Abstract:
A method for integrally molding a metal and a resin and a metal-resin composite structure obtainable by the same are provided. The method comprises steps of: A) forming a nanopore in a surface of a metal sheet; and B) melting a thermoplastic resin on the surface of the metal sheet formed with the nanopore, and then injection molding the thermoplastic resin onto the surface of the metal sheet, in which the thermoplastic resin is a mixture of a main resin and a polyolefin resin, the main resin is a mixture of polyphenylene oxide and a polyamide, and the polyolefin resin has a melting point of about 65ºC to about 105ºC.
Abstract:
A method of manufacturing an amorphous alloy article is provided. The method comprises steps of: placing a prefabricated member made of a predetermined material having a different property from that of an amorphous alloy into a mold, in which the predetermined material is dissolvable in a predetermined solution; casting a fusant of the amorphous alloy into the mold such that the prefabricated member and the amorphous alloy are joined to form a semifinished product, in which a part of the prefabricated member is exposed out of the amorphous alloy; and placing the semifinished product into the predetermined solution to dissolve the prefabricated member.
Abstract:
An amorphous and a manufacturing method thereof are provided. The amorphous alloy may have a formula of ZraCubAlcMdNe, M is at least one selected from the group consisting of Ni, Fe, Co, Mn, Cr, Ti, Hf, Ta, Nb and rare earth elements; N is at least one selected from a group consisting of Ca, Mg, and C; 40≦a≦70, 15≦b≦35, 5≦c≦15, 5≦d≦15, 0≦e≦2, and a+b+c+d+e=100.
Abstract:
A method of joining an amorphous alloy material to a heterogeneous material and a composite formed by the same are provided. The method comprises steps of: placing a pre-formed piece made of one of the amorphous alloy material and the heterogeneous material into a mold; heating the other of the amorphous alloy material and the heterogeneous material to a predetermined temperature, and casting the other of the amorphous alloy material and the heterogeneous material into the mold to form a transition connection part joining the amorphous alloy material to the heterogeneous material and having a fusion welded structure, a microstructure reinforcing connection structure and a composite connection structure; and cooling the amorphous alloy material and the heterogeneous material at a rate higher than a critical cooling rate of the amorphous alloy material to obtain a composite formed by joining the amorphous alloy material to the heterogeneous material by the transition connection part.
Abstract:
A sealing assembly for a battery, a method of preparing the sealing assembly and a lithium ion battery are provided. The sealing assembly for a battery comprises: a ceramic ring (3) having a receiving hole (31), a metal ring (4) fitted over the ceramic ring (3) for sealing an open end of the battery, and a column (2) formed in the receiving hole (31) which comprises a metal-metal composite (21), wherein the metal-metal composite (21) comprises: a metal porous body, and a metal material filled in pores of the metal porous body.
Abstract:
A method for integrally molding a metal and a resin and a metal-resin composite structure obtainable by the same are provided. The method comprises forming a nanopore in a surface of a metal sheet; melting a thermoplastic resin on the surface of the metal sheet formed with the nanopore; and injection molding the thermoplastic resin onto the surface of the metal sheet. The thermoplastic resin includes a mixture of a main resin and a polyolefin resin, the main resin is a polycarbonate, and the polyolefin resin has a melting point of about 65° C. to about 105° C.
Abstract:
An amorphous and a manufacturing method thereof are provided. The amorphous alloy may have a formula of Zr a Cu b Al c M d N e , M is at least one selected from a group consisting of Ni, Fe, Co, Mn, Cr, Ti, Hf, Ta, Nb and rare earth element; N is at least one selected from a group consisting of Ca, Mg, and C; 40≤a≤70, 15≤b≤35, 5≤c≤15, 5≤d≤15, 0≤e≤5, and a+b+c+d+e=100.