公开(公告)号:KR1020130101375A
公开(公告)日:2013-09-13
申请号:KR1020120022480
申请日:2012-03-05
Applicant: 주식회사에스티엑스종합기술원 , 서울대학교산학협력단
IPC: H01M4/139 , H01M4/36 , H01M4/64 , H01M10/052
CPC classification number: H01M4/1391 , H01M4/0404 , H01M4/0471 , H01M4/131 , H01M4/1395 , H01M4/505 , H01M4/525 , H01M4/661 , H01M10/052 , Y02E60/12
Abstract: PURPOSE: A manufacturing method of an electrode is provided to reduce the internal resistance between a metal current collector and an electrode active material through two heat treatment processes and to improve the output performance of an electrode by improving electrochemical stability in an electrode material. CONSTITUTION: A manufacturing method of an electrode for a lithium secondary battery comprises a step of manufacturing a slurry mixture by mixing an active material powder, a binder powder, and a conducting powder; a step of making the mixture penetrate into the inner pores of metal foam, conducting a first heat treatment, and forming an electrode layer; a step of a pressing the electrode layer; and a step of conducting a second heat treatment under a reduction atmosphere. [Reference numerals] (S1) Step of manufacturing a slurry mixture by mixing an active material powder, a binder powder, and a conducting powder; (S2) Step of producing a electrode layer by first heating processing after penetrating the mixture of the S1 step inside a gap of the foaming metal; (S3) Step of pressuring the electrode layer produces in the S2 step; (S4) Step of conducting a second heat treatment of the electrode layer produced in the S3 step under a reduction atmosphere
Abstract translation: 目的:提供电极的制造方法,以通过两个热处理工艺来减小金属集电体和电极活性材料之间的内部电阻,并且通过提高电极材料中的电化学稳定性来提高电极的输出性能。 构成:锂二次电池用电极的制造方法包括通过混合活性物质粉末,粘合剂粉末和导电粉末来制造浆料混合物的步骤; 使混合物渗透到金属泡沫的内部孔中,进行第一次热处理,形成电极层的工序; 按压电极层的步骤; 以及在还原气氛下进行第二次热处理的工序。 (S1)通过混合活性物质粉末,粘合剂粉末和导电粉末制造浆料混合物的步骤; (S2)通过在发泡金属的间隙内贯穿S1阶段的混合物之后的第一加热处理来制造电极层的工序; (S3)在S2步骤中产生加压电极层的工序; (S4)在还原气氛下在S3步骤中制造的电极层进行第二次热处理的步骤