고강도 금속공구의 전해 연마 방법
    21.
    发明公开
    고강도 금속공구의 전해 연마 방법 无效
    高强度金属工具的电镀方法

    公开(公告)号:KR1020120111150A

    公开(公告)日:2012-10-10

    申请号:KR1020110029498

    申请日:2011-03-31

    Inventor: 하홍수 오상수

    CPC classification number: C25F3/24

    Abstract: PURPOSE: An electrolytic polishing method for a high-strength metal tool is provided to accurately and quickly polish an object by arranging a polishing electrode corresponding to the shape of the polished surface of the object. CONSTITUTION: An electrolytic polishing method for a high-strength metal tool is as follows. An object(100) is dipped and coated in paraffin and paraffin is removed from a part to be polished. A polishing electrode(200) is processed corresponding to the shape of the polished surface of the object and separated a predetermined distance from the object, the object and the polishing electrode are dipped in electrolytic polishing liquid(300), and the polishing electrode is arranged corresponding to the shape of the polished surface of the object. (+) pole is connected to the object while (-) pole is connected to the polishing electrode. [Reference numerals] (AA) DC power supply device; (BB) Edge after polishing

    Abstract translation: 目的:提供一种用于高强度金属工具的电解抛光方法,通过布置与物体的抛光表面的形状对应的抛光电极来精确地并快速地抛光物体。 构成:高强度金属工具的电解抛光方法如下。 将物体(100)浸渍并涂覆在石蜡中,并从待抛光的部分除去石蜡。 将抛光电极(200)与物体的抛光表面的形状相对应,并与物体隔开预定的距离,物体和抛光电极被浸入电解抛光液(300)中,抛光电极被布置 对应于物体的抛光表面的形状。 (+)极连接到物体,而( - )极连接到抛光电极。 (标号)(AA)直流电源装置; (BB)抛光后的边缘

    연속 표면 분석장치
    22.
    发明公开
    연속 표면 분석장치 无效
    连续表面测量装置

    公开(公告)号:KR1020120111147A

    公开(公告)日:2012-10-10

    申请号:KR1020110029490

    申请日:2011-03-31

    Abstract: PURPOSE: A continuous surface analyzing device is provided to consecutively measure defects of a surface and the roughness of the surface of a linear material continuously provided by a reel-to-reel method, thereby providing the final linear material product of a high quality. CONSTITUTION: A continuous surface analyzing device comprises a frame(100), a reel-to-reel member(200), a defect measuring unit(300), and a controller(400). The defect measuring unit is joined to one side of the reel-to-reel member and measures defects of a surface of a linear material by irradiating lights to the surface of the linear material on a real time basis. The controller controls the operation and driving of the defect measuring unit. [Reference numerals] (AA) Wire material

    Abstract translation: 目的:提供连续的表面分析装置,连续地通过卷对卷方法连续地测量表面的缺陷和线性材料表面的粗糙度,从而提供高品质的最终线材产品。 构成:连续表面分析装置包括框架(100),卷轴对卷轴构件(200),缺陷测量单元(300)和控制器(400)。 缺陷测量单元连接到卷轴到卷轴构件的一侧,并且通过实时地将线照射到线材的表面来测量线材的表面的缺陷。 控制器控制缺陷测量单元的操作和驱动。 (标号)(AA)线材

    초전도 박막 선재를 이용한 원형 와이어의 제조방법 및 이를 이용한 초전도 케이블
    23.
    发明授权
    초전도 박막 선재를 이용한 원형 와이어의 제조방법 및 이를 이용한 초전도 케이블 有权
    使用超导涂层导体及其超导电缆制造圆线的方法

