    Abstract: 본발명은리튬-공기전지용공기극및 그제조방법에관한것으로, 보다구체적으로는리튬-공기전지용공기극에있어서, Ni 폼(foam) 상에스피넬결정구조를갖고, 나노크기의직경을갖으며, 지지체없이독립적으로서있는 MnCoO나노막대들(nanorod arrays)을포함하는것을특징으로하고, 리튬-공기전지용공기극의제조방법에있어서, 황산망간, 아세트산코발트및 요소를포함하는전구체용액을준비하는단계; 상기전구체용액에 Ni 폼(foam)을넣고수열반응을통해 Ni 폼(foam) 상에프리스탠딩(free-standing) 전구체나노막대들을형성하는단계; 상기프리스탠딩전구체나노막대들이형성된 Ni 폼(foam)을열처리하여 Ni 폼(foam) 상에프리스탠딩 MnCoO스피넬의나노막대들을제조하는단계를포함하는것을특징으로한다.

    Abstract translation: 涉及一种空气电池的空气电极和在空气电池的空气电极制造方法,并且更具体地euroneun锂发明锂的方法,具有在Ni泡沫(泡沫)尖晶石晶体结构,是具有纳米尺寸的直径,没有支撑 该方法包括一种制造空气电池的空气电极,制备前体溶液含有硫酸锰,乙酸钴和元素的方法 - 其特征在于,它包括在一个独立的(纳米棒阵列)的MnCoO纳米棒,和锂; 包括:在通过水热反应前体溶液镍泡沫插入物(泡沫),以形成一个独立的(自由站立)在Ni泡沫前体纳米棒(泡沫); 通过热处理所述自由站立的前体纳米棒的Ni泡沫形成(泡沫)的特征在于,它包括用于在镍泡沫(泡沫)制造自支撑棒MnCoO尖晶石的步骤。

    리튬 이온 전지용 게르마늄-탄소 복합체 전극 및 그 제조방법

    公开(公告)号:KR1020170058539A

    公开(公告)日:2017-05-29

    申请号:KR1020150162222

    申请日:2015-11-19

    Abstract: 본발명은리튬이온전지용게르마늄-탄소복합체전극및 그제조방법에관한것으로, 보다구체적으로는리튬이온전지용게르마늄-탄소복합체전극에있어서, 게르마늄나노입자의표면을둘러싸는탄소층; 상기전극의표면및 내부에서사방으로다량형성되는나노직경의 3차원기공들을포함하는것을특징으로하고, 리튬이온전지용게르마늄-탄소복합체전극의제조방법에있어서, 졸-겔법을이용하여이산화게르마늄(GeO) 나노입자를제조하는단계; 상기이산화게르마늄(GeO) 나노입자를액상기지에서 PVP와혼합하는단계; 상기혼합물을건조하여 PVP 고상기지에이산화게르마늄(GeO) 나노입자가분산된상태인 GeO/PVP를만드는단계; 상기 GeO/PVP를열탄소분해환원시켜 3차원다공성나노구조를갖는게르마늄-탄소복합체인 3D-Ge/C를만드는단계를포함하는것을특징으로한다.

    2차 전지용 내압 측정 장치
    15.
    发明授权
    2차 전지용 내압 측정 장치 有权
    二次电池内压测量设备

    公开(公告)号:KR101029518B1

    公开(公告)日:2011-04-25

    申请号:KR1020090008075

    申请日:2009-02-02

    Abstract: 본 발명은 2차 전지용 내압 측정 장치에 관한 것으로, 보다 자세하게는 2차 전지를 충·방전을 하는 동안 발생하는 2차 전지 내부의 전지 내압을 측정할 수 있는 2차 전지용 내압 측정 장치에 관한 것이다.
    2차 전지, 내압, 충방전, 내압 측정

