311.Lubricant additive mixtures of antimony thioantimonate and antimony trioxide 失效
Title translation: 硫代锑酸锑和三氧化锑的润滑添加剂混合物公开(公告)号:US4741845A
公开(公告)日:1988-05-03
申请号:US937261
申请日:1986-12-03
Applicant: James P. King
Inventor: James P. King
IPC: C10M20060101 , C10M103/06 , C10M125/00 , C10M125/24 , C10N10/10
CPC classification number: C10M125/24 , C10M103/06 , C10M2201/0603 , C10M2201/0613 , C10M2201/062 , C10M2201/0623 , C10M2201/065 , C10M2201/0653 , C10M2201/0663 , C10M2201/0803 , C10M2201/085 , C10M2201/0853 , C10M2201/0863 , C10M2201/0873 , C10M2201/1006 , C10M2201/1023 , C10M2201/1033 , C10M2201/1053 , C10M2201/123 , C10M2217/00 , C10M2217/02 , C10M2217/04 , C10M2221/00 , C10N2240/00 , C10N2240/22 , C10N2240/30 , C10N2240/50 , C10N2240/52 , C10N2240/54 , C10N2240/56 , C10N2240/58 , C10N2240/60 , C10N2240/66 , C10N2250/121
Abstract: A lubricant additive that includes antimony thioantimonate and antimony trioxide in a specified ratio for enhancing the extreme pressure, antiwear, and antiabrasive properties of conventional lubricants as well as for use in lubrication of a wide variety of lubricated contact surfaces.
Abstract translation: 一种润滑剂添加剂,其特征在于比例含有硫代锑酸锑和三氧化锑,以提高常规润滑剂的极压,抗磨损和抗磨损性能,并用于各种润滑接触表面的润滑。
-
公开(公告)号:US4655945A
公开(公告)日:1987-04-07
申请号:US823254
申请日:1986-01-28
Applicant: Peter J. Balsells
Inventor: Peter J. Balsells
IPC: C10M111/00 , C10M147/02
CPC classification number: C10M111/00 , C10M2201/00 , C10M2201/003 , C10M2201/0403 , C10M2201/041 , C10M2201/0413 , C10M2201/042 , C10M2201/0423 , C10M2201/0433 , C10M2201/05 , C10M2201/053 , C10M2201/0603 , C10M2201/061 , C10M2201/0613 , C10M2201/0623 , C10M2201/0653 , C10M2201/0663 , C10M2201/0803 , C10M2201/0853 , C10M2201/0863 , C10M2201/0873 , C10M2201/1006 , C10M2201/1023 , C10M2201/1033 , C10M2201/1053 , C10M2201/12 , C10M2201/123 , C10M2201/16 , C10M2201/18 , C10M2209/00 , C10M2209/02 , C10M2209/10 , C10M2209/1013 , C10M2209/102 , C10M2209/1023 , C10M2211/06 , C10M2213/00 , C10M2213/02 , C10M2213/023 , C10M2213/043 , C10M2213/0606 , C10M2213/062 , C10M2213/0623 , C10N2240/02
Abstract: The present invention includes a method for the manufacture of a bearing seal which includes providing a polymer and/or a filler coated with a polymer and thereafter heating the coated filler to bond the copolymer to the filler. Following cooling of the coated filler, it is pulverized and added to granular polytetrafluoroethylene. This admixture is then mixed to obtain a uniform blend and thereafter shaped by compacting and heating into a preselected form. Fillers suitable for the present invention may be carbon, metal, glass, carbide, disulfide, polymeric, polyester fluoride and ceramic fibers.
