公开(公告)号:CA648262A
公开(公告)日:1962-09-11
申请号:CA648262D
Applicant: HOECHST AG
Inventor: WEISSERMEL KLAUS , LEDERER MICHAEL
-
公开(公告)号:FI63245C
公开(公告)日:1983-05-10
申请号:FI771953
申请日:1977-06-22
Applicant: HOECHST AG
Inventor: LEDERER MICHAEL , BOUMAN ANTONIUS J M
IPC: C08F2/00 , C08F2/18 , C08F2/20 , C08F2/44 , C08F12/00 , C08F285/00 , C08F291/02 , C08F279/02 , C08F112/08
Abstract: There is described an improved process for the discontinuous suspension polymerization of alkenyl-aromatic compounds, which comprises re-using the aqueous polymerization medium, after separation of the polymer beads, as the polymerization medium of a subsequent polymerization. Monomer-soluble and water-soluble initiators and, optionally fresh water and dispersing agent, are added. Re-using the aqueous polymerization medium does not negatively affect the color and mechanical properties of the polymer obtained. The process of the invention results in considerable saving of energy.
-
公开(公告)号:CA1075395A
公开(公告)日:1980-04-08
申请号:CA259017
申请日:1976-08-13
Applicant: HOECHST AG
Inventor: LEDERER MICHAEL , STROBEL WOLFGANG
IPC: C08F4/00 , C08F2/16 , C08F4/28 , C08F255/00 , C08F255/04 , C08F255/06
Abstract: PROCESS FOR PREPARING IMPACT RESISTANT POLYVINYL AROMATICS of the disclosure There is disclosed an improved bulk-suspension process for polymerizing vinyl aromatic monomers in the presence of an ethylene-propylene-nonconjugated diene-rubber, which comprises using, in the suspension polymerization step, peroxy-carbonic esters as the polymerization initiator. The process of the invention yields products having improved notched impact strength, weatherability and elongation at break combined with a good shear stability.
-
公开(公告)号:CA832508A
公开(公告)日:1970-01-20
申请号:CA832508D
Applicant: HOECHST AG
Inventor: LEDERER MICHAEL , SOMMER SIEGFRIED , KOCH HEINRICH , HARREUS ALBRECHT
-
-
公开(公告)号:CA716573A
公开(公告)日:1965-08-24
申请号:CA716573D
Applicant: HOECHST AG
Inventor: LEDERER MICHAEL , JENSEN HARALD
-
公开(公告)号:CA1092294A
公开(公告)日:1980-12-23
申请号:CA281357
申请日:1977-06-24
Applicant: HOECHST AG
Inventor: LEDERER MICHAEL , BOUMAN ANTONIUS J M
IPC: C08F2/00 , C08F2/18 , C08F2/20 , C08F2/44 , C08F12/00 , C08F285/00 , C08F291/02 , C08F12/04 , C08F253/00 , C08F279/00
Abstract: There is described an improved process for the discontinuous suspension polymerization of alkenyl-aromatic compounds, which comprises re-using the aqueous polymerization medium, after separation of the polymer beads, as the polymerization medium of a subsequent polymerization. Monomer-soluble and water-soluble initiators and, optionally fresh water and dispersing agent, are added. Re-using the aqueous polymerization medium does not negatively affect the color and mechanical properties of the polymer obtained. The process of the invention results in considerable saving of energy.
-
公开(公告)号:CA1051582A
公开(公告)日:1979-03-27
申请号:CA221477
申请日:1975-03-05
Applicant: HOECHST AG
Inventor: LEDERER MICHAEL , STROBEL WOLFGANG , JASTROW HORST
IPC: C08F255/00 , C08F255/04 , C08F255/06 , C08F283/12 , C08F291/00 , C08F291/06
Abstract: PROCESS FOR PREPARING IMPACT RESISTANT POLYVINYL AROMATICS of the disclosure The invention relates to novel impact resistant graft copolymers of a vinyl aromatic on an EPTR especially characterized by an improved notched impact strengnth and resistancy to atmospheric corrosion, and a process for their preparation. Said copolymers are obtained by a two-step mass suspension polymerization process characterized by the presence of oxygen, preferably by the presence of air, at a pressure of from 0.05 to 10 atmospheres gauge during the course of the mass polymerization step.
-
公开(公告)号:AU7881775A
公开(公告)日:1976-09-09
申请号:AU7881775
申请日:1975-03-05
Applicant: HOECHST AG
Inventor: LEDERER MICHAEL , STROBEL WOLFGANG , JASTROW HORST
IPC: C08F255/00 , C08F255/04 , C08F255/06 , C08F283/12 , C08F291/00 , C08F19/04 , C08F27/00 , C08G31/22
Abstract: The invention relates to novel impact resistant graft copolymers of a vinyl aromatic on an ethylene/propylene/tercomponent rubber especially characterized by an improved notched impact strength and resistance to atmospheric corrosion, and a process for their preparation. Said copolymers are obtained by a two-step mass/suspension polymerization process characterized by the presence of oxygen, preferably by the presence of air, at a pressure of from 0.05 to 10 atmospheres gauge during the course of the mass polymerization step.
-
-
-
-
-
-
-
-
-