Heat sink used by electronic apparatus, and its manufacturing method
    21.
    发明专利
    Heat sink used by electronic apparatus, and its manufacturing method 有权
    电子设备使用的散热器及其制造方法

    公开(公告)号:JP2007035985A

    公开(公告)日:2007-02-08

    申请号:JP2005218248

    申请日:2005-07-28

    Abstract: PROBLEM TO BE SOLVED: To provide a heat sink and its method for manufacturing, in which no problem due to thermal distortion occurs even if an electronic part having different thermal expansion coefficient and a heat dissipation member are jointed, because heat generated from electronic parts such as semiconductors etc. is diffused more efficiently than before.
    SOLUTION: In a heatsink for semiconductor devices, the thermal expansion coefficient of the opposed faces are different, and further, the thermal expansion coefficient of one face is 4-14×10
    -6 /K, and that of another face is 10-24×10
    -6 /K.
    COPYRIGHT: (C)2007,JPO&INPIT

    Abstract translation: 要解决的问题:提供一种散热器及其制造方法,其中即使将具有不同热膨胀系数的电子部件和散热构件接合,也不会发生由于热变形引起的问题,因为由 电子部件如半导体等比以前更有效地扩散。 解决方案:在半导体器件的散热器中,相对面的热膨胀系数不同,一面的热膨胀系数为4-14×10 -6 / K ,另一面为10-24×10 -6 / K。 版权所有(C)2007,JPO&INPIT

    Injection molding machine
    22.
    发明专利
    Injection molding machine 审中-公开
    注塑机

    公开(公告)号:JP2005144992A

    公开(公告)日:2005-06-09

    申请号:JP2003389247

    申请日:2003-11-19

    Abstract: PROBLEM TO BE SOLVED: To provide an injection molding machine which is excellent in the durability of a screw, even if molding is performed by using a resin material containing a glass fiber and an antistatic material.
    SOLUTION: Each component of the screw is coated with a lower layer, an intermediate layer and an upper layer. The lower layer is formed as a CrN membrane. The intermediate layer on the lower layer is formed as an inclined composite membrane of CrN and TiN, wherein in terms of a ratio of mixing of CrN and TiN, a CrN content is made higher and a TiN content is made lower toward the lower layer, and the CrN content is made lower and the TiN content is made higher toward the upper layer. The upper layer on the intermediate layer is formed as a TiN membrane.
    COPYRIGHT: (C)2005,JPO&NCIPI

    Abstract translation: 要解决的问题:即使使用含有玻璃纤维和抗静电材料的树脂材料进行成型,也提供一种螺杆的耐久性优异的注塑机。 解决方案:螺杆的每个部件都涂覆有下层,中间层和上层。 下层形成为CrN膜。 下层的中间层形成为CrN和TiN的倾斜复合膜,其中,以CrN与TiN的混合比例,CrN含量越高,TiN含量越低, 使CrN含量降低,使TiN含量向上层高。 中间层上的上层形成为TiN膜。 版权所有(C)2005,JPO&NCIPI

    Hard film having excellent wear resistance and oxidation resistance, and product obtained by using the film
    24.
    发明专利
    Hard film having excellent wear resistance and oxidation resistance, and product obtained by using the film 审中-公开
    具有优异耐磨性和耐氧化性的硬膜,以及使用电影获得的产品

    公开(公告)号:JP2004162105A

    公开(公告)日:2004-06-10

    申请号:JP2002328225

    申请日:2002-11-12

    Abstract: PROBLEM TO BE SOLVED: To provide a hard film which has excellent wear resistance and oxidation resistance.
    SOLUTION: The hard film is provided with: a surface layer consisting of a complex compound composed of one or more kinds of metallic elements selected from the group consisting of the group 4A, 5A and 6A elements in the Periodic Table, Si and one or more kinds of elements selected from the group consisting of N, C and B, or a mixture of the complex compounds; a layer directly above a base metal surface composed of one or more kinds of metallic elements selected from the group consisting of the 4A, 5A and 6A elements in the Periodic Table, and one or more kinds of elements selected from N, C and B, or a mixture of the complex compounds; and an intermediate layer with a gradient coating or a stacked structure consisting of the complex compound or the mixture of the complex compounds composing the surface layer and the layer directly above the base metal surface.
    COPYRIGHT: (C)2004,JPO