    公开(公告)号:KR101118748B1

    公开(公告)日:2012-03-13

    申请号:KR1020100018544

    申请日:2010-03-02

    CPC classification number: Y02E40/64

    Abstract: 본 발명은 초전도 박막 선재를 이용한 원형 와이어의 제조방법 및 이를 이용한 초전도 케이블에 관한 것으로, 초전도 박막 선재의 초전도층에 길이 방향으로 홈을 넣는(striation) 제1단계와; 상기 홈이 형성된 초전도 박막 선재를 슬릿팅하는 제2단계와; 상기 슬릿팅된 초전도 박막 선재를 단면 형태가 사각형을 이루도록 적층하는 제3단계와; 상기 적층된 초전도 박막 선재를 둥근릴에 감되, 턴(turn) 간 확산방지를 위한 접합방지필름을 함께 감는 제4단계와; 상기 둥근릴에 감긴 초전도 박막 선재를 열처리하여 확산접합시키는 제5단계와; 상기 둥근릴에 감긴 초전도 박막 선재를 풀어 표면을 구리 도금하여 단면의 형상이 원형이 되도록 하는 제6단계;를 포함하여 이루어지는 것을 특징으로 하는 초전도 박막 선재를 이용한 원형 와이어의 제조방법 및 상기 원형 와이어를 꼬아서 형성시킨 초전도 케이블을 기술적 요지로 한다. 이에 의해 초전도 박막 선재를 이용하여 거의 손상없이 긴 원형 와이어를 용이하게 제조할 수 있고, 원형 와이어를 선재를 꼴 수 있어서 교류 손실을 줄일 수 있으며, 아울러 기존의 구리 도체를 이용한 케이블 제작방법과 거의 동일한 방법으로 원형 와이어를 꼬면서 케이블을 제작할 수 있어 교류 손실이 최소화되는 초전도 케이블을 제작할 수 있는 이점이 있다.

    틸트형 멀티 턴 릴투릴 이송장치
    24.
    发明授权
    틸트형 멀티 턴 릴투릴 이송장치 有权
    倾斜式多转转卷轴传送机

    公开(公告)号:KR101023231B1

    公开(公告)日:2011-03-21

    申请号:KR1020080117515

    申请日:2008-11-25

    Abstract: 본 발명은 기판을 이송하는 틸트형 멀티 턴 릴투릴 이송장치에 관한 것으로서, 보다 구체적으로는 공급회전축, 드럼회전축 및 수거회전축이 각각 회전중심에 형성된 공급릴, 이송드럼 및 수거릴에 테이프 형상의 기판이 감겨 이송되는 릴투릴 이송장치에 있어서, 공급릴에서 이송드럼으로 기판이 이송되는 방향과, 이송드럼에서 수거릴로 기판이 이송되는 방향이 평행하도록, 상기 공급회전축 및 수거회전축이 상기 드럼회전축의 축방향에 대해 기울어지게 형성되거나, 상기 드럼회전축이 상기 공급회전축 및 수거회전축의 축방향에 대해 편향각도로 기울어지게 형성되는 것을 기술적 특징으로 하여, 이송되는 기판의 측면으로 전단응력이 생기는 것을 방지하고, 기판이 한쪽으로 쏠려 겹쳐지게 이송되어 기판이 변형되거나, 파손되는 것을 막을 수 있는 효과가 있다.
    초전도, 각도, 드럼, 변형, 초전도 테이프

    안정화재가 형성된 초전도 박막선재 및 그의 접합방법
    25.
    发明授权
    안정화재가 형성된 초전도 박막선재 및 그의 접합방법 有权
    具有稳定器的超级电容器带及其方法

    公开(公告)号:KR100945201B1

    公开(公告)日:2010-03-03

    申请号:KR1020070110238

    申请日:2007-10-31

    CPC classification number: H01L39/143 H01L39/248

    Abstract: 본 발명은 안정화재가 형성된 초전도 박막선재 및 그의 접합방법에 관한 것으로서, 상세하게는 초전도 박막선재와 안정화재 및 접합방지기판을 알코올로 세척하는 제1단계; 상기 초전도 박막선재 및 안정화재의 일면에 각각 금속코팅층으로 얇게 코팅하는 제2단계; 상기 초전도 박막선재 및 안정화재를 금속코팅층이 있는 일면으로 서로 접합하는 제3단계; 상기 초전도 박막선재와 상기 안정화재의 외측에 상기 접합방지기판을 배치한 후, 보빈에 일정한 장력으로 서로 밀착되도록 권선하는 제4단계; 및 상기 초전도 박막선재 및 안정화재가 금속코팅층으로 확산접합되도록 열처리하는 제5단계;를 포함하여 이루어지는 것을 기술적 특징으로 하여, 두께가 두껍거나 여러 종류의 안정화재도 신속하게 초전도 박막선재에 접합할 수 있어서 공정 시간을 줄일 수 있으며, 다양한 곡률의 초전도 박막선재를 형성할 수 있고, 열처리 이전에 초전도 박막선재를 권선하여 초전도 박막선재의 변형에 따른 초전도의 특성저하를 방지할 수 있는 효과가 있다.
    안정화, 팬케이크, 권선, 초전도 선재, 접합, 열처리

    레이저윈도우 오염 방지를 위한 레이저 증착 장치
    26.
    发明授权
    레이저윈도우 오염 방지를 위한 레이저 증착 장치 失效
    레이저윈도우오염방지를위한레이저증착장치

