公开(公告)号:JP2014210683A
公开(公告)日:2014-11-13
申请号:JP2013088220
申请日:2013-04-19
Inventor: AKINO TAKEAKI , SHIMODA MASARO , SAGAWA KEIICHIRO , NAGASAWA KOJI , KAWAKAMI HIROYUKI
Abstract: 【課題】早強性を向上することができる、例えば、熱を加える養生をすることなしに調製10時間後の強度を向上することができる、水硬性組成物を提供する。【解決手段】グアニジン塩と、分散剤と、水硬性粉体と、骨材と、水とを含有し、グアニジン塩の含有量が水硬性粉体100質量部に対し0.02質量部以上、0.50質量部以下である、水硬性組成物。【選択図】なし
Abstract translation: 要解决的问题:为了提供可以提高其早期强化性能的水硬性组合物,例如其制备后10小时的强度可以在不加热/老化的情况下提高其制备。溶液:水硬性组合物含有胍盐 ,分散剂,水硬性粉末,骨料和水。 胍盐的含量为0.02-0.50。 质量在100点的基础上。 液压粉的质量。
-
公开(公告)号:JP2013018677A
公开(公告)日:2013-01-31
申请号:JP2011152903
申请日:2011-07-11
Inventor: SHIMODA MASARO , SAGAWA KEIICHIRO , NAGASAWA KOJI
Abstract: PROBLEM TO BE SOLVED: To provide a method of producing hydraulic powder comprising a hydraulic compound excellent in grinding efficiency, wherein the hydraulic powder such as a cement can be obtained in which compression strength at curing of a hydraulic composition thus obtained is improved.SOLUTION: The hydraulic powder is produced through a step of pulverizing the hydraulic compound in the presence of N-methyl diethanolamine and a 3-8C polyol.
Abstract translation: 解决问题的方案:提供一种制造水硬性粉末的方法,该液压粉末包括研磨效率优异的液压组合物,其中可获得如此获得的水硬性组合物的固化时的抗压强度得到改善的水泥粉末 。 解决方案:通过在N-甲基二乙醇胺和3-8C多元醇的存在下将水硬性化合物粉碎的步骤制备水硬性粉末。 版权所有(C)2013,JPO&INPIT
-
公开(公告)号:JP2012167002A
公开(公告)日:2012-09-06
申请号:JP2011152905
申请日:2011-07-11
Inventor: NAGASAWA KOJI , SHIMODA MASARO , SAGAWA KEIICHIRO
Abstract: PROBLEM TO BE SOLVED: To provide a method for producing hydraulic powder capable of achieving excellent crushing efficiency of a hydraulic compound, and simultaneously obtaining hydraulic powder such as cement for improving compressive strength when curing an obtained hydraulic composition.SOLUTION: This hydraulic powder is produced through a step for crushing the hydraulic compound in the presence of glycerin monoacetic acid ester and N-methyl diethanolamine.
Abstract translation: 解决问题的方案:提供一种能够获得水硬性化合物优异的破碎效率的水硬性粉末的制造方法,同时获得水硬性粉末如水泥,以在固化所获得的水硬性组合物时提高抗压强度。
解决方案:该水硬性粉末是通过在甘油单乙酸酯和N-甲基二乙醇胺存在下破碎水硬性化合物的步骤制备的。 版权所有(C)2012,JPO&INPIT
-
公开(公告)号:JP2012131883A
公开(公告)日:2012-07-12
申请号:JP2010284313
申请日:2010-12-21
Inventor: OKAUCHI NOBUAKI , KOYANAGI KOJI , YABE KENICHIRO , SAGAWA KEIICHIRO
Abstract: PROBLEM TO BE SOLVED: To provide a novel polyalkylene glycol polymer that permits easy design of a polymer structure to achieve target properties.SOLUTION: The polyalkylene glycol polymer includes a constituting unit represented by general formula (I) (wherein A, Aand Aare each a 2-4C alkylene group; and n1, n2 and n3 are each a numerical value of 6-300).
