Method for manufacturing cooling structure
    153.
    发明专利
    Method for manufacturing cooling structure 有权
    制冷结构的方法

    公开(公告)号:JP2010235978A

    公开(公告)日:2010-10-21

    申请号:JP2009082752

    申请日:2009-03-30

    Abstract: PROBLEM TO BE SOLVED: To provide a method for manufacturing a cooling structure which can improve cooling capability by sufficiently reducing heat resistance between a heat-receiving platform and a cooling pipe.
    SOLUTION: There is provided a cooling pipe (11) in which a cooling medium flows, and the heat-receiving platform (10) which is attached to an object to be cooled and covers the cooling pipe while securing a small clearance between the external surface of the cooling pipe and the heat-receiving platform. The small clearance is sealed with a kneaded material (12) formed by kneading a powder composition with water and/or alcohol.
    COPYRIGHT: (C)2011,JPO&INPIT

    Abstract translation: 解决的问题:提供一种通过充分降低受热平台与冷却管之间的耐热性来提高冷却能力的冷却结构的制造方法。 解决方案:提供冷却介质流动的冷却管道(11),以及附接到待冷却物体的热接收平台(10),同时确保冷却管道之间的小间隙 冷却管的外表面和受热平台。 通过将粉末组合物与水和/或醇捏合而形成的捏合材料(12)密封小间隙。 版权所有(C)2011,JPO&INPIT

    Graphite-containing filler
    154.
    发明专利
    Graphite-containing filler 有权
    含石墨的填料

    公开(公告)号:JP2010235343A

    公开(公告)日:2010-10-21

    申请号:JP2009082766

    申请日:2009-03-30

    Abstract: PROBLEM TO BE SOLVED: To provide a graphite-containing filler which can exhibit superior thermal conductivity while using water and/or alcohol as working liquid. SOLUTION: The graphite-containing filler is prepared by adding water and/or alcohol to a powder composition comprising: graphite of ≥80 mass%; amorphous carbon having an average particle size smaller than that of the graphite of ≥0.1 mass%; and a water-soluble polymer of ≥1 mass%. COPYRIGHT: (C)2011,JPO&INPIT

    Abstract translation: 要解决的问题:提供一种在使用水和/或醇作为工作液体的情况下可以表现出优异的导热性的含石墨的填料。 解决方案:含石墨的填料是通过向粉末组合物中加入水和/或醇制备的,该组合物包括:≥80质量%的石墨; 平均粒径小于石墨质量≥0.1质量%的无定形碳; 和≥1质量%的水溶性聚合物。 版权所有(C)2011,JPO&INPIT

    Aqueous spray material for hot repair
    155.
    发明专利
    Aqueous spray material for hot repair 审中-公开
    水性修补材料

    公开(公告)号:JP2010235340A

    公开(公告)日:2010-10-21

    申请号:JP2009082737

    申请日:2009-03-30

    Abstract: PROBLEM TO BE SOLVED: To provide an aqueous spray material for hot repair which hardly causes effluence of a carbonaceous resin upon spraying although the carbonaceous resin is included as a substance for forming carbon bond in hot process, and hardly strips a spray worked product. SOLUTION: The aqueous spray material for hot repair comprises refractory aggregate and the carbonaceous resin, wherein a part of the carbonaceous resin is compounded in such a form as to form granulated matter together with powder to be granulated and the remaining part is compounded in the form of powder without forming the granulated matter. COPYRIGHT: (C)2011,JPO&INPIT

    Abstract translation: 待解决的问题:为了提供一种用于热修复的水性喷涂材料,其在喷涂中几乎不引起碳质树脂的流出,尽管碳热树脂作为热加工中形成碳键的物质被包括在内,几乎不会喷涂加工 产品。 解决方案:用于热修复的水性喷涂材料包括耐火骨料和碳质树脂,其中一部分碳质树脂以形成颗粒状的形式与待造粒的粉末一起混合,剩余部分复合 以粉末的形式,而不形成颗粒状物质。 版权所有(C)2011,JPO&INPIT

    Method for using sliding nozzle device
    156.
    发明专利
    Method for using sliding nozzle device 有权
    使用滑动喷嘴装置的方法

