생화학분해성 기화성 방청필름 제조방법
    276.
    发明公开
    생화학분해성 기화성 방청필름 제조방법 有权
    可生物降解的挥发性腐蚀抑制剂薄膜制造方法

    公开(公告)号:KR1020100011081A

    公开(公告)日:2010-02-03

    申请号:KR1020080072138

    申请日:2008-07-24

    Applicant: (주)선우팩

    Abstract: PURPOSE: A biodegradable volatile corrosion inhibitor film is provided to prevent the corrosion of iron or nonferrous metal, to enable fast degradation during a biodegradable process, and to prevent the generation of harmful materials. CONSTITUTION: A method for preparing a biodegradable volatile corrosion inhibitor film comprises: a first mixing step(S10) for mixing sodium benzoate, benzotriazole, dextrin and gelatin to form a first mixture; a pulverization step(S20) for pulverizing the first mixture; a second mixing step(S30) for mixing metal with thermal conductivity of at least 200 Kcal/mhr°C and polyethylene wax with the first mixture to form a second mixture; a third mixing step(S40) for mixing a polyethylene resin with a second mixture to form a third mixture; and an extrusion step(S50) for extruding the third mixture through a film extruder.

    Abstract translation: 目的:提供可生物降解的挥发性腐蚀抑制剂膜,以防止铁或有色金属的腐蚀,从而在生物降解过程中能够快速降解,并防止产生有害物质。 构成:制备可生物降解的挥发性腐蚀抑制剂膜的方法包括:将苯甲酸钠,苯并三唑,糊精和明胶混合以形成第一混合物的第一混合步骤(S10) 粉碎步骤(S20),用于粉碎第一混合物; 第二混合步骤(S30),用于将具有至少200Kcal / mhr℃的导热性的金属和聚乙烯蜡与第一混合物混合以形成第二混合物; 第三混合步骤(S40),用于将聚乙烯树脂与第二混合物混合以形成第三混合物; 以及挤出步骤(S50),用于通过膜挤出机挤出第三混合物。

    칼 보관대
    279.
    发明授权
    칼 보관대 失效
    杀死案例

    公开(公告)号:KR100814989B1

    公开(公告)日:2008-03-18

    申请号:KR1020070049045

    申请日:2007-05-21

    Applicant: 김해자

    Inventor: 김해자

    Abstract: A knife case is provided to allow a user to insert knives regardless of the direction by holding the inserted knives using many sticks and to sterilize knives and sticks in the knife case by installing an ultraviolet lamp operated by a timer at the bottom of the knife case. A knife case comprises a box type body(10), sticks(20), a transmission plate(40), an ultraviolet lamp(30), and a timer. The top of the box type body is open. The box type body is full of a large number of the sticks. The sticks are loaded on the transmission plate. The ultraviolet lamp is installed under the transmission plate in the box. The timer is installed under the transmission plate to turn on the ultraviolet lamp from time to time. An assembly hole is formed at the lower part of the box type body to house the ultraviolet lamp. The ultraviolet lamp is attached to a bracket(32) installed to cover the assembly hole.

    Abstract translation: 提供刀盒以允许使用者通过使用许多棒夹住插入的刀来插入刀,并且通过在刀盒的底部安装由定时器操作的紫外灯来对刀盒中的刀和棒进行消毒 。 刀盒包括箱型主体(10),棒(20),传输板(40),紫外灯(30)和定时器。 盒型身体的顶部是开放的。 盒子身体里充满了大量的棒子。 棒装在传动板上。 紫外灯安装在箱内的传输板下面。 定时器安装在传输板下面,以不时地打开紫外线灯。 在盒型主体的下部形成组装孔以容纳紫外线灯。 紫外线灯被安装到安装以覆盖组装孔的支架(32)上。

    난연성 열가소성 폴리카보네이트 조성물, 그의 용도 및제조 방법
    280.
    发明公开
    난연성 열가소성 폴리카보네이트 조성물, 그의 용도 및제조 방법 无效
    阻燃剂热塑性聚碳酸酯组合物,用途及其制造方法

    公开(公告)号:KR1020060050281A

    公开(公告)日:2006-05-19

    申请号:KR1020050071888

    申请日:2005-08-05

    Abstract: 우수한 물성을 갖는 난연성 열가소성 조성물은 폴리카보네이트 수지 약 20 내지 약 90 중량%; 충격 개질제 약 35중량% 이하; 폴리다이메틸실록세인 단위 약 8 내지 약 30중량% 또는 다른 등몰량의 다이오가노실록세인 단위를 포함하는 폴리실록세인-폴리카보네이트 공중합체 약 0.5 내지 약 30중량%; 및 인-함유 난연제 약 0.5 내지 약 20중량%(상기 각 중량%는 충전제를 제외한 열가소성 조성물의 전체 조합 중량 기준임)을 포함한다. 한 실시양태에서 2.5 mm(±10%) 두께를 갖는 열가소성 조성물의 샘플은 UL94 5VA 등급을 달성한다. 더 얇은 샘플도 또한 상기 등급을 달성할 수 있다. 상기 조성물은 난연성 얇은-벽 제품을 형성하는데 유용하다.

    Abstract translation: 具有优异物理性能的阻燃热塑性组合物包含约20至约90重量%的聚碳酸酯树脂; 至多约35重量%的抗冲改性剂; 约0.5至约30重量%的聚硅氧烷 - 聚碳酸酯共聚物,其包含约8至约30重量%的聚二甲基硅氧烷单元或等摩尔量的其它二有机硅氧烷单元; 和约0.5至约20重量%的含磷阻燃剂,各自基于热塑性组合物的总组合重量,不包括任何填料。 在一个实施方案中,厚度为2.5mm(±10%)的热塑性组合物的样品达到UL94 5VA等级稀释剂样品也可达到该等级。 该组合物可用于形成阻燃薄壁制品。