Abstract translation: 要解决的问题:提供一种新颖的聚亚烷基二醇聚合物,其允许容易地设计聚合物结构以实现目标性能。 解决方案:聚亚烷基二醇聚合物包括由通式(I)表示的构成单元(其中A
1 SP>,A 2 SP >和A 3 SP>分别是2-4C亚烷基; n1,n2和n3分别为6-300的数值)。 版权所有(C)2012,JPO&INPIT -
公开(公告)号:JP2015003868A
公开(公告)日:2015-01-08
申请号:JP2013128349
申请日:2013-06-19
Inventor: NAGASAWA KOJI , NAKAMURA KEISUKE , SHIMODA MASARO , SAGAWA KEIICHIRO
Abstract: 【課題】使用上、安全な化合物であり、かつ還元効果の高い炭素数2以上、6以下の単糖類をホルムアルデヒドから製造するにあたり、未反応のホルムアルデヒドが少なく、且つ炭素数7以上の単糖類といった副生物が少ない、製造方法を提供する。【解決手段】ホルムアルデヒドを水可溶性の塩基性無機物質の存在下で縮合させる炭素数2以上、6以下の単糖類の製造方法であって、ホルムアルデヒド水溶液に水可溶性の塩基性無機物質を滴下する工程Aを有し、ホルムアルデヒド水溶液中のホルムアルデヒドと、滴下する水可溶性の塩基性無機物質の全量とのモル比が、ホルムアルデヒド/水可溶性の塩基性無機物質の全量で、1/0.50以上、1/0.10以下であり、水可溶性の塩基性無機物質の滴下速度が、ホルムアルデヒド水溶液中のホルムアルデヒド1.0モルに対して、0.01モル/1時間以上、0.25モル/1時間以下である、単糖類の製造方法。【選択図】なし
Abstract translation: 要解决的问题:提供当生产碳数为2以上且6以下的单糖的碳原子数为7以上的单糖的未反应的甲醛和副产物的还原剂的制造方法,其为安全化合物 当使用时具有高的还原效果。解决方案:通过在水溶性碱性无机物质的存在下使甲醛进行缩合反应,生产碳数为2以上且6以下的单糖的方法包括: 将水溶性碱性无机物质滴入甲醛水溶液中,其中甲醛水溶液中甲醛的摩尔比与水溶性碱性无机物的总量相比为1 / 0.50以上至1 / 0.10以下, 甲醛/水溶性碱性无机物的总量,水溶性碱性无机物的滴入速度为0.01摩尔/ 1小时以上, 0.25mol / 1小时或更少至1.0mol甲醛水溶液中的甲醛。
-
公开(公告)号:JP2014189417A
公开(公告)日:2014-10-06
申请号:JP2013064187
申请日:2013-03-26
Inventor: SAGAWA KEIICHIRO , SHIMODA MASARO , NAGASAWA KOJI
CPC classification number: C07C41/50 , C04B7/52 , C04B24/023 , C04B28/02 , C04B2103/52 , C07C43/317 , C04B18/08 , C04B18/141 , C04B18/146 , C04B24/16 , C04B24/30 , C04B24/122
Abstract: PROBLEM TO BE SOLVED: To provide a strength improver composition for hydraulic powder which makes it possible to obtain a hardening body high in early strength.SOLUTION: A strength improver composition for hydraulic powder comprises a reaction product obtained by the reaction between (a1) one or more compound selected from polyhydric alcohols of di- or more and penta- or less valent, and (a2) an aldehyde compound or a ketone compound.
Abstract translation: 要解决的问题:提供一种用于水硬性粉末的强度改进剂组合物,其可以获得早期强度高的硬化体。溶液:用于水硬性粉末的强度改进剂组合物包含通过(a1)一种 或更多选自二元以上且五价以下的多元醇的化合物,和(a2)醛化合物或酮化合物。
-
公开(公告)号:JP2014118331A
公开(公告)日:2014-06-30
申请号:JP2012275559
申请日:2012-12-18
Inventor: SHIMODA MASARO , SAGAWA KEIICHIRO , NAGASAWA KOJI
Abstract: PROBLEM TO BE SOLVED: To provide a method for manufacturing a water-curable powder capable of obtaining a water-curable powder affording an improved pulverizing efficiency at a step of pulverizing a water-curable compound and yielding a water-curable composition exhibiting an improved compressive strength at the time of the curing thereof.SOLUTION: The provided method for manufacturing a water-curable powder includes a step of pulverizing a water-curable compound in the presence of resorcinol (component (A)) and at least one type selected from the group consisting of glycerin and an ethylene oxide adduct of glycerin (component (B)), whereas the mass ratio of the component (A) and the component (B) (component (A)/component (B)) is 1/99 or above and 45/55 or below.
