公开(公告)号:CN103074787B
公开(公告)日:2016-12-28
申请号:CN201310004567.1
申请日:2013-01-07
Applicant: 浙江宏晟技术转让服务有限公司
Inventor: 段仲达
IPC: D07B1/10
CPC classification number: D07B1/062 , D07B2201/2002 , D07B2201/2048 , D07B2201/2059 , D07B2401/208 , D07B2801/12 , D07B2801/14
Abstract: 一种高渗胶率的高强度钢丝帘线,包括中间的一根芯股钢丝,其外围包绕由多根钢丝捻至形成的单层结构;所述的芯股钢丝截面为正四方形,且其外接圆直径(D芯)要大于外围绕的钢丝直径(d外)。该种帘线创造了丰富的间隙,能更好保证帘线在硫化时渗胶全面;同时由于芯股钢丝的异形,在帘线截面结构图中,正四边形棱角很稳定嵌入外围绕钢丝中,有效避免芯股钢丝自身转动;同时为制做大捻距提供保证,解决芯股硫化时冒芯问题,提高生产效率。
-
公开(公告)号:CN104968857A
公开(公告)日:2015-10-07
申请号:CN201380066790.7
申请日:2013-12-17
Applicant: 卡萨尔钢丝绳萨尔有限公司
Inventor: B·劳尔
CPC classification number: D07B1/0693 , D07B1/0686 , D07B1/165 , D07B5/00 , D07B5/007 , D07B7/02 , D07B7/027 , D07B2201/1016 , D07B2201/102 , D07B2201/1036 , D07B2201/1064 , D07B2201/2048 , D07B2201/2067 , D07B2207/4059 , D07B2801/60 , D07B2801/24
Abstract: 本发明涉及一种用于生产钢丝绳(1)的方法,其中,将绳股芯(3)压实并且随后将绳股绞合线(2)绞合到所述绳股芯(3)上,在绳股绞合线(2)绞合之前对绳股芯(3)进行锤击,以便使该绳股芯的表面(10)光滑。有利地,在绳股绞合线(2)绞合之前将塑料层施加到绳股芯(3)上,其中,绳股绞合线(2)优选在塑料层(7)被加热的情况下压入塑料层(7)。在本发明的优选实施形式中,所述绳股芯是绳芯(3)并且所述绳股绞合线是钢丝绳(1)的绞合线(2)或者所述绳股芯是绞合线芯(3)并且所述绳股绞合线是钢丝绳的绳芯的外部绳芯绞合线。通过借助锤子使绳股芯(3)变光滑可以实现比利用辊式压实机变紧凑的绳股芯(1)更大的钢丝绳(1)抗断强度。本发明还涉及所述钢丝绳(1)并且涉及一种用于生产所述钢丝绳(1)的设备。
-
公开(公告)号:CN102892947B
公开(公告)日:2015-03-11
申请号:CN201180024675.4
申请日:2011-05-06
Applicant: 米其林集团总公司 , 米其林研究和技术股份有限公司
IPC: D07B1/06
CPC classification number: D02G3/48 , D02G3/12 , D07B1/0626 , D07B1/0633 , D07B1/0646 , D07B1/0653 , D07B7/145 , D07B2201/2011 , D07B2201/2028 , D07B2201/2037 , D07B2201/2046 , D07B2201/2048 , D07B2201/2059 , D07B2201/2082 , D07B2205/2003 , D07B2205/2082 , D07B2207/205 , D07B2207/4072 , D07B2401/208 , D07B2501/2046 , D07B2801/12 , D07B2801/18 , D07B2801/16
Abstract: 本发明涉及用于制备金属帘线的方法,所述金属帘线具有“原位橡胶处理”类型的M+N+P构造的三个同心层(C1、C2、C3),亦即,所述帘线在其实际制备过程中从内部使用橡胶或橡胶组合物进行橡胶处理,所述帘线包括:由直径d1的M根丝线形成的直径dc的第一层或芯(C1)、在所述芯(C1)周围N根直径d2的丝线以螺距p2以螺旋形式缠绕在一起以形成第二层(C2)。此外,直径d3的P根丝线在第二层周围以螺距p3以螺旋形式缠绕在一起以形成第三层(C3)。所述方法包括如下步骤:为了在称为“组装点”的点处形成M+N构造的中间帘线或“芯股”,而在芯(C1)周围组装第二层(C2)的N根丝线的步骤;在所述组装点的上游和/或下游,通过使前述橡胶或所述橡胶组合物穿过至少一个挤出头而覆盖芯和/或芯股的步骤;以及在芯股(M+N)周围组装第三层(C3)的P根丝线以形成从内部进行橡胶处理的M+N+P构造的帘线的步骤。本发明的特征在于所述橡胶为熔融挤出的不饱和热塑性弹性体,优选热塑性苯乙烯(TPS)类型弹性体,如SBS、SBBS、SIS或SBIS嵌段共聚物。
-
公开(公告)号:CN102906330B
公开(公告)日:2015-02-04
申请号:CN201180024664.6
申请日:2011-05-06
Applicant: 米其林集团总公司 , 米其林研究和技术股份有限公司
CPC classification number: D02G3/02 , D07B1/062 , D07B1/0633 , D07B1/0646 , D07B1/0653 , D07B5/12 , D07B7/145 , D07B2201/2028 , D07B2201/2046 , D07B2201/2048 , D07B2201/2059 , D07B2201/2062 , D07B2201/2082 , D07B2205/2003 , D07B2205/2082 , D07B2207/205 , D07B2207/4072 , D07B2501/2046 , D07B2801/12 , D07B2801/18 , D07B2801/16
