公开(公告)号:CA2480281C
公开(公告)日:2009-10-20
申请号:CA2480281
申请日:2003-05-06
Applicant: ATI PROPERTIES INC
Inventor: CAO WEI-DI
Abstract: A nickel-base alloy includes, in weight percent, up to about 0.10 percent carbon; about 12 up to about 20 percent chromium; up to about 4 percent molybdenum; up to about 6 percent tungsten, wherein the sum of molybdenum and tungsten is at least about 2 percent and not more than about 8 percent; about 5 up to about 12 percent cobalt; up to about 14 percent iron; about 4 percent up to about 8 percent niobium; about 0.6 percent up to about 2.6 percent aluminum; about 0.4 percent up to about 1.4 percent titanium; about 0.003 percent up to about 0.03 percent phosphorous; about 0.003 percent up to about 0.015 percent boron; nickel; and incidental impurities. The sum of atomic percent aluminum and atomic percent titanium is from about 2 to about 6 percent, the ratio of atomic percent aluminum to atomic percent titanium is at least about 1.5, and the atomic percent of aluminum plus titanium divided by the atomic percent of niobium equals about 0.8 to about 1.3. The nickel-base alloy may be provided in the form of an article of manufacture, such as, for example, a disk, a blade, a fastener, a case, or a shaft. A method for making a nickel-base alloy also is disclosed. It is emphasized that this abstract is provided to comply with the rules requiring an abstract that will allow a searcher or other reader to quickly ascertain the subject matter of the technical disclosure. It is submitted with the understanding that it will not be used to interpret or limit the scope or meaning of the claims.
-
公开(公告)号:DE602004015325D1
公开(公告)日:2008-09-04
申请号:DE602004015325
申请日:2004-08-17
Applicant: ATI PROPERTIES INC
Inventor: CAO WEI-DI
Abstract: A precipitation hardenable martensitic stainless steel that includes, in percent by weight, 11.0 to 12.5 percent chromium, 1.0 to 2.5 percent molybdenum, 0.15 to 0.5 percent titanium, 0.7 to 1.5 percent aluminum, 0.5 to 2.5 percent copper, 9.0 to 11.0 percent nickel, up to 0.02 percent carbon, up to 2.0 percent tungsten, and up to 0.001 percent boron. Articles formed from the stainless steel and methods of forming the same are also disclosed.
-
公开(公告)号:AU2006324147A1
公开(公告)日:2007-08-02
申请号:AU2006324147
申请日:2006-05-09
Applicant: ATI PROPERTIES INC
Inventor: KENNEDY RICHARD L , CAO WEI-DI
IPC: C22F1/10
-
公开(公告)号:AU2014237609A1
公开(公告)日:2015-04-09
申请号:AU2014237609
申请日:2014-03-07
Applicant: ATI PROPERTIES INC
Inventor: FORBES JONES ROBIN M , KENNEDY RICHARD L , CAO WEI-DI
Abstract: A method of processing an alloy workpiece to reduce thermal cracking may comprise spraying a metallic coating material onto at least a portion of a surface of the alloy workpiece to form a surface coating metallurgically bonded to the alloy workpiece. The surface coating may be more ductile than the alloy workpiece and reduces heat loss from the alloy workpiece.
-
公开(公告)号:AU2006324147A8
公开(公告)日:2009-01-22
申请号:AU2006324147
申请日:2006-05-09
Applicant: ATI PROPERTIES INC
Inventor: KENNEDY RICHARD L , CAO WEI-DI
IPC: C22F1/10
-
公开(公告)号:AT402273T
公开(公告)日:2008-08-15
申请号:AT04821341
申请日:2004-08-17
Applicant: ATI PROPERTIES INC
Inventor: CAO WEI-DI
Abstract: A precipitation hardenable martensitic stainless steel that includes, in percent by weight, 11.0 to 12.5 percent chromium, 1.0 to 2.5 percent molybdenum, 0.15 to 0.5 percent titanium, 0.7 to 1.5 percent aluminum, 0.5 to 2.5 percent copper, 9.0 to 11.0 percent nickel, up to 0.02 percent carbon, up to 2.0 percent tungsten, and up to 0.001 percent boron. Articles formed from the stainless steel and methods of forming the same are also disclosed.
