BRITTLE OXIDE SUBSTRATES STRENGTHENED BY CROSS-LINKABLE SILANES
    11.
    发明申请
    BRITTLE OXIDE SUBSTRATES STRENGTHENED BY CROSS-LINKABLE SILANES 审中-公开
    可交联硅烷增强的稀土氧化物基体

    公开(公告)号:WO1995000259A2

    公开(公告)日:1995-01-05

    申请号:PCT/US1994007034

    申请日:1994-06-21

    CPC classification number: C03C17/30

    Abstract: A method is described for strengthening or restoring strength to a brittle oxide substrate which includes the steps of coating the brittle oxide substrate with an aqueous solution containing a silane-based composition, and curing the coating to form a transparent layer on the brittle oxide substrate. Also disclosed are novel compositions used to coat brittle oxide substrates, and silane-coated brittle oxide containers.

    Abstract translation: 描述了一种强化或恢复脆性氧化物衬底的强度的方法,该方法包括以下步骤:用含有硅烷类组合物的水溶液涂覆脆性氧化物衬底,并固化该涂层以在脆性氧化物衬底上形成透明层。 还公开了用于涂覆脆性氧化物衬底和硅烷涂覆的脆性氧化物容器的新型组合物。

    COATED GLASS ARTICLE
    12.
    发明申请
    COATED GLASS ARTICLE 审中-公开
    涂层玻璃制品

    公开(公告)号:WO1993012934A1

    公开(公告)日:1993-07-08

    申请号:PCT/US1992010874

    申请日:1992-12-21

    Abstract: A coated-glass article is prepared by the chemical-vapor deposition of a mixture of a tin oxide precursor, a silicon dioxide precursor and an accelerant such as triethyl phosphite at deposition rates higher than 350 ANGSTROM /sec. onto glass having a temperature from 450 to 650 DEG C. The layer of material deposited can be combined with other layers to produce an article with specific properties such as controlled emissivity, refractive index, abrasion resistance, or appearance.

    Abstract translation: 通过以高于350安培/秒的沉积速率通过化学气相沉积氧化锡前体,二氧化硅前体和促进剂如亚磷酸三乙酯的混合物来制备涂覆玻璃制品。 放置在450至650℃的玻璃上。沉积的材料层可以与其他层结合,以产生具有特定性质如受控发射率,折射率,耐磨性或外观的制品。