Abstract:
Thermoplastic molding compositions comprising A) from 10 to 93% by weight of a thermoplastic polyester B) from 1 to 20% by weight of a phosphinic salt C) from 1 to 20% by weight of a nitrogen-containing flame retardant D) from 5 to 50% by weight of a long-fiber reinforcing material with fiber length from 2 to 25 mm and L/D ratio from 500 to 4000 E) from 0 to 50% by weight of other additives, where the total of the percentages by weight of components A) to E) is 100%.
Abstract:
A composition has at least one polyarylene (ether) sulfone, semi-aromatic polyamide, aluminum phosphate, and acid scavenger. The composition may further include at least one compatibilizer, fibrous or particulate filler, impact modifier, or auxiliary. The compositions can form a fiber, film, foam, or shaped article. The composition also has 20 to 80% by weight of the polyarylene (ether) sulfone. The polyarylene (ether) sulfone has at most 0.05% by weight of phenolic end groups.
Abstract:
Thermoplastic molding compositions comprising a thermoplastic polyester, a poly(ε-caprolactone), a biodegradable polyester differing from the poly(ε-caprolactone), a phosphinic salt and a polar modified polyolefin wax prepared by means of metallocene catalysts, the use of the thermoplastic molding compositions for the production of flame-retardant moldings of any type, to the resultant moldings, and to the use of the polar modified polyolefin wax prepared by means of metallocene catalysts for an improvement of the flame retardancy of thermoplastic molding compositions comprising a thermoplastic polyester.
Abstract:
Disclosed herein is a thermoplastic molding composition which includes A) from 10 to 99.9% by weight of a thermoplastic polyamide, B) from 0.1 to 20% by weight of at least one hyperbranched polyester having an acid number in the range of from 10 to 700 mg KOH/g and a hydroxyl number in the range of from 0 to 550 mg KOH/g, C) from 0 to 50% by weight of fibrous or particulate fillers, and D) from 0 to 45% by weight of further additives, where the total of the percentages by weight of components A) to D) is 100% by weight.
Abstract:
The present invention relates to a process for producing a shaped body, wherein, in step i), a layer of a sinter powder (SP) comprising at least one mineral flame retardant inter alia is provided and, in step ii), the layer provided in step i) is exposed. The present invention further relates to a process for producing a sinter powder (SP) and to a sinter powder (SP) obtainable by this process. The present invention also relates to the use of the sinter powder (SP) in a sintering process and to shaped bodies obtainable by the process of the invention.
Abstract:
A thermoplastic molding composition is disclosed. The thermoplastic molding composition includes A) from 20 to 96.9% by weight of a thermoplastic polyamide, B) from 1 to 20% by weight of an inorganic phosphinate salt, C) from 1 to 15% by weight of an organic phosphinate salt, D) from 1 to 15% by weight of melamine cyanurate, E) from 0.1 to 10% by weight of a polyvinylpyrrolidone homopolymer, and F) from 0 to 50% by weight of other additives. The total of the percentages by weight of A) to F) is 100%.
Abstract:
The invention relates to thermoplastic molding compositions comprising A) from 10 to 97% by weight of a thermoplastic polyester B) from 1 to 20% by weight of a phosphinic salt C) from 1 to 20% by weight of a nitrogen-containing flame retardant D) from 0.5 to 30% by weight of a dicarboxylic salt of the formula where R1 to R4 are mutually independently halogen or hydrogen, with the proviso that at least one moiety R1 to R4 is halogen, x=from 1 to 3 m=from 1 to 9 n=from 2 to 3 M=alkaline earth metal, Ni, Ce, Fe, In, Ga, Al, Pb, Y, Zn, Hg E) from 0 to 50% by weight of other additives, where the total of the percentages by weight of components A) to E) gives 100%.
Abstract:
The invention relates to thermoplastic molding compositions comprising A) from 10 to 97% by weight of a thermoplastic polyester B) from 1 to 20% by weight of a phosphinic salt C) from 1 to 20% by weight of a nitrogen-containing flame retardant D) from 0.5 to 30% by weight of a dicarboxylic salt of the formula where R1 to R4 are mutually independently halogen or hydrogen, with the proviso that at least one moiety R1 to R4 is halogen, x=from 1 to 3 m=from 1 to 9 n=from 2 to 3 M=alkaline earth metal, Ni, Ce, Fe, In, Ga, Al, Pb, Y, Zn, Hg E) from 0 to 50% by weight of other additives, where the total of the percentages by weight of components A) to E) gives 100%.
Abstract:
Thermoplastic molding compositions comprising A) from 10 to 99.8% by weight of a thermoplastic polyamide, B) from 0.1 to 60% by weight of red phosphorus, C) from 0.05 to 5% by weight of a catalyst comprising copper and zinc and support material, D) from 0 to 40% by weight of an impact modifier, E) from 0 to 60% by weight of further additives, where the total of the percentages by weight of A) to E) is 100%.
Abstract:
The present invention relates to the use of aromatic P—N-compounds in flame retardant polymer compositions. These compositions are especially useful for the manufacture of flame retardant compositions based onthermoplastic polymers, especially polyolefin homo- and copolymers, polycondensates, such as polyamines or polyesters and duroplastic polymers, such as polyepoxides.