公开(公告)号:KR1020130088669A
公开(公告)日:2013-08-08
申请号:KR1020120010054
申请日:2012-01-31
Applicant: 전자부품연구원
IPC: H01M4/1391 , H01M4/525 , H01M4/505 , H01M10/052
CPC classification number: H01M4/485 , C01G45/1228 , C01G51/50 , C01G53/50 , C01P2002/52 , C01P2002/72 , C01P2004/03 , C01P2004/61 , C01P2006/12 , C01P2006/14 , C01P2006/40 , H01M4/505 , H01M4/525 , H01M10/052
Abstract: PURPOSE: A manufacturing method of an anode active material is provided to mass produce the anode active material which has high surface porosity, and uniform composition and particle size, and capable of adjusting a particle size and a shape of the anode material. CONSTITUTION: A manufacturing method of an anode active material for a lithium secondary battery comprises: a step of manufacturing a metal salt solution which includes a lithium source, a manganese source, a nickel source and cobalt source; a step of manufacturing a slurry by performing a wet grinding of the metal salt solution at 2000-6000 rpm for 2-12 hours with using a beads in which a particle diameter is 0.05-0.30 mm; a step of adding a carbon source in the slurry; a step of manufacturing s mixed powder by drying with spraying the slurry; a step of heat-treating the mixed powder. [Reference numerals] (AA) Voltage [V]; (BB) Capacity [mAh]
Abstract translation: 目的:提供阳极活性材料的制造方法,以大量生产具有高表面孔隙率,均匀组成和粒度的阳极活性材料,并且能够调节阳极材料的粒度和形状。 构成:锂二次电池用负极活性物质的制造方法包括:制造包含锂源,锰源,镍源和钴源的金属盐溶液的工序; 通过使用粒径为0.05〜0.30mm的珠子,以2000〜6000rpm对金属盐溶液进行2〜12小时的湿磨,制造浆料的工序; 在浆料中添加碳源的步骤; 通过喷雾浆料干燥制造混合粉末的步骤; 对该混合粉末进行热处理的工序。 (标号)(AA)电压[V]; (BB)容量[mAh]
-
公开(公告)号:KR101920485B1
公开(公告)日:2018-11-21
申请号:KR1020110097059
申请日:2011-09-26
Applicant: 전자부품연구원
IPC: H01M4/525 , H01M4/505 , H01M4/1391 , H01M10/052
CPC classification number: H01M4/131 , B82Y30/00 , C01G53/00 , C01G53/006 , C01G53/44 , C01G53/50 , C01P2002/52 , C01P2004/03 , C01P2004/32 , C01P2004/62 , C01P2004/64 , C01P2006/40 , H01M4/483 , H01M4/505 , H01M4/523 , H01M4/525 , H01M4/54 , H01M10/052 , H01M10/0525 , H01M2004/021 , H01M2004/028 , Y02E60/122 , Y02P70/54
Abstract: 리튬이차전지용전구체, 이를포함하는양극활물질, 이의제조방법및 상기양극활물질을포함하는리튬이차전지에관한것으로, 더욱상세하게는두께가약 1 내지약 30nm인판상형플레이트(plate)를가지며, 하기화학식 1로표시되는전구체를제공한다. [화학식 1] NiCoMnM(OH)(0
-