굴절률이 향상된 아크릴 점착제 및 그 제조방법
    21.
    发明公开
    굴절률이 향상된 아크릴 점착제 및 그 제조방법 有权
    高折射率丙烯酸酯胶粘剂及其制备方法

    公开(公告)号:KR1020120012706A

    公开(公告)日:2012-02-10

    申请号:KR1020100074886

    申请日:2010-08-03

    CPC classification number: C09J133/08 C09J4/00 C09J9/00 C09J11/06

    Abstract: PURPOSE: An acrylic adhesive is provided to use for an optical film, and to reduce the difference of a refractive index with an optical film by improving refractive index. CONSTITUTION: An acrylic adhesive comprises 2-ethylhexylacrylate, 2-ethylhexylacrylate, acrylic acid, and zirconium carboxyethylacrylate in chemical formula 1 or 2-phenoxyethylacrylate in chemical formula 2. The adhesive manufactured by mixing 80-98 weight% of 2-ethylhexylacrylat, 1-10 weight% of acrylic acid, and 0.1-1.5 weight% of zirconium carboxyethylacrylate on the basis of total weight of a monomer, and through a solvent-polymerization. The adhesive is manufactured by using methyl arizidine derivatives as a hardener.

    Abstract translation: 目的:提供用于光学膜的丙烯酸粘合剂,并通过提高折射率来减小与光学膜的折射率差异。 构成:丙烯酸类粘合剂包括丙烯酸2-乙基己酯,丙烯酸2-乙基己基酯,丙烯酸和化学式1中的丙烯酸羧基乙酯和丙烯酸2-苯氧基乙酯。通过将80-98重量%的2-乙基己基丙烯酸酯,1- 10重量%的丙烯酸和0.1-1.5重量%的基于单体总重量的丙烯酸羧乙酯锆,并通过溶剂聚合。 粘合剂通过使用甲基三氮茚衍生物作为硬化剂制造。

    탄소나노튜브를 포함하는 아크릴계 점착제 및 그 제조방법
    22.
    发明公开
    탄소나노튜브를 포함하는 아크릴계 점착제 및 그 제조방법 有权
    包含碳纳米管的丙烯酸压敏粘合剂及其制备方法

    公开(公告)号:KR1020110094812A

    公开(公告)日:2011-08-24

    申请号:KR1020100014444

    申请日:2010-02-18

    CPC classification number: C09J11/04 C08K3/04 C08K2201/011 C09J9/00 C09J133/08

    Abstract: PURPOSE: A method for preparing an acrylic pressure-sensitive adhesive is provided to improve adhesive properties while maintaining transparency by adding carbon nanotubes. CONSTITUTION: A method for preparing an acrylic pressure-sensitive adhesive comprises the steps of: dispersing carbon nanotubes into n-vinyl pyrrolidone toi preparing a dispersion; mixing the dispersion, 2-ethylhexylacrylate, and acrylic acids to prepare a mixture; reacting the mixture at 60~80 °C for 0.5~1 hours; adding the mixed solution in which a solvent and an initiator are added 3 times. The n-vinyl pyrrolidone dispersion includes 0.1~0.3 weight% of carbon nanotube.

    Abstract translation: 目的:提供一种制备丙烯酸压敏粘合剂的方法,以通过添加碳纳米管来保持透明性,从而改善粘合性能。 构成:制备丙烯酸类压敏粘合剂的方法包括以下步骤:将碳纳米管分散在n-乙烯基吡咯烷酮中以制备分散体; 将分散体,丙烯酸2-乙基己酯和丙烯酸混合以制备混合物; 混合物在60〜80℃下反应0.5〜1小时; 加入其中加入溶剂和引发剂的混合溶液3次。 所述N-乙烯基吡咯烷酮分散体包含0.1〜0.3重量%的碳纳米管。