A METHOD FOR PRODUCING A MULTILAYER MACHINE GLAZED PAPER COMPRISING HIGHLY REFINED CELLULOSE FIBERS AND A MULTILAYER MACHINE GLAZED PAPER PRODUCED

    公开(公告)号:CA3190646A1

    公开(公告)日:2022-03-10

    申请号:CA3190646

    申请日:2021-08-31

    Applicant: STORA ENSO OYJ

    Abstract: The present invention relates to a method for manufacturing a multilayer machine glazed paper comprising highly refined cellulose fibers, the method comprising the steps of: forming a first wet web by applying at least one first pulp suspension comprising highly refined cellulose fibers on a first wire; partially dewatering the first wet web to obtain a first partially dewatered web; forming a second wet web by applying at least one second pulp suspension comprising highly refined cellulose fibers on a second wire; partially dewatering the second wet web to obtain a second partially dewatered web; joining the first and second partially dewatered web to obtain a multilayer web; optional dewatering the multilayer web in a dewatering unit, and glazing the multilayer web in at least one glazing unit to obtain a multilayer machine glazed paper comprising highly refined cellulose fibers. The invention also relates to a multiply MG paper produced according to the method.

    Multilayer film comprising mfc
    13.
    发明专利

    公开(公告)号:SE2051029A1

    公开(公告)日:2022-03-02

    申请号:SE2051029

    申请日:2020-09-01

    Applicant: STORA ENSO OYJ

    Abstract: The present invention relates to a method for manufacturing a multilayer film comprising microfibrillated cellulose (MFC) in a paper-making machine, the method comprising the steps of:a) forming a bottom web layer by applying a first pulp suspension comprising at least 50% by dry weight of cellulose based fibrous material having an SR (Schopper-Riegler) value in the range of 18-75 on a bottom web wire;b) forming or applying an intermediate web layer formed from a second pulp suspension comprising at least 50% by dry weight of MFC having an SR value in the range of 80-100 on the bottom web layer;c) applying a top web layer formed from a third pulp suspension comprising at least 50% by dry weight of cellulose based fibrous material having an SR (Schopper-Riegler) value in the range of 18-75 on the intermediate web layer to form a multilayer web; andd) dewatering, and optionally drying, the formed multilayer web to obtain a multilayer film comprising MFC.