-
公开(公告)号:ZA201502056B
公开(公告)日:2016-01-27
申请号:ZA201502056
申请日:2015-03-25
Applicant: ATI PROPERTIES INC
Inventor: KENNEDY RICHARD L , CAO WEI-DI , FORBES JONES ROBIN M
Abstract: A method of processing an alloy workpiece to reduce thermal cracking comprises inserting the alloy workpiece into a metallic canister, wherein the metallic canister has a lower coefficient of thermal expansion than the alloy workpiece and includes an inner surface comprising a nickel-boron coating on at least a portion of the inner surface, encapsulating the alloy workpiece in the metallic canister to provide a canned assembly, removing at least a portion of gas from the interior of the canned assembly, and heating the canned assembly to transient liquid phase bond the alloy workpiece to the metallic canister.
-
公开(公告)号:AU2006324147B2
公开(公告)日:2011-05-12
申请号:AU2006324147
申请日:2006-05-09
Applicant: ATI PROPERTIES INC
Inventor: KENNEDY RICHARD L , CAO WEI-DI
IPC: C22F1/10
-
公开(公告)号:AU2003234486B2
公开(公告)日:2010-04-01
申请号:AU2003234486
申请日:2003-05-06
Applicant: ATI PROPERTIES INC
Inventor: CAO WEI-DI
Abstract: A nickel-base alloy includes, in weight percent, up to about 0.10 percent carbon; about 12 up to about 20 percent chromium; up to about 4 percent molybdenum; up to about 6 percent tungsten, wherein the sum of molybdenum and tungsten is at least about 2 percent and not more than about 8 percent; about 5 up to about 12 percent cobalt; up to about 14 percent iron; about 4 percent up to about 8 percent niobium; about 0.6 percent up to about 2.6 percent aluminum; about 0.4 percent up to about 1.4 percent titanium; about 0.003 percent up to about 0.03 percent phosphorous; about 0.003 percent up to about 0.015 percent boron; nickel; and incidental impurities. The sum of atomic percent aluminum and atomic percent titanium is from about 2 to about 6 percent, the ratio of atomic percent aluminum to atomic percent titanium is at least about 1.5, and the atomic percent of aluminum plus titanium divided by the atomic percent of niobium equals about 0.8 to about 1.3. The nickel-base alloy may be provided in the form of an article of manufacture, such as, for example, a disk, a blade, a fastener, a case, or a shaft. A method for making a nickel-base alloy also is disclosed. It is emphasized that this abstract is provided to comply with the rules requiring an abstract that will allow a searcher or other reader to quickly ascertain the subject matter of the technical disclosure. It is submitted with the understanding that it will not be used to interpret or limit the scope or meaning of the claims.
-
公开(公告)号:BRPI0415106A
公开(公告)日:2006-11-28
申请号:BRPI0415106
申请日:2004-09-28
Applicant: ATI PROPERTIES INC
Inventor: CAO WEI-DI , KENNEDY RICHARD L
Abstract: The present invention relates to a method of heat treating a nickel-base alloy, the nickel-base alloy comprising, in percent by weight, up to 0.1 carbon, from 12 to 20 chromium, up to 4 molybdenum, up to 6 tungsten, from 5 to 12 cobalt, up to 14 iron, from 4 to 8 niobium, from 0.6 to 2.6 aluminium, from 0.4 to 1.4 titanium, from 0.003 to 0.03 phosphorus, from 0.003 to 0.015 boron, balance nickel and incidental impurities; wherein a sum of the weight percent of molybdenum and the weight percent of tungsten is at least 2 and not more than 8, and wherein a sum of atomic percent aluminium and atomic percent titanium is from 2 to 6, a ratio of atomic percent aluminium to atomic percent titanium is at least 1.5, and the sum of atomic percent aluminium and atomic percent titanium divided by atomic percent niobium is from 0.8 to 1.3, the method comprising: solution treating the nickel-base alloy for no greater than 4 hours at a solution temperature ranging from 940°C (1725°F) to 1010°C (1850°F), cooling the nickel-base alloy at a first cooling rate after solution treating the nickel-base alloy, aging the solution treated nickel-base alloy in a first aging treatment for no greater than 8 hours at a temperature ranging from 740°C (1365°F) to 788°C (1450°F), and aging the nickel-base alloy in a second aging treatment for at least 8 hours at a second aging temperature, the second aging temperature ranging from 621°C (1150°F) to 704°C (1300°F).
-
-
-
-
-
-
-
-
-