Improvements to metal wires used for reinforcing elastomeric material
    241.
    发明公开
    Improvements to metal wires used for reinforcing elastomeric material 失效
    Metalldrähte,die zur Armierung von Elastomermaterial verwendet werden。

    公开(公告)号:EP0283738A1

    公开(公告)日:1988-09-28

    申请号:EP88102594.4

    申请日:1988-02-23

    Inventor: Van Ooij, Wim J.

    Abstract: The invention concerns a metal wire, used to produce reinforcing elements for articles of elastomeric material, which is provided with a coating able to ensure at the same time a good resistance to corrosion, good values of initial adhesion and a low decay, due to ageing, of the bond with the elastomeric material, said coating being formed by two concentric layers of a Zn/Ni alloy, where the radially inner layer contains Zn in an amount ranging between 60% and 90% on the layer total and the radially outer layer contains Ni in an amount ranging between 60% and 80% on the layer total.

    Abstract translation: 本发明涉及一种用于生产弹性体材料用增强元件的金属丝,其具有能够同时确保良好的耐腐蚀性,良好的初始粘合值和较低衰变的涂层,由于老化 与弹性体材料的结合,所述涂层由Zn / Ni合金的两个同心层形成,其中径向内层在层总数和径向外层上含有介于60%和90%之间的Zn 含有总量为60%至80%之间的Ni。

    접착력이 향상된 타이어용 스틸코드
    243.
    发明公开
    접착력이 향상된 타이어용 스틸코드 有权
    具有改进的橡胶附属性的轮胎钢丝绳

    公开(公告)号:KR1020080073845A

    公开(公告)日:2008-08-12

    申请号:KR1020070012554

    申请日:2007-02-07

    Inventor: 최용제 김민안

    Abstract: A steel cord for a tire with the enhanced adhesion force is provided to put coating solution on the surface of a wet-type fiber and to have the stable rubber coverage. A compound selected from a group consisting of 97% of 4-carboxybenzaldehyde or 98% of anthranilonitrile is coated on the surface of the wet type cord plated by brass. The compound is melted by the wet type lubricating solution of 1-50 mol% and then the wet type cord plated by brass is impregnated into the solution for 15-80 seconds and dried, so that the steel cord for a tire is manufactured. The steel cord is used as a reinforcing member of the tire. The concentration of the melting solution is 1-50 mol% preferably. In the manufacturing processes, a sample piece is manufactured and the adhesion force of the sample piece and the erosion resistance property are evaluated.

    Abstract translation: 提供具有增强的粘附力的用于轮胎的钢丝帘线,以将涂布溶液涂布在湿式纤维的表面上并具有稳定的橡胶覆盖。 选自97%的4-羧基苯甲醛或98%的邻氨基苯腈的化合物涂覆在用黄铜镀覆的湿式帘线的表面上。 该化合物通过1-50mol%的湿式润滑溶液熔化,然后将用黄铜镀覆的湿式帘线浸渍在溶液中15-80秒,并干燥,制成轮胎用钢丝帘线。 钢帘线用作轮胎的加强构件。 熔融溶液的浓度优选为1-50mol%。 在制造过程中,制造样品片,评价样品的粘附力和耐侵蚀性。

    PC 강연선의 방청 피막 형성 방법
    244.
    发明授权
    PC 강연선의 방청 피막 형성 방법 有权
    在预应力条件下形成腐蚀保护涂层的方法