Abstract translation: 本发明包括制造轴承密封件的方法,其包括提供涂覆有聚合物的聚合物和/或填料,然后加热涂覆的填料以将共聚物粘合到填料上。 在涂覆的填料冷却后,将其粉碎并加入到颗粒状聚四氟乙烯中。 然后将该混合物混合以获得均匀的共混物,然后通过压实和加热成型为预选形式。 适用于本发明的填料可以是碳,金属,玻璃,碳化物,二硫化物,聚合物,聚酯氟化物和陶瓷纤维。
-
公开(公告)号:US4575429A
公开(公告)日:1986-03-11
申请号:US677828
申请日:1984-12-04
Applicant: Charles B. Jacobson
Inventor: Charles B. Jacobson
IPC: C08K3/00 , C08K3/08 , C08K3/34 , C08L27/18 , C10M111/04 , C10N10/08 , C10N40/02 , F16C33/04 , F16C33/12 , F16C33/20
CPC classification number: F16C33/201 , C10M111/04 , F16C33/206 , C10M2201/00 , C10M2201/05 , C10M2201/053 , C10M2201/0603 , C10M2201/061 , C10M2201/0613 , C10M2201/0623 , C10M2201/0653 , C10M2201/0663 , C10M2201/0803 , C10M2201/0853 , C10M2201/0863 , C10M2201/0873 , C10M2201/1006 , C10M2201/1023 , C10M2201/103 , C10M2201/1033 , C10M2201/1053 , C10M2201/123 , C10M2201/16 , C10M2201/18 , C10M2211/06 , C10M2213/00 , C10M2213/02 , C10M2213/023 , C10M2213/043 , C10M2213/0606 , C10M2213/062 , C10M2213/0623 , C10M2217/00 , C10M2217/02 , C10M2217/04 , C10M2217/044 , C10M2217/045 , C10M2221/00 , C10M2221/003 , C10M2221/025 , C10M2221/0405 , C10N2210/04 , C10N2240/02 , Y10T428/12007 , Y10T428/12042 , Y10T428/12056
Abstract: Improved composite bearings are provided employing cold forming and sintering techniques. Improvements in compositions for impregnating porous layers of composite bearings are provided comprising lead or lead alloy, perfluorinated polymer, particulate thermoplastic polymer and clay in particular proportions. When such materials are formed into bearings and subsequently sintered, improved resistance to stripping and wear is provided.
Abstract translation: 使用冷成型和烧结技术提供改进的复合轴承。 提供了用于浸渍复合轴承的多孔层的组合物的改进,其包括铅或铅合金,全氟化聚合物,颗粒状热塑性聚合物和特定比例的粘土。 当这种材料形成轴承并随后烧结时,提供了提高的剥离和磨损性。
-
公开(公告)号:US4432883A
公开(公告)日:1984-02-21
申请号:US329009
申请日:1981-12-09
Applicant: Allen F. Denzine , William E. F. Thurber, Jr.
Inventor: Allen F. Denzine , William E. F. Thurber, Jr.
IPC: C10M111/04 , E21B10/22 , F16C33/20 , C10M7/28 , C10M7/52
CPC classification number: E21B10/22 , C10M111/04 , F16C33/201 , C10M2201/00 , C10M2201/0413 , C10M2201/0423 , C10M2201/05 , C10M2201/053 , C10M2201/0603 , C10M2201/061 , C10M2201/0613 , C10M2201/0623 , C10M2201/0653 , C10M2201/0663 , C10M2201/0803 , C10M2201/0853 , C10M2201/0863 , C10M2201/0873 , C10M2201/1006 , C10M2201/1023 , C10M2201/1033 , C10M2201/1053 , C10M2201/123 , C10M2201/16 , C10M2201/18 , C10M2211/06 , C10M2213/00 , C10M2213/02 , C10M2213/023 , C10M2213/043 , C10M2213/0606 , C10M2213/062 , C10M2213/0623 , C10M2217/0403 , C10M2217/0415 , C10M2217/042 , C10M2217/0425 , C10M2217/043 , C10M2217/0435 , C10M2217/044 , C10M2217/0443 , C10M2217/045 , C10M2217/0453 , C10M2217/0465 , C10M2221/003 , C10M2221/02 , C10M2221/025 , C10M2221/0405
Abstract: A part is made of a material comprising less than 90% by weight of a polymer selected from the group consisting of polytetrafluoroethylene, polyurethane, nitrile, fluoroelastomer, and polyphenylene sulfide; and more than 10% by weight of another material, comprising about 15% to 60% by volume of grains of titanium carbide dispersed through a metal matrix.
