PROBLEM TO BE SOLVED: To provide a method and an apparatus for forming glass tumblers with drawn legs, by which the glass tumblers free from seam and each having a long leg part can be efficiently and continuously manufactured.
    SOLUTION: When the glass tumblers are formed by a burn off machine 1, the pedestal part 41 and the moil 42 of each glass product 40 to be shaped, having the moil, are held by a pedestal part holding mechanism 2 and a moil chuck mechanism 3, respectively, and at the same time, the leg part is heated while rotating the chuck mechanism 3 at a constant speed. Then, the pedestal part holding mechanism 2 is raised to extend and form the leg part 43, and thereafter, the moil 42 is cut and removed. In the shaping apparatus, the pedestal part holding mechanisms 2 with respective rotation driving mechanisms and the moil chuck mechanisms 3 are attached to the burn off machine 1, and a burner 4 for heating the leg part is provided at the lower part of each pedestal part holding mechanism 2, and further each pedestal part holding mechanism 2 is made vertically movable in the upward direction, in order to shape the glass tumblers.
    COPYRIGHT: (C)2004,JPO

    3-dimensional measurement inspection method and its system

    公开(公告)号:JP2004061349A

    公开(公告)日:2004-02-26

    申请号:JP2002221214

    申请日:2002-07-30

    Abstract: PROBLEM TO BE SOLVED: To drastically enhance inspection precision and reduce time for 100% inspection by automatically inspecting an opaque object such as pottery products and tiles.
    SOLUTION: An inspection system for inspecting the opaque object comprises: a conveyance device moving at a constant speed; an inspection object which is the opaque object placed on the conveyor device; a laser irradiation means positioned above the object for irradiating the object with a laser beam; a CCD camera disposed opposite to the irradiation means, provided with a three dimensional position measuring means receiving reflection light of the laser beam and having a resolution of not less than 1 million pixels; an image processor converting data acquired by point measurement into image information, a judging means for making comparison with reference form information inputted in advance; and an expelling means for expelling the data which falls out of a dimensional precision of the data of the reference form information.
    COPYRIGHT: (C)2004,JPO

    Flame retardant and flame retardant resin composition
    145.
    发明专利
    Flame retardant and flame retardant resin composition 审中-公开
    阻燃剂和阻燃树脂组合物

    公开(公告)号:JP2003327842A

    公开(公告)日:2003-11-19

    申请号:JP2002134524

    申请日:2002-05-09

    Inventor: ODA TATSUAKI

    Abstract: PROBLEM TO BE SOLVED: To provide a flame retardant imparting a high flame retardancy to a resin while suppressing content of a hydrous metal compound at a reduced amount, and to provide a flame retardant resin composition compounded with the flame retardant.
    SOLUTION: The flame retardant comprises the hydrous metal compound, a nitrate and phosphorus or a phosphorus compound as the component imparting the flame retardancy to the resin. The degradation of the resin compounded with the flame retardant is promoted at a temperature region lower than the starting temperature of burning.
    COPYRIGHT: (C)2004,JPO

    Abstract translation: 要解决的问题:提供一种阻止树脂赋予阻燃性的阻燃剂,同时抑制含水金属化合物的含量减少,并提供与阻燃剂混合的阻燃树脂组合物。 解决方案:阻燃剂包括含水金属化合物,硝酸盐和磷或磷化合物作为赋予树脂阻燃性的成分。 在低于燃烧起始温度的温度区域促进与阻燃剂混合的树脂的降解。 版权所有(C)2004,JPO

    Corrugated fiberboard box structure and method of packaging the same
    146.
    发明专利
    Corrugated fiberboard box structure and method of packaging the same 审中-公开
    CORRUGATED FIBERBOARD BOX结构及其包装方法