    公开(公告)号:JP2010234421A

    公开(公告)日:2010-10-21

    申请号:JP2009086230

    申请日:2009-03-31

    Abstract: PROBLEM TO BE SOLVED: To provide a method for using a sliding nozzle by which life of a plate can be increased. SOLUTION: In the method for using the sliding nozzle device which uses a plate obtained from a refractory raw material composition containing a zirconia mullite raw material and/or an alumina zirconia raw material, sliding velocity V (m/h) of the plate of the sliding nozzle device is preobtained, and the plate in which ZrO 2 content Z (mass%) satisfies expression (1) with respect to the sliding velocity V (m/h) of the plate is used. In addition, the sliding velocity V (m/h) of the plate is made to satisfy expression (2) with respect to the ZrO 2 content Z (mass%) in the plate. Z≥(V-0.3)/0.158...(1), V≤0.158Z+0.3... (2). COPYRIGHT: (C)2011,JPO&INPIT

    Abstract translation: 要解决的问题:提供一种使用能够增加板的寿命的滑动喷嘴的方法。 解决方案:在使用由含有氧化锆莫来石原料和/或氧化铝氧化锆原料的耐火材料组合物获得的板的滑动喷嘴装置的使用方法中,滑动速度V(m / h) 预先获得滑动喷嘴装置的板,并且相对于板的滑动速度V(m / h),ZrO 2 / Sb含量Z(质量%)满足表达式(1)的板是 用过的。 此外,使板的滑动速度V(m / h)相对于板中的ZrO 2 S 2含量Z(质量%)满足表达式(2)。 Z≥(V-0.3)/0.158 ...(1),V≤0.158Z+ 0.3 ...(2)。 版权所有(C)2011,JPO&INPIT

    Immersion nozzle for continuous casting and method for designing the same
    157.
    发明专利
    Immersion nozzle for continuous casting and method for designing the same 审中-公开
    用于连续铸造的浸入式喷嘴及其设计方法

    公开(公告)号:JP2010221277A

    公开(公告)日:2010-10-07

    申请号:JP2009072492

    申请日:2009-03-24

    Abstract: PROBLEM TO BE SOLVED: To provide an immersion nozzle having a structure of blowing a gas from the inner wall to the inner hole of the nozzle, in which the blowing amount of the gas on the cross-sectional face in a gas-blowing region can be uniformized or intentionally changed so as to increase the effect for the prevention of the sticking of inclusions or the like to the inner wall.
    SOLUTION: In the immersion nozzle 10 for continuous casting, a permeable refractory 2 is arranged at a part of the inner wall facing the inner hole 1 to be a molten steel flow passage, and a gas is blown from the permeable refractory 2 to the inner hole 1, a first hollow chamber 4 is provided at the outer circumferential side of the permeable refractory 2, separately from the first hollow chamber 4, a second hollow chamber 5 is provided in a hardly permeable refractory having permeability relatively lower than that of the permeable refractory, the first hollow chamber 4 and the second hollow chamber 5 are communicated by a plurality of through-holes 6 between the hollow chambers, and further, the second hollow chamber 5 and a gas feed port 7 are communicated by a gas feed passage 8.
    COPYRIGHT: (C)2011,JPO&INPIT

    Abstract translation: 要解决的问题:提供一种具有从内壁吹送气体到喷嘴内孔的结构的浸入式喷嘴,其中,气体喷射管的横截面上的气体的吹送量, 吹风区域可以均匀化或有意地改变,从而增加了防止夹杂物等粘附到内壁上的效果。 解决方案:在用于连续铸造的浸入式喷嘴10中,在面向内孔1的内壁的一部分处设置可渗透耐火材料2作为钢水流道,并且从可渗透耐火材料2吹出气体 在内孔1中,与第一中空室4分开地,在可渗透耐火物2的外周侧设置有第一中空室4,第二中空室5设置在难渗透性耐火材料中,其耐渗透性相对低于 的第一中空室4和第二中空室5通过中空室之间的多个通孔6连通,另外,第二中空室5和气体供给口7通过气体连通 饲料通道8.版权所有(C)2011,JPO&INPIT

    Fixed joint-filling material
    158.
    发明专利
    Fixed joint-filling material 有权
    固定接头材料