Abstract translation: 部件由包含小于90重量%的选自聚四氟乙烯,聚氨酯,腈,含氟弹性体和聚苯硫醚的聚合物的材料制成; 和超过10重量%的另一种材料,其包含通过金属基体分散的约15体积%至60体积%的碳化钛颗粒。
-
公开(公告)号:US4379062A
公开(公告)日:1983-04-05
申请号:US318814
申请日:1981-11-06
Applicant: Raymond D. Prengaman
Inventor: Raymond D. Prengaman
IPC: C10M111/00 , C10M1/10
CPC classification number: C10M111/00 , C10M2201/05 , C10M2201/053 , C10M2201/0603 , C10M2201/0613 , C10M2201/062 , C10M2201/0623 , C10M2201/063 , C10M2201/0653 , C10M2201/0663 , C10M2201/0803 , C10M2201/0853 , C10M2201/0863 , C10M2201/0873 , C10M2201/1006 , C10M2201/102 , C10M2201/1023 , C10M2201/1033 , C10M2201/105 , C10M2201/1053 , C10M2201/123 , C10M2203/1006 , C10M2203/1025 , C10M2203/1045 , C10M2203/1065 , C10M2203/1085 , C10N2210/02 , C10N2240/00 , C10N2240/22 , C10N2240/30 , C10N2240/50 , C10N2240/52 , C10N2240/54 , C10N2240/56 , C10N2240/58 , C10N2240/60 , C10N2240/66
Abstract: A thread sealing and lubricating composition which can be employed at elevated temperatures without carburization of stainless steel fittings is disclosed. The composition contains 8-25% finely divided copper flakes, 5-20% finely divided aluminum particles, and 4-15% non-metallic, non-carbon powder suspended in a petroleum vehicle. The preferred composition contains 10% copper flakes, 5% aluminum powder, 5% non-metallic powder and 80% viscous petroleum vehicle.
Abstract translation: 公开了一种螺纹密封和润滑组合物,其可以在高温下使用,而不会使不锈钢配件渗碳。 该组合物含有8-25%细碎的铜薄片,5-20%细碎的铝颗粒和悬浮在石油载体中的4-15%非金属非碳粉末。 优选的组合物包含10%的铜薄片,5%的铝粉,5%的非金属粉末和80%的粘稠的石油载体。
-
316.Antifriction paste and solid antifriction coating prepared from same 失效
Title translation: 减摩膏和固体抗磨涂层由同样制备公开(公告)号:US4329238A
公开(公告)日:1982-05-11
申请号:US62509
申请日:1979-07-30
Applicant: Alla K. Mitrofanova , Militsa N. Zelenskaya
Inventor: Alla K. Mitrofanova , Militsa N. Zelenskaya
IPC: C10M169/04 , C10M5/02
CPC classification number: F16C33/201 , C10M169/04 , C10M2201/041 , C10M2201/042 , C10M2201/05 , C10M2201/0603 , C10M2201/0613 , C10M2201/0623 , C10M2201/065 , C10M2201/0653 , C10M2201/066 , C10M2201/0663 , C10M2201/0803 , C10M2201/084 , C10M2201/0853 , C10M2201/0863 , C10M2201/0873 , C10M2201/1006 , C10M2201/102 , C10M2201/1023 , C10M2201/1033 , C10M2201/1053 , C10M2201/123 , C10M2209/1003 , C10M2209/101 , C10M2215/04 , C10M2215/26 , C10M2217/046 , C10M2217/06
Abstract: An antifriction paste containing epoxy resin, molybdenum disulphide, graphite, aluminum, copper, alumosilicate and polyethylenepolyamine, the components being used in the following proportions (in parts by weight):epoxy resin: 40-80molybdenum disulphide: 15-30graphite: 10-15aluminum: 5-10copper: 5-10alumosilicate: 8-15polyethylenepolyamine: 5-10.The antifriction paste may also contain a solvent for the epoxy resin in an amount from 5 to 30 parts by weight. This paste is suitable for both small-and large-size friction assemblies. On the basis of this paste a solid lubricating coating with high antifriction performance is produced. Thus, a coefficient of sliding friction f.sub.fr. at a sliding speed V=0.06 m/s at a load P=10 kgf/cm.sup.2 is 0.2; linear wear rate I.sub.h under the same conditions is 1.0.10.sup.-9, and service life is as high as 500 km.