    公开(公告)号:JP2003072747A

    公开(公告)日:2003-03-12

    申请号:JP2001265855

    申请日:2001-09-03

    Inventor: YAMADA YASUO

    Abstract: PROBLEM TO BE SOLVED: To propose a corrugated fiberboard box structure and a method of packaging it wherein fastening with bands is not necessary, unpacking is easy, in addition a lid to be put on is not necessary, and a cover lid can be provided if necessary in stacking and packaging corrugated fiberboard box bodies with an upper part opened. SOLUTION: The corrugated fiberboard box structure comprises two inner boxes 21 and 22 having bottom 23 and 24 forms of the same size and upper portions 25 and 26 opened, and an outer box 20 having a bottom 11, side faces 12 and a lid face 13 with such a size that can receive the two inner boxes which are stacked in two stages and equipped with a cutoff portion 16 via cut lines 14 and 15 approximately at the center in a height direction of the side face. A lower half 31 of the outer box and an upper half 32 of the outer box can be used as cover lids C1 and C2 for the respective two inner boxes.

    Abstract translation: 要解决的问题:提出一种瓦楞纸箱结构及其包装方法,其中不需要用带固定,打开包装容易,另外不需要盖上盖子,并且可以提供盖盖,如果 瓦楞纸箱体的堆放和包装必须在上部打开。 解决方案:瓦楞纸箱体结构包括两个具有底部23和24个相同尺寸的形状的内箱21和22以及打开的上部25和26,以及具有底部11,侧面12和盖面13的外箱20 具有这样的尺寸,其可以容纳两个层叠在两个阶段中并且经由切割线14和15大致在侧面的高度方向上的中心配备有切断部分16的内盒。 外箱的下半部31和外箱的上半部32可以用作相应的两个内箱的盖盖C1和C2。

    Manufacturing method of resin containing additive
    147.
    发明专利
    Manufacturing method of resin containing additive 审中-公开
    含有添加剂的树脂的制造方法

    公开(公告)号:JP2003003075A

    公开(公告)日:2003-01-08

    申请号:JP2001188519

    申请日:2001-06-21

    Abstract: PROBLEM TO BE SOLVED: To provide a manufacturing method of a resin containing an additive, a method provided with the manufacturing steps which prevent the agglomeration of the additive and which are safe in the respect of scarcely giving adverse influences to the human body or environment. SOLUTION: Antibacterial glasses having an average particle size of

    Abstract translation: 要解决的问题:为了提供含有添加剂的树脂的制造方法,提供了防止添加剂凝聚并且在几乎不会对人体或环境造成不利影响的情况下是安全的制造步骤的方法。 溶液:将作为添加剂1的平均粒径<5μm的抗菌玻璃添加到作为液体树脂2的聚酯多元醇中,制备浓度为80重量%的添加剂分散液3。 添加剂分散液3与给定比例的聚酰胺树脂一起用挤出机熔融捏合并进行成型步骤,得到母料或树脂的成型产品。 使用聚酰胺作为稀释树脂稀释母料并进行熔融纺丝。 因此,发现纺丝机过滤器部分的压力积聚非常低,抗菌玻璃的分散性优异。

    硫黄系悪臭の消臭剤
    148.
    发明专利

    公开(公告)号:JP2021194124A

    公开(公告)日:2021-12-27

    申请号:JP2020100935

    申请日:2020-06-10

    Abstract: 【課題】硫化水素に対する即効性と、メチルメルカプタンに対する持続性を併せ持つ硫黄系悪臭の消臭剤を提供する。 【解決手段】本発明の硫黄系悪臭の消臭剤は、銅含有ガラスの粉末とZnO粉末とを、2:8〜8:2の質量比で混合したものである。両者の混合により、特にメチルメルカプタンの消臭率につき優れた相乗効果が発揮される。なお、銅含有ガラスが、4〜13モル%のCuOを含有することが好ましい。また、銅含有ガラスが非溶解性ガラスからなることが好ましい。ここでいう非溶解性ガラスとはD 50 =3μmの銅含有ガラスの粉末0.1gを超純水10mlに添加し24時間経過後の溶出量が1000ppm以下であるガラスを指す。 【選択図】図2