Abstract: 本发明涉及用于制备多层金属帘线的方法,所述多层金属帘线具有“原位橡胶处理”(即,在其制备过程中使用橡胶或橡胶组合物从内部进行橡胶处理)类型的多个丝线的同心层,所述多个同心层包括一个或多个内层和外层。所述方法包括至少如下步骤:至少一个用前述橡胶或所述橡胶组合物通过穿过至少一个挤出头而覆盖至少一个内层的步骤;以及在邻近的内层周围组装外层的丝线以形成从内部进行橡胶处理的多层帘线的步骤。本发明的特征在于所述橡胶为熔融挤出的不饱和热塑性弹性体,优选热塑性苯乙烯(TPS)类型弹性体如SBS、SBBS、SIS或SBIS嵌段共聚物。
-
公开(公告)号:CN101606207A
公开(公告)日:2009-12-16
申请号:CN200880004789.0
申请日:2008-01-16
Applicant: 贝卡尔特股份有限公司
Inventor: X·阿米尔斯
CPC classification number: H01B5/104 , D07B1/147 , D07B5/007 , D07B7/027 , D07B2201/2019 , D07B2201/2048 , D07B2201/2059 , D07B2201/2061 , H01B13/0006 , D07B2801/12 , D07B2801/14
Abstract: 提供了一种输电电缆,其包含具有至少两根独立涂覆并绞合的线材的电缆芯线,和围绕该芯线的导体,其中该芯线是紧压的。此外,提供了制造这类紧压钢芯的方法。
-
公开(公告)号:CN1276451A
公开(公告)日:2000-12-13
申请号:CN00109031.3
申请日:2000-06-02
Applicant: 弘德钢丝绳株式会社
CPC classification number: D07B1/0633 , D07B1/0613 , D07B1/062 , D07B1/0646 , D07B1/0653 , D07B3/106 , D07B7/025 , D07B2201/2003 , D07B2201/2007 , D07B2201/2023 , D07B2201/2036 , D07B2201/2048 , D07B2201/2059 , D07B2207/203 , D07B2207/205 , D07B2207/208 , D07B2207/209 , D07B2501/2046 , D07B2501/2076 , D07B2801/12 , D07B2801/14
Abstract: 一种加强钢丝绳,它是将镀黄铜外部元件钢丝绕着扁平螺旋形扭绞芯体捻合形成,芯体扭绞方向与钢丝绳捻合方向相同或相反。芯体节距设成使得在钢丝绳节距内芯体被扭绞0.2至2次,从而形成足够间隙。由于间隙的存在,橡胶材料完全填充在钢丝绳中,钢丝绳在抗弯曲疲劳性、橡胶渗透性、空气渗透率、橡胶附着力、相对橡胶的老化附着力、钢丝镀黄铜表面的保护及制造橡胶制品时的可加工性得以改进。本发明还涉及制造钢丝绳的方法和装置。
-
27.
公开(公告)号:US20140345098A1
公开(公告)日:2014-11-27
申请号:US14455899
申请日:2014-08-09
Applicant: Hjortur Erlendsson
Inventor: Hjortur Erlendsson
IPC: D07B7/02
CPC classification number: D07B5/12 , D04C1/12 , D07B1/025 , D07B1/185 , D07B7/165 , D07B2201/102 , D07B2201/1096 , D07B2201/2048 , D07B2201/2053 , D07B2201/2066 , D07B2201/2067 , D07B2201/2074 , D07B2201/209 , D07B2201/2095 , D07B2201/2096 , D07B2205/2003 , D07B2205/2014 , D07B2205/2042 , D07B2205/2064 , D07B2205/2096 , D07B2207/405 , D07B2207/4059 , D07B2207/4068 , D07B2301/258 , D07B2301/3591 , D07B2401/205 , D07B2401/2055 , D07B2501/2038 , D07B2501/2061 , D07B2801/10 , D07B2801/60 , D07B2801/24 , D07B2801/14 , D07B2801/16
Abstract: Disclosed is a method for producing a high strength synthetic strength member (7) containing rope (1) capable of being used with powered blocks where such rope has lighter weight and similar or greater strength than steel wire strength member containing ropes used with powered blocks. Disclosed also is the product resulting from such method. The product includes a synthetic strength member, a first synthetic portion (9) and a second synthetic portion. The first synthetic pillion is enclosed within the strength member and the second synthetic portion is situated external the strength member. At least a portion of the second synthetic portion also is situated internal a sheath (8) formed about the strength member. The second synthetic portion has a minimal of 8% at a temperature of between negative 20 and negative 15° C.
