Propylene-based polymer composition
    293.
    发明授权

    公开(公告)号:US09969870B2

    公开(公告)日:2018-05-15

    申请号:US15313456

    申请日:2015-04-28

    Abstract: A propylene polymer composition comprising: A) from 81 wt % to 91 wt % of a propylene ethylene copolymer containing from 1.0 wt % to 3.5 wt % of ethylene derived units having a fraction soluble in xylene at 25° C. comprised between 10 wt % and 3 wt %; and a melt flow rate ranging from 5 to 50 g/10 min; B) from 9 wt % to 19 wt %, of a copolymer of propylene and ethylene with from 21.0 wt % to 31.0 wt % of ethylene derived units; the sum A)+B) being 100; the composition having an melt flow rate ranging from 20 to 35 g/10 min; the xylene soluble fraction to 25° C. ranging from 13.0 wt % to 25.0 wt % and the intrinsic viscosity of the fraction soluble in xylene at 25° C. ranging from 0.7 dl/g to 1.9 dl/g.

    CONTAINERS COMPRISING PROPYLENE-BASED TERPOLYMERS

    公开(公告)号:US20170291972A1

    公开(公告)日:2017-10-12

    申请号:US15511976

    申请日:2015-09-09

    Abstract: The present disclosure provides an article of manufacture made from or containing a propylene-based terpolymer, having (i) ethylene-derived units in the range from about 0.5 wt. % to about 1.8 wt. %; (ii) 1-butene-derived units in the range from about 1.5 wt. % to about 2.5 wt. %; (iii) a ratio of C2 wt %/C4 wt % in the range from about 0.40 to about 0.80, wherein C2 wt % is the weight percent of ethylene-derived units and C4 wt % is the weight percent of 1-butene-derived units; (iv) a melt flow rate in the range from about 30 g/10 min to about 80 g/10 min; (v) a xylene soluble fraction at 25° C. lower than about 5.0 wt. %; and (vi) a melting point higher than about 140° C. The article can be a container, which can be used for food applications.

    POLYOLEFIN NANOCOMOSITES MATERIALS
    297.
    发明申请

    公开(公告)号:US20170275436A1

    公开(公告)日:2017-09-28

    申请号:US15591979

    申请日:2017-05-10

    Abstract: A polyolefin nanocomposite material comprising the following components: (A) a crystalline or semi-crystalline polyolefin resin; and (B) a nanosized mineral filler comprising or substantially consisting of a hydrotalcite, wherein the amount of the hydrotalcite is from 0.02 to 6 parts by weight per 100 parts by weight of the nanocomposite material, and the ratio MFR (1)/MFR (2) of the melt flow rate value MFR (1) of component (A) to the melt flow rate value MFR (2) of the polyolefin nanocomposite material is of at least 1.02, characterized in that the said polyolefin nanocomposite material includes a compatibilizer the dispersion of the mineral filler (B) and compatibilizer in the polyolefin resin is produced at shear mixing rates from 30 to 300 sec−1,