    公开(公告)号:JP2010207894A

    公开(公告)日:2010-09-24

    申请号:JP2009058371

    申请日:2009-03-11

    Abstract: PROBLEM TO BE SOLVED: To provide a fixed joint-filling material which can exactly shield an air infiltration passage.
    SOLUTION: The fixed joint-filling material 10 has a shape in which a sheet material is formed so as to be the shape of a reverse truncated cone. The reduced-diameter part side in the fixed joint-filling material 10 is an inner hole near part 10a near the inner hole so as to be the flow passage of a molten metal, and is made thicker than the other part. Further, the cross-section of the fixed joint-filling material 10 has a taper shape in which thickness gradually reduces from the inner hole near part 10a toward the outer circumferential edge part 10b so as to be the reduced-diameter part side. Provided that the thickness of the edge face on the inner hole near part 10a in which the thickness is made the maximum in the fixed joint-filling material is defined as A and the thickness of the edge face on the outer circumferential edge part 10b in which the thickness is made the minimum in the fixed joint-filling material 10 is defined as B, A×(1-the compression rate of the fixed joint-filling material 10)≤B is satisfied.
    COPYRIGHT: (C)2010,JPO&INPIT

    Abstract translation: 要解决的问题:提供可以精确地遮蔽空气渗透通道的固定的接头填充材料。 解决方案:固定接头填充材料10具有形成为倒圆锥体形状的片材的形状。 固定接头填充材料10中的缩径部侧是靠近内孔的靠近10a的内孔,作为熔融金属的流动通道,并且比其他部分更厚。 此外,固定接头填充材料10的截面具有锥形形状,其中厚度从靠近部分10a的内孔朝向外周边缘部分10b逐渐减小,从而成为缩径部分侧。 假设在固定接头填充材料中厚度达到最大值的部分10a附近的内孔上的边缘面的厚度被定义为A和外周边缘部10b上的边缘面的厚度,其中 固定接头填充材料10中的厚度最小限定为B,满足A×(1-固定接头填充材料10的压缩率)≤B。 版权所有(C)2010,JPO&INPIT

    Immersion nozzle for continuous casting
    159.
    发明专利
    Immersion nozzle for continuous casting 有权
    连铸喷嘴

    公开(公告)号:JP2010207844A

    公开(公告)日:2010-09-24

    申请号:JP2009055525

    申请日:2009-03-09

    Abstract: PROBLEM TO BE SOLVED: To provide an immersion nozzle for continuous casting capable of suppressing local erosion of a fire resistant material for supplying gas and of uniformly stably carrying out blow-in of an inert gas in a circumferential direction.
    SOLUTION: The immersion nozzle 10 for continuous casting carries out flow control of molten steel from a tundish by a stopper 12 arranged at an inlet 11 for molten steel flow formed of the fire resistant material for supplying gas and charges the molten steel in a molten steel passage 13 from a discharge port 14 to a mold while blowing the inert gas into the molten steel from the fire resistant material for supplying gas. When the inner diameter D of the molten steel passage below a position P abutting on the stopper 12 and at the height position of the discharging port 14 is made to be D, at least a part of a working surface 17 within a range R where a length H from the upper end position T1 of the inlet 11 for the molten steel flow to the below is 40 mm or more and (1.1×D+78) mm or less is formed of the fire resistant material for supplying gas, and a fire resistant material 18 for preventing errosion is arranged at a part of the working surface 17 within the range R below the position P abutting on the stopper 12.
    COPYRIGHT: (C)2010,JPO&INPIT

    Abstract translation: 要解决的问题:提供一种能够抑制用于供给气体的耐火材料的局部腐蚀并且均匀地稳定地在圆周方向上进行惰性气体吹入的连续铸造用浸渍喷嘴。 解决方案:用于连续铸造的浸入式喷嘴10通过设置在用于供应气体的耐火材料形成的钢水流入口11处的塞子12从中间包进行钢水的流量控制,并将钢水充入 从用于供给气体的耐火材料吹入惰性气体进入钢水的从出料口14到模具的钢水通道13。 当钢水通道的低于位于止动件12上的位置P和排出口14的高度位置的内径D为D时,工作表面17的至少一部分在R的范围内,其中a 从用于钢水流入口的入口11的上端位置T1的长度H为40mm以上,并且由用于供给气体的耐火材料形成(1.1×D + 78)mm以下, 在工件表面17的一部分上,在与止动件12邻接的位置P下方的范围R内布置防止磨损的耐磨材料18.(C)2010,JPO&INPIT