Abstract translation: 公开了一种用于制造能够与动力块一起使用的绳索(1)的高强度合成强度构件(7)的方法,其中该绳索具有比具有动力块的绳索的钢丝绳强度构件更轻的重量和相似或更大的强度。 还公开了由这种方法产生的产品。 该产品包括合成强度构件,第一合成部分(9)和第二合成部分。 第一合成柱被包围在强度构件内,第二合成部分位于加强构件外部。 第二合成部分的至少一部分也位于围绕强度构件形成的护套(8)的内部。 第二合成部分在负20和负15℃之间的温度下具有最小的8%。
-
公开(公告)号:US06622766B1
公开(公告)日:2003-09-23
申请号:US10165073
申请日:2002-06-07
Applicant: Donald William Baldwin, Jr.
Inventor: Donald William Baldwin, Jr.
IPC: B60K1504
CPC classification number: D07B1/0613 , B60C15/04 , B60C2200/14 , D07B2201/1004 , D07B2201/102 , D07B2201/1036 , D07B2201/104 , D07B2201/2023 , D07B2201/2024 , D07B2201/2039 , D07B2201/2048 , D07B2201/2059 , D07B2201/2061 , D07B2205/306 , D07B2205/3085 , D07B2501/2053 , D07B2801/14
Abstract: A light weight cable bead core 30 is described having an inner core 33 made of a metal wire 34 with an outer sheath 35 of steel cord wires 36. Each cord 36 is made of a plurality of filaments 37. The bead core 30 is particularly suited for heavy-duty service conditions in tires 100 for aircraft, off-road equipment, and commercial trucks.
Abstract translation: 描述了一种重量轻的电缆胎圈芯30,其具有由金属线34制成的内芯33,其具有钢帘线36的外护套35.每个帘线36由多根细丝37制成。胎圈芯30特别适合 用于飞机,越野设备和商用卡车的轮胎100的重型服务条件。
-
公开(公告)号:US1916135A
公开(公告)日:1933-06-27
申请号:US31684128
申请日:1928-11-02
Applicant: PLYMOUTH CORDAGE CO
Inventor: GATES BERNARD W
IPC: D07B1/06
CPC classification number: D07B1/0686 , D07B2201/2048 , D07B2201/2066 , D07B2801/24
-
30.
公开(公告)号:WO2004020732A3
公开(公告)日:2005-04-07
申请号:PCT/IS0300025
申请日:2003-09-01
Applicant: HAMPIDJAN HF , ERLENDSSON HJORTUR
Inventor: ERLENDSSON HJORTUR
CPC classification number: D07B7/16 , D07B1/025 , D07B1/165 , D07B5/12 , D07B2201/102 , D07B2201/1096 , D07B2201/2048 , D07B2201/2053 , D07B2201/2066 , D07B2201/2088 , D07B2201/209 , D07B2205/2003 , D07B2205/2014 , D07B2205/205 , D07B2205/2064 , D07B2205/2096 , D07B2205/3025 , D07B2207/4045 , D07B2207/4059 , D07B2401/205 , D07B2401/2055 , D07B2501/2038 , D07B2801/24 , D07B2801/14 , D07B2801/22 , D07B2801/16 , D07B2801/60
Abstract: A rope with high stiffness and breaking strength is provided. The rope is produced by providing a stiff core (1) and fibre rope jacket (4) surrounding the core and by changing the phase condition of the core while stretching the rope, such that inside vacancies between the fibre rope jacket (4) and the core (1)are eliminated permanently. A method and apparatus for producing such rope are provided, wherein the core (1) is heated up and stretched such that it will be permanently elongated. In a preferred embodiment the thermoplastic core (1) changes from solid phase to liquid phase by means of heating. While in liquid phase the core material adapts to the encapsulating space of the surrounding sheet. The rope is then cooled down under tension until the core has returned to solid phase.
Abstract translation: 提供了具有高刚度和断裂强度的绳索。 该绳索是通过提供围绕该芯的硬芯(1)和纤维绳护套(4)而产生的,并且通过在拉伸绳索的同时改变芯的相位状态,使得纤维绳护套(4)和 核心(1)被永久消除。 提供了一种用于生产这种绳索的方法和装置,其中芯(1)被加热和拉伸,使得其将被永久拉长。 在优选实施例中,热塑性芯(1)通过加热从固相变为液相。 在液相中,芯材料适应于周围片材的封装空间。 然后在张力下将绳索冷却,直到芯已经返回到固相。
-
-
-
-
-
-
-
-
-