Abstract:
The present invention relates to a process for producing surface-postcrosslinked water-absorbent polymer particles by coating of water-absorbent polymer particles having a content of residual monomers in the range from 0.03 to 15% by weight with at least one surface-postcrosslinker and thermal surface-postcrosslinking at temperatures in the range from 100 to 180° C.
Abstract:
The present invention relates to a process for producing water-absorbent polymer particles by polymerizing droplets of a monomer solution comprising less than 0.3% by weight of persulfate and at least 0.05% by weight of azo initiator and thermal aftertreatment of the formed polymer particles at less than 100° C. in a fluidized bed for 60 to 300 minutes.
Abstract:
The present invention relates to a process for producing surface-postcrosslinked water-absorbent polymer particles comprising polymerizing droplets of a monomer solution, wherein water-absorbent polymer particles having an average particle diameter from 420 to 700 μm, an amount of water-absorbent polymer particles having a particle size of less than 300 μm of less than 5% by weight and an amount of water-absorbent polymer particles having a particle size of more than 800 μm of less than 5% by weight are coated with at least one surface-postcrosslinker and thermal surface-postcrosslinked.
Abstract:
The present invention relates to a process for producing water-absorbent polymer particles by polymerizing droplets of a monomer solution comprising less than 0.3% by weight of persulfate and at least 0.05% by weight of azo initiator and thermal aftertreatment of the formed polymer particles at less than 100° C. in a fluidized bed for 60 to 300 minutes.