公开(公告)号:AU5819400A
公开(公告)日:2001-01-31
申请号:AU5819400
申请日:2000-06-23
Applicant: BASF AG
Inventor: FISCHER MICHAEL , RAU WALTER , WELZ MARTIN
Abstract: A composite is composed of at least one first molding and one second molding, where the first molding and the second molding have been immovably bonded to one another via at least one partial region of one surface alpha of the first molding and of one surface beta of the second molding, via a welded region, and where, based on the first molding, at least 50% by weight of the first molding is composed of a molding composition comprising:A) from 5 to 99% by weight of a polyester,B) from 1 to 95% by weight of a fibrous filler pretreated with an aminosilane compound and with an epoxy polymer,C) from 0 to 30% by weight of an elastomeric polymer, andD) from 0 to 40% by weight of other additives,where the total of the percentages by weight of components A) to D) is 100%.Laminates made from these composites, and products produced therefrom and recycled materials obtained therefrom, are described, as is the use of all of these, in particular in automotive construction.
-
公开(公告)号:CA2370093A1
公开(公告)日:2001-01-04
申请号:CA2370093
申请日:2000-06-23
Applicant: BASF AG
Inventor: WELZ MARTIN , RAU WALTER , FISCHER MICHAEL
Abstract: The invention relates to a composite material that consists of at least one first molded part and one second molded part. Said first molded part and sai d second molded part are rigidly linked with each other across at least a partial section with a surface .alpha. of the first molded part and a surfac e .beta. of the second molded part by means of a welded zone. At least the fir st molded part consists by at least 50 % by weight, based on the first molded part, of a molding compound that contains: A) 5 to 99 % by weight of a polyester, B) 1 to 95 % by weight of a fibrous filler that is treated with a n aminosilane compound and an epoxypolymer, C) 0 to 30 % by weight of a rubber - elastic polymer, D) 0 to 40 % by weight of further additives, the weight percentages of components A) to D) adding up 100 %. The invention also relat es to laminates that consist of said composites and to structures and recycled products obtained thereof and to the use of all these products, especially i n the manufacture of automobiles.
-
公开(公告)号:DE19929302A1
公开(公告)日:2000-12-28
申请号:DE19929302
申请日:1999-06-25
Applicant: BASF AG
Inventor: FISCHER MICHAEL , RAU WALTER
IPC: C08J5/00 , B32B5/18 , B32B27/36 , C08F265/04 , C08K3/04 , C08K7/02 , C08L25/00 , C08L25/12 , C08L51/00 , C08L51/04 , C08L67/02 , C08L69/00 , C08L51/08
Abstract: A molding composition (I) comprises (A) up to 99.59 wt.% of a polycondensate (B1) 0.1-20 wt.% of a particulate graft copolymer having a glass transition temperature of the soft phase of less than 0 deg C and an average particle size of 50-1000 nm (C) 0.1-20 wt.% of a copolymer comprising (C1) 50-90 wt.% of a vinyl aromatic monomer (C2) 10-50 wt.% acrylonitrile and/or methacrylonitrile. A molding composition (I) comprises: (A) up to 99.59 wt.% of a polycondensate; (B) composition (B) comprises: (1) (B1) 0.1-20 wt.% of a particulate graft copolymer having a glass transition temperature of the soft phase of less than 0 deg C and an average particle size of 50-1000 nm; (C) 0.1-20 wt.% of a copolymer comprises: (1) (C1) 50-90 wt.% of a vinyl aromatic monomer; and (2) (C2) 10-50 wt.% acrylonitrile and/or methacrylonitrile; (D) 0-20 wt.% of a copolymer having differing amounts of vinyl aromatic monomer, acrylonitrile and/or methacrylonitrile to those in (C); (E) 0.1-20 wt.% of a polyester different to (A); (F) 0.01-10 wt.% of: (1) (F1) a nucleation agent; and (2) (F2) an esterification stabilizer whereby the wt. ratio of (F1) to (F2) of 1:100-100:1; and (G) 0.1-10 wt.% of conventional additive such as carbon black, UV stabilizers, anti-oxidants and release agents. Independent claims are included for: (i) a molded article (II) prepared from the composition (I) ; (ii) a laminated (III) comprising the molded article (II) and a polycondensate foam; and (iii) recycled material obtained from (I), (II) or (III).
-
公开(公告)号:DE19929301A1
公开(公告)日:2000-12-28
申请号:DE19929301
申请日:1999-06-25
Applicant: BASF AG
Inventor: FISCHER MICHAEL , RAU WALTER , WELZ MARTIN
Abstract: In a composite with at least two moulded parts bonded together at a weld zone, at least 50 wt% of at least one of these parts consists of a fibre-reinforced polyester moulding material in which the fibrous filler is pretreated with an aminosilane compound and an epoxy polymer. A composite with at least two moulded parts (1, 2) rigidly bonded together at a weld zone covering at least part of their surfaces ( alpha and beta respectively), in which at least 50 wt% of at least part 1 consists of a moulding material containing: (A) 5-99 wt% polyester; (B) 1-95 wt% fibrous filler pretreated with an aminosilane compound and an epoxy polymer; (C) 0-30 wt% rubber-elastic polymer; and (D) 0-40 wt% other additives. Independent claims are also included for: (a) a process for the production of these composites by welding at least part of surfaces alpha and beta together to form a weld zone; (b) composites obtained by this process; (c) recycling moulded parts or moulding materials from these composites or the composites themselves; (d) recycled material obtained from the parts, moulding materials or composites; and (e) formed products or laminates containing these composites and/or recycled materials.
-
-
-