WAXING COMPOUND COMPOSITION FOR AUTOMOBILE AND ITS PREPARATION

    公开(公告)号:JPH01225681A

    公开(公告)日:1989-09-08

    申请号:JP5074488

    申请日:1988-03-04

    Applicant: KAO CORP

    Abstract: PURPOSE:To obtain the title composition excellent in water repellency, storage stability, etc., by mixing a solid wax, a di(long-chain alkyl) quaternary ammonium salt, a polyoxyethylenealkylamine, and a polyhydric alcohol in specified weight proportions, and solubilizing the mixture. CONSTITUTION:10-16.5wt% solid wax (e.g., a paraffin wax) is mixed with 5-8wt.% di(long-chain alkyl) quaternary ammonium salt (e.g., distearyldimethylammonium chloride) and 0.5-3.5wt.% polyoxyethylenealkyl amine. After the mixture is uniformly melted at 85 deg.C or higher, 2-15wt.% polyhydric alcohol (e.g., ethylene glycol) is added thereto. The obtained mixture is cooled to 62.5-70 deg.C, and warm water of 62.5-70 deg.C is slowly added thereto to solubilize the solid wax, thus giving a waxing compound composition for an automobile.