    Abstract translation: 要解决的问题:提供具有优异的耐磨性和抗氧化性的硬膜。 解决方案:硬膜设置有:由由周期表中的4A,5A和6A族元素组成的组中的一种或多种金属元素组成的络合物组成的表面层,Si和 选自N,C和B的一种或多种元素,或该配合物的混合物; 由选自元素周期表中的4A,5A和6A元素的一种或多种金属元素组成的贱金属表面上方的层以及选自N,C和B中的一种或多种元素, 或复合化合物的混合物; 以及由复合化合物或构成表面层的复合化合物和直接在母材表面上方的层的混合物组成的梯度涂层或层叠结构的中间层。 版权所有(C)2004,JPO

    ブレーキ用焼結摩擦材
    26.
    发明专利

    公开(公告)号:JP2018150532A

    公开(公告)日:2018-09-27

    申请号:JP2018046328

    申请日:2018-03-14

    CPC classification number: C09K3/14 C22C1/05 C22C19/03 C22C27/04 F16D69/02

    Abstract: 【課題】高い摩擦係数を有するとともに、高温域でも摩擦係数の低下が抑えられ、安定したブレーキ性能を維持できるブレーキ用焼結摩擦材を提供する。 【解決手段】 Ni又はNi+Fe(少量)を金属マトリックスとし、固体潤滑材(a)と摩擦調整材(b)を含有する焼結摩擦材であって、摩擦調整材(b)として、W、Mo、Cr、FeWの中から選ばれる1種以上からなる平均粒径が50μm以上の金属又は合金粒子(b1)と、酸化物、窒化物、炭化物、金属間化合物の中から選ばれる1種以上からなる無機粒子(b2)を含有し、金属又は合金粒子(b1)の平均粒径d b1 と無機粒子(b2)の平均粒径d b2 がd b1

    b2を満足する。Ni又はNi+Fe(少量)の金属マトリックスに、摩擦調整材(b)として特定の条件を満足する金属又は合金粒子(b1)と無機粒子(b2)を分散させることにより、焼結摩擦材の塑性変形を抑制するのに適した粒子の幾何学構造(粒子の高充填密度構造)が得られる。
    【選択図】なし

    ブレーキ用焼結摩擦材
    27.
    发明专利

    公开(公告)号:JP6360270B1

    公开(公告)日:2018-07-18

    申请号:JP2018046328

    申请日:2018-03-14

    CPC classification number: C09K3/14 C22C1/05 C22C19/03 C22C27/04 F16D69/02

    Abstract: 【課題】高い摩擦係数を有するとともに、高温域でも摩擦係数の低下が抑えられ、安定したブレーキ性能を維持できるブレーキ用焼結摩擦材を提供する。 【解決手段】 Ni又はNi+Fe(少量)を金属マトリックスとし、固体潤滑材(a)と摩擦調整材(b)を含有する焼結摩擦材であって、摩擦調整材(b)として、W、Mo、Cr、FeWの中から選ばれる1種以上からなる平均粒径が50μm以上の金属又は合金粒子(b1)と、酸化物、窒化物、炭化物、金属間化合物の中から選ばれる1種以上からなる無機粒子(b2)を含有し、金属又は合金粒子(b1)の平均粒径d b1 と無機粒子(b2)の平均粒径d b2 がd b1

    b2を満足する。Ni又はNi+Fe(少量)の金属マトリックスに、摩擦調整材(b)として特定の条件を満足する金属又は合金粒子(b1)と無機粒子(b2)を分散させることにより、焼結摩擦材の塑性変形を抑制するのに適した粒子の幾何学構造(粒子の高充填密度構造)が得られる。
    【選択図】なし