    수소저장합금의 표면 특성 개량 방법
    16.
    发明授权
    수소저장합금의 표면 특성 개량 방법 失效
    氢储存合金表面改性方法

    公开(公告)号:KR100871903B1

    公开(公告)日:2008-12-05

    申请号:KR1020070040825

    申请日:2007-04-26

    Abstract: 본 발명은 Ni-MH 2차 전지의 음극용 수소저장합금의 표면 처리 방법에 관한 것으로 수소저장합금의 분말을 알칼리 수세화 처리한 후, 산성 무전해 구리 도금 또는 산성 무전해 니켈 도금 처리하여 Ni-MH 2차 전지의 음극 재료로 이용되는 수소저장합금의 초기 활성화뿐만 아니라 싸이클 수명, 방전용량 및 충·방전 효율을 개선한 수소저장합금의 표면 처리방법을 제시하는 수소저장합금의 표면 특성 개량 방법에 관한 것이다.
    Ni-MH 2차 전지, 수소저장합금, 알칼리 수세화 처리, 산성 무전해 구리 도금, 산성 무전해 니켈 도금

    수소저장합금의 표면 특성 개량 방법
    17.
    发明公开
    수소저장합금의 표면 특성 개량 방법 失效
    氢储存合金表面改性方法

    公开(公告)号:KR1020080096013A

    公开(公告)日:2008-10-30

    申请号:KR1020070040825

    申请日:2007-04-26

    Abstract: A method for surface modification of hydrogen storage alloy for improving the initial activation of hydrogen storage alloy used as the cathode material of an Ni-MH secondary battery, the cycle life, and the discharge capacity and charge and discharge efficiency thereof. A method for surface modification of hydrogen storage alloy is comprises the following steps; a step preparing for the hydrogen storage alloyed powder(100); a step for selecting the hydrogen storage alloy powder to the constant size(200); a step for dipping and alkaline washing the selected hydrogen storage alloy powder in the alkaline solution(300); and a step performing the acidity electroless plating the hydrogen storage alloyed powder after alkaline washing(400).

    Abstract translation: 用于改善用作Ni-MH二次电池的阴极材料的储氢合金的初始活化的储氢合金的表面改性方法,循环寿命及其放电容量及其充放电效率。 储氢合金的表面改性方法包括以下步骤: 制备储氢合金粉末(100)的步骤; 将储氢合金粉末选择为恒定尺寸(200)的步骤; 在碱性溶液(300)中浸渍和碱洗所选择的储氢合金粉末的步骤; 以及在碱性洗涤后对储氢合金粉末进行酸性化学镀的步骤(400)。

    환원제를 포함하는 알칼리 수용액을 이용한 수소저장합금표면 개질 방법
    20.
    发明公开
    환원제를 포함하는 알칼리 수용액을 이용한 수소저장합금표면 개질 방법 失效
    通过使用碱性溶液进行表面改性的储氢合金的方法,包括减少

    公开(公告)号:KR1020090070909A

    公开(公告)日:2009-07-01

    申请号:KR1020070139073

    申请日:2007-12-27

    Abstract: A method for surface modification of hydrogen storage alloy through alkali soaking using an alkaline solution including reductant is provided to elute the components except for nickel from the surface of hydrogen storage alloy powder and form catalyst bed on the surface of hydrogen storage alloy, thereby improving discharge capacitance and lifetime. A method for surface modification of hydrogen storage alloy comprises a step(S100) of preparing hydrogen storage alloy powder, a step(S200) of selecting the hydrogen storage alloy powder of specific size, a step(S300) of alkali-soaking the selected hydrogen storage alloy powder by dipping it in an alkaline solution including reductant, and a step(S400) of washing and drying the treated hydrogen storage alloy powder.

    Abstract translation: 提供一种通过使用包含还原剂的碱性溶液的碱浸渍对储氢合金进行表面改性的方法,从储氢合金粉末表面除去除镍以外的组分,并在储氢合金表面形成催化剂床,从而改善放电 电容和寿命。 储氢合金的表面改性方法包括制备储氢合金粉末的步骤(S100),选择特定尺寸的储氢合金粉末的步骤(S200),将选择的氢气碱浸渍的步骤(S300) 将其浸渍在包含还原剂的碱性溶液中的储存合金粉末和洗涤和干燥处理过的储氢合金粉末的步骤(S400)。