    公开(公告)号:KR100745610B1

    公开(公告)日:2007-08-02

    申请号:KR1020060032939

    申请日:2006-04-11

    Abstract: A pulsed laser deposition apparatus having a function of preventing a laser window from being contaminated is provided to uniformly supply the laser beam energy by forming a plume screen part in the laser window. A plume screen part(100) is formed between a plume(8) and a laser window(3). The plume screen part includes a body(110) formed on a laser window port to be communicated with a vacuum chamber(2), and laser beam passes through the body. The laser window is provided on a front end of the body onto which the laser beam is incident. A screen(120) is formed in the body of the laser window to prevent contamination of the laser window.

    Abstract translation: 提供具有防止激光窗口被污染的功能的脉冲激光沉积设备,以通过在激光窗口中形成羽流屏幕部分来均匀地提供激光束能量。 烟羽筛网部件(100)形成在羽流(8)和激光窗口(3)之间。 烟幕部分包括形成在激光窗口上以与真空室(2)连通的主体(110),并且激光束穿过主体。 激光窗口设置在激光束入射到其上的主体的前端。 屏幕(120)形成在激光窗的主体中以防止激光窗的污染。

    고온초전도 테이프의 연속 임계전류 측정장치
    27.
    发明公开
    고온초전도 테이프의 연속 임계전류 측정장치 失效
    用于测量高温超导体带的连续电流的装置

    公开(公告)号:KR1020040056597A

    公开(公告)日:2004-07-01

    申请号:KR1020020083106

    申请日:2002-12-24

    Abstract: PURPOSE: An apparatus for measuring continuous critical current of a high-temperature superconducting tape is provided to measure continuously the critical current in unit length of the high-temperature superconducting tape by using a contact method and a non-contact method. CONSTITUTION: An apparatus for measuring continuous critical current of a high-temperature superconducting tape includes a guide roller, a high-temperature superconducting tape supporter, a positive and a negative current terminal, and a positive and a negative voltage terminal. The guide roller(3A,3B) is used for transferring a high-temperature superconducting tape(1) to a liquid nitrogen tank(2). The high-temperature superconducting tape supporter is used for supporting the high-temperature superconducting tape in the inside of the liquid nitrogen tank. The positive and the negative current terminals(50,80) and the positive and the negative voltage terminals(60,70) are arranged at the high-temperature superconducting tape. The apparatus for measuring continuous critical current of the high-temperature superconducting tape has a structure for controlling the pressure of the voltage terminals and the pressure of the current terminals. A current measurement terminal is installed at a top side of the tape supporter.

    Abstract translation: 目的:提供一种用于测量高温超导带的连续临界电流的装置,通过使用接触方法和非接触方法连续测量高温超导带的单位长度的临界电流。 构成:用于测量高温超导带的连续临界电流的装置包括引导辊,高温超导带支架,正极和负极端子以及正和负电压端子。 引导辊(3A,3B)用于将高温超导带(1)转移到液氮罐(2)。 高温超导带支架用于支撑液氮罐内部的高温超导带。 正极和负极端子(50,80)和正极和负极端子(60,70)布置在高温超导带上。 用于测量高温超导带的连续临界电流的装置具有用于控制电压端子的压力和电流端子的压力的结构。 电流测量端子安装在磁带支架的顶侧。

    초전도 선재 소세징 측정 방법 및 시스템
    28.
    发明公开
    초전도 선재 소세징 측정 방법 및 시스템 失效
    测量超导线路成员的测量方法和系统

    公开(公告)号:KR1020030054152A

    公开(公告)日:2003-07-02

    申请号:KR1020010084271

    申请日:2001-12-24

    Abstract: PURPOSE: A method and a system for measuring a sausaging of a superconductive wire member are provided to reduce manufacturing cost of the superconductive wire member by measuring time and size of the sausaging during a drawing process. CONSTITUTION: A sausaging measuring system includes a base(18), a drawing rail(17), a drawing dice(12), a drawing jig(13), a load cell(14), a data display/storage device(15) and a drawing carriage(16). One end of the base(18) makes contact with a lower portion of the drawing dice(12). The drawing jig(13) and the load cell(14) are attached to the drawing carriage(16). The drawing jig(13) grips a front portion of a superconductive wire member(11), which passes through the drawing dice(12). The load cell(14) moves along the drawing rail(17) when a drawing process of the superconductive wire member(11) is carried out so as to detect variation of tensile force generated from the superconductive wire member(11).