Abstract translation: 要解决的问题:提供一种能够获得水可固化粉末的水可固化粉末的制备方法,其在粉化水可固化化合物的步骤中获得改善的粉碎效率,并产生显示出改进的压缩性的水可固化组合物 制备水可固化粉末的方法包括在间苯二酚(组分(A))存在下粉碎水可固化化合物的步骤和选自以下的至少一种: 甘油和甘油的环氧乙烷加合物(组分(B))组成的组分为成分(A)和组分(B)(组分(A)/组分(B))的质量比为1/99或 以上和45/55以下。
-
公开(公告)号:JP2012121794A
公开(公告)日:2012-06-28
申请号:JP2011249709
申请日:2011-11-15
Inventor: SAGAWA KEIICHIRO , SHIMODA MASARO , NAGASAWA KOJI , HAMAI TOSHIMASA
IPC: C04B24/12 , C04B24/22 , C04B28/02 , C04B103/40
CPC classification number: C04B40/0039 , C04B28/02 , C04B2103/408 , C08G10/02 , C08G10/04 , C08L61/34 , C04B24/122 , C04B24/226 , C04B14/00
Abstract: PROBLEM TO BE SOLVED: To provide a dispersing agent for a hydraulic composition, which strikes a balance between the improvement in flow retentivity of the hydraulic composition and early strength thereof by using a naphthalene sulfonate formaldehyde condensation product as a dispersing agent.SOLUTION: The dispersing agent for the hydraulic composition contains, in a predetermined weight ratio, the naphthalene sulfonate formaldehyde condensation product and an alkyldiethanolamine having an alkyl group having 1-3 carbon atoms.
Abstract translation: 要解决的问题:提供一种用于水硬性组合物的分散剂,其通过使用萘磺酸甲醛缩合产物作为分散剂来平衡水硬性组合物的流动保持性的提高和其早期强度之间的平衡。 解决方案:水硬性组合物用分散剂含有预定重量比的萘磺酸甲醛缩合物和具有1-3个碳原子的烷基的烷基二乙醇胺。 版权所有(C)2012,JPO&INPIT
-
29.
公开(公告)号:JP2010120826A
公开(公告)日:2010-06-03
申请号:JP2008297671
申请日:2008-11-21
Inventor: SAGAWA KEIICHIRO , HAMADA DAISUKE
CPC classification number: C04B28/02 , C04B24/2647 , C04B2103/14 , C04B2103/34 , C04B2103/408 , C04B24/243 , C04B24/2641
Abstract: PROBLEM TO BE SOLVED: To provide a dispersion maintaining agent for a hydraulic composition, which shows low effect of imparting initial fluidity and excels in fluidity retention and development of initial strength of the hydraulic composition.
SOLUTION: The dispersion maintaining agent for a hydraulic composition comprises a copolymer obtained by polymerizing a specific alkenyl ether monomer 1 which is represented by formula (1) and has an average addition mole number of alkylene oxide in a range of 60-150 and 2-hydroxyethyl acrylate (monomer 2), provided that a sum of the monomer 1 and the monomer 2 corresponds to ≥90 wt.% of all monomers composing the copolymer.
COPYRIGHT: (C)2010,JPO&INPITAbstract translation: 要解决的问题:提供一种水硬性组合物的分散维持剂,其表现出低的赋予初始流动性的效果和优异的流动性保持性和水硬性组合物的初始强度的发展。 解决方案:水硬性组合物的分散维持剂包括通过使由式(1)表示的特定链烯基醚单体1聚合而得到的共聚物,其平均加成摩尔数为环氧烷的范围为60-150 和丙烯酸2-羟乙酯(单体2),条件是单体1和单体2之和相当于构成共聚物的所有单体的≥90重量%。 版权所有(C)2010,JPO&INPIT
-
公开(公告)号:JP2010024130A
公开(公告)日:2010-02-04
申请号:JP2009140994
申请日:2009-06-12
Inventor: NAKA YOSHIHITO , FUJITA SHUICHI , HAMAI TOSHIMASA , HAMADA DAISUKE , SAGAWA KEIICHIRO
IPC: C04B24/26 , C04B24/22 , C04B28/02 , C04B103/40
CPC classification number: C04B24/226 , C04B24/2641 , C04B24/30 , C04B2103/408 , C08F220/06 , C08F220/28 , C08G10/02 , C08L61/02
Abstract: PROBLEM TO BE SOLVED: To provide a dispersant for hydraulic composition capable of suppressing reduction of dispersibility and increase of viscosity with passage of time to improve the workability, also available as an easy to handle product form. SOLUTION: The dispersant for hydraulic composition contains a polymer (A) of which at least 70 wt.% of the constituent monomer is expressed by formula (1): H 2 C=CHCOOCH 2 CH 2 OH and a naphthalenesulfonic acid formaldehyde condensate (B). COPYRIGHT: (C)2010,JPO&INPIT
Abstract translation: 要解决的问题:为了提供能够抑制分散性的降低和通过时间的粘度增加的水硬性组合物分散剂,以提高加工性,也可以作为易于处理的产品形式提供。 解决方案:用于水硬性组合物的分散剂包含聚合物(A),其中至少70重量%的构成单体由式(1)表示:H
2 = CHCOOCH 2 SB> 2 SB> OH和萘磺酸甲醛缩合物(B)。 版权所有(C)2010,JPO&INPIT
-
-
-
-
-
-
-
-
-