기포 안정성이 향상된 점착제 조성물 및 그의 제조방법
    15.
    发明公开
    기포 안정성이 향상된 점착제 조성물 및 그의 제조방법 有权
    具有改进的泡沫稳定性的胶粘组合物及其制造方法

    公开(公告)号:KR1020130142284A

    公开(公告)日:2013-12-30

    申请号:KR1020120065365

    申请日:2012-06-19

    Abstract: The present invention provides an adhesive composition including: a copolymer which is polymerized with 5-50 wt% of polar functional group-containing monomers with respect to 100 wt% of (meta)acrylic acid ester monomers; and hollow glass fillers or bubbles. Moreover, a manufacturing method of the adhesive composition includes: a step of preparing a copolymer by polymerizing 5-50 wt% of polar functional group-containing monomers with respect to 100 wt% of (meta) acrylic acid ester monomers, a step of preparing a mixture by adding a surfactant, a photoinitiator, and a photocuring agent to the copolymers, and a step of adding hollow glass fillers or injecting gas bubbles into the mixture. [Reference numerals] (AA) Example 1;(BB) Comparative example 1

    Abstract translation: 本发明提供了一种粘合剂组合物,其包含:相对于100重量%的(甲基)丙烯酸酯单体与5-50重量%的含极性官能团的单体聚合的共聚物; 和中空玻璃填料或气泡。 此外,粘合剂组合物的制造方法包括:相对于100重量%的(甲基)丙烯酸酯单体聚合5-50重量%的含极性官能团的单体制备共聚物的步骤,制备 通过向共聚物中添加表面活性剂,光引发剂和光固化剂的混合物,以及向混合物中添加中空玻璃填料或注入气泡的步骤。 (附图标记)(AA)实施例1;(BB)比较例1

    기포 안정성이 향상된 난연용 점착제 조성물 및 그의 제조방법
    18.
    发明公开
    기포 안정성이 향상된 난연용 점착제 조성물 및 그의 제조방법 有权
    具有改进的泡沫稳定性的火焰复合胶粘剂组合物及其制造方法

    公开(公告)号:KR1020140008007A

    公开(公告)日:2014-01-21

    申请号:KR1020120074864

    申请日:2012-07-10

    Abstract: Provided is an adhesive composition which comprises: a copolymer prepared by polymerizing 10-50 parts by weight of polar functional group-containing monomers with 100 parts by weight of (meth)acrylic acid ester-based monomers; a heat conductive inorganic filler; and a hollow glass filler or foams. Provided is a method for manufacturing the adhesive composition, which comprises the steps of: manufacturing the copolymer by polymerizing 10-50 parts by weight of the polar functional group-containing monomers with 100 parts by weight of the (meth)acrylic acid ester-based monomers; manufacturing a mixture by adding the heat conductive inorganic filler, a surfactant, a photoinitiator, and a photo hardener to the copolymer; and adding the hollow glass filler or injecting foams to the mixture. [Reference numerals] (AA) Example 1; (BB) Comparative example 1

    Abstract translation: 提供一种粘合剂组合物,其包含:通过使10-50重量份的含极性官能团的单体与100重量份的(甲基)丙烯酸酯类单体聚合而制备的共聚物; 导热无机填料; 和中空玻璃填料或泡沫。 提供了一种粘合剂组合物的制造方法,其包括以下步骤:通过将10-50重量份的含极性官能团的单体与100重量份的(甲基)丙烯酸酯系 单体; 通过向共聚物中加入导热性无机填料,表面活性剂,光引发剂和光硬化剂来制造混合物; 并加入中空玻璃填料或将泡沫注入混合物。 (标号)(AA)实施例1; (BB)比较例1