Abstract translation: 含有环氧树脂,二硫化钼,石墨,铝,铜,铝硅酸盐和聚亚乙基多胺的减摩膏,该组分按以下比例(以重量份计)使用:环氧树脂:40-80二硫化钼:15-30石墨:10 -15铝:5-10铜:5-10铝硅酸盐:8-15聚亚乙基多胺:5-10。 减摩膏也可以含有5〜30重量份的环氧树脂用溶剂。 该浆料适用于小型和大型摩擦组件。 在该糊状物的基础上,产生具有高抗摩擦性能的固体润滑涂层。 因此,滑动摩擦系数ffr。 在载荷P = 10kgf / cm2时的滑动速度V = 0.06m / s为0.2; 在相同条件下的线性磨损率Ih为1.0.10-9,使用寿命高达500公里。
-
公开(公告)号:US2490949A
公开(公告)日:1949-12-13
申请号:US78029947
申请日:1947-10-16
Applicant: DE LORENZO JOSEPH P
Inventor: DE LORENZO JOSEPH P
IPC: C10M111/00 , C10M169/04
CPC classification number: C10M111/00 , C10M101/02 , C10M103/06 , C10M105/14 , C10M105/24 , C10M107/34 , C10M169/04 , C10M2201/0603 , C10M2201/0613 , C10M2201/0623 , C10M2201/0653 , C10M2201/0663 , C10M2201/0803 , C10M2201/0853 , C10M2201/0863 , C10M2201/0873 , C10M2201/1006 , C10M2201/102 , C10M2201/1023 , C10M2201/1033 , C10M2201/1053 , C10M2201/123 , C10M2203/1006 , C10M2203/1025 , C10M2203/1045 , C10M2203/1065 , C10M2203/1085 , C10M2207/022 , C10M2207/0225 , C10M2207/1203 , C10M2207/1213 , C10M2207/125 , C10M2207/1253 , C10M2207/129 , C10M2207/163 , C10M2207/183 , C10M2207/203 , C10M2207/243 , C10M2209/1033 , C10M2209/104 , C10M2209/1045 , C10M2209/105 , C10M2209/1055 , C10M2209/1065 , C10M2209/1075 , C10M2209/1085 , C10M2209/1095 , C10N2210/00 , C10N2210/01 , C10N2210/02 , C10N2210/03 , C10N2240/00 , C10N2240/22 , C10N2240/30 , C10N2240/50 , C10N2240/52 , C10N2240/54 , C10N2240/56 , C10N2240/58 , C10N2240/60 , C10N2240/66
-
公开(公告)号:US1917089A
公开(公告)日:1933-07-04
申请号:US46471430
申请日:1930-06-28
Applicant: BOUGHTON WILLIS A
Inventor: BOUGHTON WILLIS A
IPC: C10M103/06 , C10M173/02
CPC classification number: C10M103/06 , C10M125/24 , C10M125/26 , C10M173/02 , C10M2201/02 , C10M2201/0603 , C10M2201/0613 , C10M2201/0623 , C10M2201/0653 , C10M2201/0663 , C10M2201/0803 , C10M2201/085 , C10M2201/0853 , C10M2201/0863 , C10M2201/087 , C10M2201/0873 , C10M2201/10 , C10M2201/1006 , C10M2201/102 , C10M2201/1023 , C10M2201/1033 , C10M2201/105 , C10M2201/1053 , C10M2201/123 , C10N2250/02
-
公开(公告)号:TW324739B
公开(公告)日:1998-01-11
申请号:TW085105769