    公开(公告)号:KR100563113B1

    公开(公告)日:2006-03-27

    申请号:KR1020040010684

    申请日:2004-02-18

    Abstract: 종래 기술에서는, PC 강연선(鋼撚線)에 요구되고 있는 유연성과, 콘크리트와의 부착 강도를 손상하지 않도록 하여 인장(引張) 피로 특성의 향상을 도모하도록 하고, 또한 피막의 손상에 의한 소지(素地)의 노출을 방지하기 위해 표층부(외주면)에 두꺼운 피막을 형성하는 것이다.
    PC 강연선의 방청(corrosion protection) 피막 2중 결합 구조 형성 가공 방법은 PC 강연선을, 되풀기 측선을 심선(心線)으로부터 느슨하게 풀어 소지 조정을 하는 전처리 공정과, 이 전처리 공정 후에 심선에 대하여 측선을 꼬아 합쳐 느슨하게 닫고, 꼬아 합치는 것에 의한 나선형 홈부를 제외한 표층부에 합성 수지 분체(粉體) 도료를 도포하는 동시에 가열하여 부착시키고, 그 후 냉각하여 표층부에만 수지 피막을 형성하는 1차 도장 공정과, 이 1차 도장 공정 후에, PC 강연선의 측선을 심선으로부터 느슨하게 풀고, 심선 조정 수단을 경유하여, 느슨하게 풀린 상태에 있는 심선 및 측선의 각각 외주면에 합성 수지 분체 도료를 도포하는 동시에 가열하여 균등하게 부착시킨 후에 냉각하고, 측선에서 일부가 2중의 결합 피막이 되는 각각 단독 상태의 수지 피막을 형성하는 2차 도장 공정과, 이 2차 도장 공정 후에, 상기 2중의 결합 피막 부분이 연선의 표층부에 위치하도록 심선에 대하여 측선을 원래의 상태로 꼬아 합치는 공정으로 이루어지는 것이며, 유연성 및 콘크리트 부착 강도의 특성을 저해하지 않고, 특수 구조물로서 피막 손상의 우려가 드러나는 외표면을 보호하기 위해, 두꺼운 2중의 결합 피막을 용이하게 형성할 수 있다.
    PC 강연선, 표층부, 심선, 측선, 나선형 홈부.

    고무접착성이 우수한 스틸 타이어코드
    245.
    发明授权
    고무접착성이 우수한 스틸 타이어코드 失效
    钢轮胎帘线具有优异的橡胶粘合性能

    公开(公告)号:KR100291467B1

    公开(公告)日:2001-05-15

    申请号:KR1019990017993

    申请日:1999-05-19

    Inventor: 김홍기

    Abstract: 본발명은타이어의보강재로사용되는스틸타이어코드의고무접착성개선에관한것이다. 본발명은, 표면도금층이형성된여러가닥의스틸와이어가꼬여져구성된스틸타이어코드에있어서, 상기스틸와이어는그 표면에황동도금층이와이어 1Kg당 1 ∼8g 의범위로부착되고, 황동도금층위에코발트도금층이와이어 1Kg당 0.1 ∼ 1.0g의범위로부착되며, 다시코발트도금층위로구리도금층이와이어 1Kg당 0.1 ∼ 1.0g의범위로부착된 3중층의도금층으로이루어진데에기술적특징이있다. 본발명은스틸타이어코드를구성하는스틸와이어의표면에황동도금층과코발트도금층및 구리도금층이순차피복되어구성됨으로써종래의스틸타이어코드에비해초기접착성의저하됨이없이향상된경시접착력특성을나타내어종래의황동도금또는 3원합금도금스틸코드에비해타이어의보강용으로사용시타이어의수명을연장시키는효과가기대되고있다.

    고무접착성이 우수한 스틸 타이어코드
    246.
    发明公开
    고무접착성이 우수한 스틸 타이어코드 失效
    钢丝绳优良的橡胶胶粘性

    公开(公告)号:KR1020000074219A

    公开(公告)日:2000-12-15

    申请号:KR1019990017993

    申请日:1999-05-19

    Inventor: 김홍기

    Abstract: PURPOSE: Provided is steel tire cord comprising twisted steel wires, which is used for a reinforcement of a tire and improved a rubber adhesive property. CONSTITUTION: The surface of the steel wire comprises triple plating layers: 1-8 g (based on the steel wire of 1 Kg) of a brass plating layer; 0.1-1.0 g (based on the steel wire of 1 Kg) of a cobalt plating layer on the brass plating layer; 0.1-1.0 g (based on the steel wire of 1 Kg) of a copper plating layer on the cobalt plating layer.

