산성광산배수를 이용한 철코팅 모래의 제조방법 및 이를이용한 중금속 함유 수 처리방법
    11.
    发明公开
    산성광산배수를 이용한 철코팅 모래의 제조방법 및 이를이용한 중금속 함유 수 처리방법 失效
    通过使用酸性矿物排放制备铁皮涂层的方法和使用铁包覆砂处理含重金属的水的方法

    公开(公告)号:KR1020090077386A

    公开(公告)日:2009-07-15

    申请号:KR1020080003312

    申请日:2008-01-11

    CPC classification number: Y02W10/15 C02F11/10 C02F9/00 C02F2103/10 Y02W10/20

    Abstract: A method of manufacturing iron oxide coated sand using acid mine drainage and a method of treating heavy metal-containing water using the iron oxide coated sand are provided to economically reuse drainage containing contaminants and effectively remove arsenic presenting in contaminated water using the manufactured iron oxide coated sand. A method of manufacturing iron oxide coated sand using acid mine drainage comprises the steps of: obtaining the inorganic precipitant only after forming an inorganic precipitant by adding an alkali salt to acid mine drainage; mixing the inorganic precipitant with sand to prepare a slurry; heating the slurry at 60 to 550 deg.C for one hour to three days to coat sand with the inorganic precipitant; and removing the inorganic precipitant that has not been coated on sand, and washing and drying the iron oxide coated sand.

    Abstract translation: 提供使用酸性矿井排水制造氧化铁涂层砂的方法和使用氧化铁涂覆的砂处理含重金属的水的方法,以经济地再利用含有污染物的排水,并使用所制造的氧化铁涂层有效地去除污染水中的砷 砂。 使用酸性矿井排水制造氧化铁涂层砂的方法包括以下步骤:仅在通过向酸性矿井排水中加入碱金属形成无机沉淀剂后获得无机沉淀剂; 将无机沉淀剂与砂混合以制备浆料; 在60〜550℃下加热浆料1小时〜3天,用无机沉淀剂涂覆沙子; 并且除去未被涂覆在砂上的无机沉淀剂,以及洗涤和干燥氧化铁涂覆的砂。

Patent Agency Ranking