    Abstract translation: 目的:提供一种用于测量超导线构件的腊肠的方法和系统,以通过在拉伸过程中测量腊肠的时间和尺寸来降低超导线构件的制造成本。 构成:腊肠测量系统包括基座(18),拉丝轨(17),绘图骰子(12),绘图夹具(13),称重传感器(14),数据显示/存储装置(15) 和一个绘图托架(16)。 基部(18)的一端与图形骰子(12)的下部接触。 牵引夹具(13)和称重传感器(14)安装在拉伸托架(16)上。 绘图夹具(13)夹住通过绘图骰子(12)的超导线构件(11)的前部。 当执行超导线构件(11)的拉拔处理以便检测从超导线构件(11)产生的拉伸力的变化时,称重传感器(14)沿着牵引轨道(17)移动。

    초전도 선의 접합 방법
    29.
    发明授权
    초전도 선의 접합 방법 有权
    초전도선의접합방법

    公开(公告)号:KR100380630B1

    公开(公告)日:2003-04-23

    申请号:KR1020000052501

    申请日:2000-09-05

    Abstract: PURPOSE: A superconductor wire connecting method is provided to improve critical current characteristic of a superconductor connection portion. CONSTITUTION: A superconductor core having a hole and a superconductor sleeve(10) configured of a conductive coat covering the core are provided. Particles and oxide on the surface of the sleeve are removed. An insulating layer formed on the surface of a connection portion of a superconductor wire(20) is eliminated. A base metal that supports a superconductor filament of the superconductor wire and is exposed to the outside is removed. The superconductor filament is cleaned. The cleaned superconductor filament is inserted into the hole of the sleeve, and at least one additional superconductor wire(40) is also inserted into the hole together with a superconductor wire to be connected. The sleeve is compressed to fix the superconductor wires to the sleeve. The portion of the additional superconductor wire, other than the inserted filament portion, is cut and removed.

    Abstract translation: 目的:提供一种超导体导线连接方法,以改善超导体连接部分的临界电流特性。 本发明提供了一种具有孔的超导体芯和由覆盖该芯的导电涂层构成的超导体套管(10)。 套筒表面上的颗粒和氧化物被去除。 消除了在超导体线材(20)的连接部分的表面上形成的绝缘层。 支撑超导体线的超导体细丝并暴露于外部的基体金属被去除。 超导体灯丝被清洁。 将清洁过的超导体细丝插入到套管的孔中,并且还将至少一根另外的超导体线(40)与待连接的超导体线一起插入该孔中。 套管被压缩以将超导电线固定到套管上。 除了插入的细丝部分之外,额外超导体导线的部分被切割并移除。

    초전도 선의 접합 방법
    30.
    发明公开
    초전도 선의 접합 방법 有权
    超导线连接方法

    公开(公告)号:KR1020020019323A

    公开(公告)日:2002-03-12

    申请号:KR1020000052501

    申请日:2000-09-05

    Abstract: PURPOSE: A superconductor wire connecting method is provided to improve critical current characteristic of a superconductor connection portion. CONSTITUTION: A superconductor core having a hole and a superconductor sleeve(10) configured of a conductive coat covering the core are provided. Particles and oxide on the surface of the sleeve are removed. An insulating layer formed on the surface of a connection portion of a superconductor wire(20) is eliminated. A base metal that supports a superconductor filament of the superconductor wire and is exposed to the outside is removed. The superconductor filament is cleaned. The cleaned superconductor filament is inserted into the hole of the sleeve, and at least one additional superconductor wire(40) is also inserted into the hole together with a superconductor wire to be connected. The sleeve is compressed to fix the superconductor wires to the sleeve. The portion of the additional superconductor wire, other than the inserted filament portion, is cut and removed.

    Abstract translation: 目的:提供超导线连接方法,以改善超导体连接部分的临界电流特性。 构成:提供一种具有孔的超导体芯和由覆盖该芯的导电涂层构成的超导体套管(10)。 除去套筒表面上的颗粒和氧化物。 消除了在超导线(20)的连接部分的表面上形成的绝缘层。 移除支撑超导线的超导体细丝并暴露于外部的贱金属。 超导体丝被清洁。 清洁的超导体细丝被插入到套筒的孔中,并且至少一个额外的超导体线(40)也与要连接的超导体线一起插入孔中。 套筒被压缩以将超导线固定到套筒上。 除了插入的细丝部分之外,附加超导体线的部分被切割和移除。

Patent Agency Ranking