    Abstract translation: 目的:提供包括扭绞钢丝的钢轮胎帘线,其用于加强轮胎并提高橡胶粘合性能。 构成:钢丝的表面包括三层镀层:1-8g(基于1Kg的钢丝)黄铜镀层; 在黄铜镀层上0.1-1.0g(基于钢丝1Kg)钴镀层; 在钴镀层上0.1-1.0g(基于1Kg的钢丝)镀铜层。

    이중 방청 PC 강연선
    247.
    发明公开
    이중 방청 PC 강연선 有权
    双重防爆PC条

    公开(公告)号:KR1020130115974A

    公开(公告)日:2013-10-22

    申请号:KR1020120103254

    申请日:2012-09-18

    Abstract: PURPOSE: A double rustproof PC strand is provided to adjust a core wire and a side wire in different diameter thicknesses determined for each wire and to improve durability as the strand has a double rustproof structure in which a synthetic resin film is formed on a plating layer. CONSTITUTION: A double rustproof PC strand is a PC strand which has been through a rustproof treatment by forming a synthetic resin film on an outer circumference surface. Each strand (1) of a core wire and a side wire which compose the PC strand is the strand in which a plating layer (2) is formed by conducting wired drawing and a plating treatment, which is twisted after adjusting under a wired diameter adjusting condition of (A)-(C), and which has tensile strength exceeding 1850N/mm^2. The wire diameter adjusting conditions are as follows; (A) 4.42±0.05 mm of the core wire diameter and 4.25±0.05 mm of the side wire diameter; (B) 5.22±0.05 mm of the core wire diameter and 5.06±0.05 mm of the side wire diameter, or (C) 5.40±0.05 mm of the core wire diameter and 5.25±0.05 mm of the side wire diameter.

    Abstract translation: 目的:提供双防锈PC绞线,用于调整每根导线确定的不同直径厚度的芯线和侧线,并提高耐久性,因为绞线具有双层防锈结构,其中在镀层上形成合成树脂膜 。 构成:双防锈PC股是通过在外周面上形成合成树脂膜而进行防锈处理的PC股。 构成PC绞合线的芯线和侧线的每个绞合线(1)是通过进行布线拉伸和电镀处理而形成镀层(2)的绞合线,其在有线直径调节 (A) - (C)的条件,拉伸强度超过1850N / mm ^ 2。 线径调整条件如下: (A)芯线直径为4.42±0.05mm,侧线直径为4.25±0.05mm; (B)芯线直径为5.22±0.05mm,侧线直径为5.06±0.05mm,或(C)芯线直径为5.40±0.05mm,侧线直径为5.25±0.05mm。

    PC 강연선의 방청 피막 형성 방법
    250.
    发明公开
    PC 강연선의 방청 피막 형성 방법 有权
    通过在形成涂层涂层之后形成芯线和侧线上的双重腐蚀保护涂层和执行喷砂工艺,形成预定混凝土条的腐蚀保护涂层的方法

    公开(公告)号:KR1020040077470A

    公开(公告)日:2004-09-04

    申请号:KR1020040010684

    申请日:2004-02-18

    Abstract: PURPOSE: A method of forming corrosion protection coating on prestressed concrete strand by forming double corrosion protection coating on a core wire and side wires and performing a blasting process after formation of plating coating is provided to achieve improved adhesion of resin coating to plating coating and corrosion protection performance of resin coating. CONSTITUTION: A method comprises a step of forming a plating coating(12) on the outer surface of an element wire(11); a step of wire drawing the element wire where the plating coating is formed; a step of forming a prestressed concrete strand constituted by core wire and side wires, by twisting and combining element wires; a step of temporarily unwinding the prestressed concrete strand, and performing a blasting process on the core and side wires; a step of forming resin coating on the outer surfaces of the blasted core and side wires; and a step of cooling the resin coating, and re-twisting and combining the prestressed concrete strand.

    Abstract translation: 目的:通过在芯线和侧线上形成双重防腐涂层并在形成镀层后进行喷砂处理,提供预应力混凝土桁架上防腐蚀涂层的方法,以提高树脂涂层对镀层和腐蚀的粘附性 树脂涂层的保护性能。 构成:一种方法包括在元件线(11)的外表面上形成镀覆层(12)的步骤; 对形成有镀覆层的元件线进行拉丝的工序; 通过扭转和组合元件线形成由芯线和侧线构成的预应力混凝土线的步骤; 暂时退绕预应力混凝土桁条,对芯线和侧线执行喷砂处理的步骤; 在喷丸芯和侧线的外表面上形成树脂涂层的步骤; 以及冷却树脂涂层的步骤,并且将预应力混凝土绞线进行再加捻和组合。