사이클로덱스트린 유도체를 도입한 가소제 조성물, 이를포함하는 가소제 유출 저감형 연질 PVC 조성물 및 그제조방법
    21.
    发明公开
    사이클로덱스트린 유도체를 도입한 가소제 조성물, 이를포함하는 가소제 유출 저감형 연질 PVC 조성물 및 그제조방법 有权
    包含环糊精衍生物的增塑剂组合物,柔性PVC组合物抑制含有它们的塑化剂的迁移及其制造方法

    公开(公告)号:KR1020080071754A

    公开(公告)日:2008-08-05

    申请号:KR1020070010023

    申请日:2007-01-31

    CPC classification number: C08L27/06 C08K5/0016 C08L5/16 C08L2666/26

    Abstract: A method for preparing a soft PVC composition, a soft PVC composition, and a plasticizer composition are provided to reduce the elusion of a plasticizer without the deterioration of the physical properties of PVC. A method for preparing a soft PVC composition comprises the steps of preparing a cyclodextrin derivative represented by the formula 3; mixing the cyclodextrin derivative, PVC and a liquid phase low molecular weight plasticizer to make a plastisol; and heating the plastisol until it becomes a solution state and cooling it, wherein R are independently a C1-C20 group represented by the formula 4 and has a degree of substitution of 5-100 %; and n is an integer of 6-26. In the formula 4, a, b, c, d, e, f and g are an integer of 0 or more, and a+b+c+d+e+f+g is 1 or more; and R is a group comprising random covalent bond of H, C, N, O and S.

    Abstract translation: 提供了制备软质PVC组合物,软质PVC组合物和增塑剂组合物的方法,以减少增塑剂的剥离,而不会使PVC的物理性能下降。 制备软质PVC组合物的方法包括制备由式3表示的环糊精衍生物的步骤; 混合环糊精衍生物,PVC和液相低分子量增塑剂制成增塑溶胶; 加热增塑溶胶直到溶解状态并冷却,其中R独立地为由式4表示的C1-C20基团,取代度为5-100%; n为6-26的整数。 在式4中,a,b,c,d,e,f和g为0以上的整数,a + b + c + d + e + f + g为1以上, 并且R是包含H,C,N,O和S的无规共价键的基团。

    사이클로덱스트린을 이용한 다공성 이산화티탄의 제조 방법
    22.
    发明授权
    사이클로덱스트린을 이용한 다공성 이산화티탄의 제조 방법 失效
    使用环糊精的多孔二氧化钛的制备方法

    公开(公告)号:KR100773134B1

    公开(公告)日:2007-11-02

    申请号:KR1020060119438

    申请日:2006-11-30

    Inventor: 곽승엽 정재우

    Abstract: A method for preparing porous titanium dioxide using cyclodextrin is provided to produce titanium dioxide having a uniform pore size and a large specific surface area, facilitate the control of pore size, and be a simple process without requiring a separate sintering process. A method for preparing porous titanium dioxide using cyclodextrin includes the steps of: (S1) preparing a cyclodextrin or cyclodextrin derivative, and a titanium precursor; and (S2) reacting the cyclodextrin or cyclodextrin derivative with the titanium precursor in an aqueous solution of sulfuric acid. The step(S2) is carried out in the presence of a reaction inhibitor for controlling a polymerization rate of the titanium precursor. A molar ratio of the cyclodextrin to the titanium precursor is 1:0.5-1:12.

    Abstract translation: 提供了使用环糊精制备多孔二氧化钛的方法,以制备具有均匀孔径和大比表面积的二氧化钛,有助于控制孔径,并且是简单的工艺,不需要单独的烧结工艺。 使用环糊精制备多孔二氧化钛的方法包括以下步骤:(S1)制备环糊精或环糊精衍生物和钛前体; 和(S2)使环糊精或环糊精衍生物与钛前体在硫酸水溶液中反应。 步骤(S2)在用于控制钛前体的聚合速率的反应抑制剂的存在下进行。 环糊精与钛前体的摩尔比为1:0.5-1:12。

    메조기공 TiO2 및 기공 내에 전이금속이 함침된 가시광응답 메조기공 TiO2의 합성 방법
    23.
    发明公开
    메조기공 TiO2 및 기공 내에 전이금속이 함침된 가시광응답 메조기공 TiO2의 합성 방법 有权
    用于合成具有可见光活性的MOPOPOROUS TIO2和过渡金属 - 印迹的MESOPOROUS TIO2的方法

    公开(公告)号:KR1020050114563A

    公开(公告)日:2005-12-06

    申请号:KR1020040039844

    申请日:2004-06-01

    Inventor: 곽승엽 김동석

    Abstract: 본 발명은 계면활성제를 이용하여 메조기공 TiO
    2 를 합성하고 기공 내에 전이금속 백금(Pt)을 함침시켜 가시광선영역에서 고활성 고내구성을 가지는 광촉매를 제조하는 방법에 관한 것으로, 계면활성제의 소수성 부분의 길이를 조절하여 메조기공을 의도된 크기로 조절할 수 있고 합성조건에 따라 판형 및 육방형 형태와 같은 여러 종류의 메조기공 TiO
    2 을 합성할 수 있으며, 특히 기공 내에 여러 가지 전이금속을 농도별로 함침시킬 수 있는 것을 특징으로 한다.
    본 발명에 따른 메조기공 TiO
    2 및 기공내의 전이금속 함침은 기공 내에만 전이금속을 함침시킴으로써 광촉매 TiO
    2 의 표면을 그대로 유지시킬 수 있을 뿐만 아니라 광촉매의 촉매활성을 지속시킬 수 있고, 더 나아가 전이금속에 의해서 가시광선영역에서 활성을 가지는 광촉매를 제조하고 이에 따른 광활성을 증대시킬 수 있는 효과가 있어, 실용화 단계에서의 단점이었던 촉매의 지속성 및 안전성 문제를 동시에 해결하고 고내구성 및 고활성을 가지는 가시광선활성 광촉매를 제조할 수 있는 것을 특징으로 한다.

Patent Agency Ranking