申请日:1996-05-15
Applicant: 提姆克有限公司
Inventor: 漢斯–魯道夫.史陶伯
IPC: C10M
CPC classification number: C10M169/044 , C10M103/00 , C10M103/02 , C10M103/06 , C10M125/24 , C10M125/26 , C10M145/14 , C10M145/40 , C10M2201/003 , C10M2201/02 , C10M2201/0403 , C10M2201/041 , C10M2201/0413 , C10M2201/042 , C10M2201/0423 , C10M2201/0433 , C10M2201/0603 , C10M2201/0613 , C10M2201/0623 , C10M2201/0653 , C10M2201/0663 , C10M2201/0803 , C10M2201/085 , C10M2201/0853 , C10M2201/0863 , C10M2201/087 , C10M2201/0873 , C10M2201/10 , C10M2201/1006 , C10M2201/102 , C10M2201/1023 , C10M2201/1033 , C10M2201/105 , C10M2201/1053 , C10M2201/12 , C10M2201/123 , C10M2209/084 , C10M2209/12 , C10N2240/402 , C10N2240/403 , C10N2240/404 , C10N2240/405 , C10N2240/406 , C10N2240/407 , C10N2240/408 , C10N2240/409
Abstract: 本發明是關於一種使用在表面溫度為800℃到1300℃之細工品的潤滑劑組成物。
Abstract in simplified Chinese: 本发明是关于一种使用在表面温度为800℃到1300℃之细工品的润滑剂组成物。
-
公开(公告)号:TW296990B
公开(公告)日:1997-02-01
申请号:TW084102769
申请日:1995-03-22
Applicant: 日新製鋼股份有限公司
IPC: B21B
CPC classification number: C10M173/02 , B21B45/0242 , C10M103/06 , C10M125/10 , C10M145/12 , C10M145/14 , C10M145/40 , C10M2201/02 , C10M2201/0603 , C10M2201/0613 , C10M2201/062 , C10M2201/0623 , C10M2201/0653 , C10M2201/0663 , C10M2201/0803 , C10M2201/0853 , C10M2201/0863 , C10M2201/0873 , C10M2201/1006 , C10M2201/1023 , C10M2201/1033 , C10M2201/1053 , C10M2201/123 , C10M2209/082 , C10M2209/084 , C10M2209/12 , C10N2240/402 , C10N2240/403 , C10N2240/404 , C10N2240/405 , C10N2240/406 , C10N2240/407 , C10N2240/408 , C10N2240/409 , C10N2250/02
Abstract: 一種高鉻不銹鋼之熱軋用潤滑劑,即於進行高鉻不銹鋼之熱軋之際,針對與該被軋製材料接觸之軋輥表面,至少在進行該軋製之間,連續供應之熱軋用潤滑劑,可提供溶解有由水溶性高分子製成之增粘劑在水中而成之粘性水溶液中,將平均粒徑 0.1 μm以上,不到 1 之氫氧化鐵粉末,以10~40重量%之比率,分散懸浮在其中而成,且公稱粘度( nominal viscosity )有1000~5000 cP(厘泊: cc ntipose)者。
Abstract in simplified Chinese: 一种高铬不锈钢之热轧用润滑剂,即于进行高铬不锈钢之热轧之际,针对与该被轧制材料接触之轧辊表面,至少在进行该轧制之间,连续供应之热轧用润滑剂,可提供溶解有由水溶性高分子制成之增粘剂在水中而成之粘性水溶液中,将平均粒径 0.1 μm以上,不到 1 之氢氧化铁粉末,以10~40重量%之比率,分散悬浮在其中而成,且公称粘度( nominal viscosity )有1000~5000 cP(厘泊: cc ntipose)者。
-
-
-
-
-
-
-
-
-