Abstract:
Thermoplastic vulcanizate elastomer obtained by dynamic vulcanization of a heterophasic polyolefin composition in presence of at least (i) an alkenyl-substituted alkoxysilane grafting agent and (ii) water; wherein said heterophasic polyolefin composition has flexural modulus equal to or lower than 150 MPa,and comprises: (a) a crystalline propylene homopolymer or copolymer of propylene with up to 15% of ethylene or other alpha-olefin comonomer(s), or their combinations, and (b) a copolymer or a composition of copolymers of ethylene with other alpha-olefins, containing from 15% to 40% of ethylene, said thermoplastic vulcanizate elastomer having compression set values in the range from 45 -65%, the ratio of elongation at break to compression set values over 10 and hardness shore A values below 90.
Abstract:
The present disclosure provides a polyolefin-based composition suitable for use as adhesives and/or tie-layer adhesive compositions as well as a multi-layered structure made from and/or containing the polyolefin-based composition. The polyolefin-based composition is made from and/or contains (a) a grafted polyolefin composition, (b) a first polymer composition, (c) a polypropylene-containing blend composition, and (d) optionally, an additives composition having one or more additives.
Abstract:
A polyolefin nanocomposite material comprising the following components: (A) a crystalline or semi-crystalline polyolefin resin; and (B) a nanosized mineral filler comprising or substantially consisting of a hydrotalcite, wherein the amount of the hydrotalcite is from 0.02 to 6 parts by weight per 100 parts by weight of the nanocomposite material, and the ratio MFR (1)/MFR (2) of the melt flow rate value MFR (1) of component (A) to the melt flow rate value MFR (2) of the polyolefin nanocomposite material is of at least 1.02, characterized in that the said polyolefin nanocomposite material includes a compatibilizer the dispersion of the mineral filler (B) and compatibilizer in the polyolefin resin is produced at shear mixing rates from 30 to 300 sec−1,
Abstract:
Polyolefin compositions comprising, by weight: A) 30-80% of a polyolefin component containing not less than 80% of a waste material selected from polyethylene, polypropylene or their mixtures; B) 20-70% of a heterophasic polyolefin composition having flexural modulus equal to or lower than 600 MPa.
Abstract:
Filled polyolefin compositions comprising: A) from 10% to 75% by weight of a polypropylene component; B) from 20% to 80% by weight of a filler; C) from 3% to 50% of a polybutene-1 component; wherein the percentages of A), B) and C) are referred to the sum of A) B) and C).
Abstract:
Polypropylene compositions having a MFR value (2.16 kg, 230 °C) from 15 to 200 g/10 min., comprising: A) a propylene polymer or polymer composition selected from propylene homopolymers or copolymers of propylene containing up to 5% by moles of comonomer(s), said homopolymers and copolymers having values of MFR, obtained without degradation treatments, from 500 to 2500 g/10 min., or combinations of the said homopolymers or copolymers; B) a filler or pigment, or their combinations; and optionally C) from 0.5 to 5% by weight, with respect to the total weight of A), B) and C), of a compatibilizer.