A resin composition for powder coatings
    371.
    发明公开
    A resin composition for powder coatings 失效
    粉末涂料的树脂组合物

    公开(公告)号:EP0480120A3

    公开(公告)日:1993-01-13

    申请号:EP91105085.4

    申请日:1991-03-28

    Abstract: There is disclosed a resin composition for powder coatings, which comprises a blend of two acrylic resins being obtained by polymerizing a proscribed amount of monomer component (a-1) represented by formula (I) and a prescribed amount of another monomer component (a-2), respectively, and having different polymerization degrees represented by viscosities at 140°C and a polybasic acid compound in 1.5 to 0.5 equivalent ratio of the glycidyl groups in said acrylic resins to the acid groups in the polybasic acid compound.
    wherein R 1 and R 2 each represent a hydrogen atom or a lower alkyl group. Disclosure described provides a resin composition for powder coatings that can form a coating film having a mat smooth appearance and excellent in flexibility as shown Du pont impact resistance and the Ericksen test as well as excellent in nail scratch resistance.

    A resin composition for powder coatings
    373.
    发明公开
    A resin composition for powder coatings 失效
    HarzmischungfürPulverlacke。

    公开(公告)号:EP0480120A2

    公开(公告)日:1992-04-15

    申请号:EP91105085.4

    申请日:1991-03-28

    Abstract: There is disclosed a resin composition for powder coatings, which comprises a blend of two acrylic resins being obtained by polymerizing a proscribed amount of monomer component (a-1) represented by formula (I) and a prescribed amount of another monomer component (a-2), respectively, and having different polymerization degrees represented by viscosities at 140°C and a polybasic acid compound in 1.5 to 0.5 equivalent ratio of the glycidyl groups in said acrylic resins to the acid groups in the polybasic acid compound.
    wherein R 1 and R 2 each represent a hydrogen atom or a lower alkyl group. Disclosure described provides a resin composition for powder coatings that can form a coating film having a mat smooth appearance and excellent in flexibility as shown Du pont impact resistance and the Ericksen test as well as excellent in nail scratch resistance.

    Abstract translation: 公开了一种用于粉末涂料的树脂组合物,其包含两种丙烯酸树脂的共混物,其通过将受限量的由式(I)表示的单体组分(a-1)和规定量的另一单体组分(a- 2),并且具有以140℃的粘度表示的不同聚合度和多元酸化合物,所述丙烯酸树脂中的缩水甘油基与多元酸化合物中的酸基的当量比为1.5至0.5当量比。 其中R1和R2各自表示氢原子或低级烷基。 所公开的公开内容提供了一种用于粉末涂料的树脂组合物,其可以形成具有平滑外观和柔韧性优异的涂膜,如杜邦耐冲击性和埃克森克氏试验以及耐刮擦性优异。

    Durch Protonieren mit Säure wasserverdünnbares Bindemittel, dessen Herstellung und Verwendung
    374.
    发明公开
    Durch Protonieren mit Säure wasserverdünnbares Bindemittel, dessen Herstellung und Verwendung 失效
    通过用酸的水可稀释粘合剂,其制备和用途质子化。

    公开(公告)号:EP0225530A2

    公开(公告)日:1987-06-16

    申请号:EP86116191.7

    申请日:1986-11-22

    Abstract: Die Erfindung betrifft durch Protonieren mit Säure wasserverdünnbare Bindemittel, Verfahren zu deren Herstellung und deren Verwendung.
    Diese Bindemittel sind durch Umsetzung eines

    A) Reaktionsprodukts einer

    a) carboxylgruppenhaltigen Komponente, bestehend aus einem

    a1) carboxylgruppenhaltigen Butadien/Acrylnitrilcopolymeren mit einem Molekulargewicht von 500 bis 8000,
    gegebenenfalls im Gemisch mit
    a2) einer von a1) verschiedenen Dicarbonsäure und gegebenenfalls
    a3) einer Monocarbonsäure und einem

    b) diprimären und/oder primären/sekundären Amin mit der Maßgabe, daß 0,7 bis 5 Mol des diprimären und/oder des primären/sekundä­ren Amins pro Mol Carboxylgruppen der Komponente a) eingesetzt werden

    mit mindestens einem
    B) Epoxidharz mit einem mittleren Molekulargewicht von 300 bis 6000 und im Mittel 1,5 bis 3,0 Epoxidgruppen pro Molekül und gegebenenfalls
    C) einem sekundären aliphatischen oder cycloaliphatischen Amin
    erhältlich.
    Sie eignen sich in Kombination mit einem Vernetzer als Überzugsmittel, insbesondere für die kathodische Elektrotauchlackierung.

    Abstract translation: 本发明涉及水可稀释的通过质子化与酸结合剂,它们的制备方法以及它们的用途。 这些粘合剂是通过使一个)的反应产物获得的a)成分组成的a1的羧基)的丁二烯/丙烯腈共聚物具有分子量500至8000,任选地与混合含羧基,A2)A1中的一个)不同的二羧酸和任选的a3)的 一元羧酸和一b)二伯和/或伯/仲胺,条件是所述二伯的0.7至5摩尔和/或每个组分a)的羧基基团的摩尔伯/仲胺与至少一个所使用的,b) 环氧树脂可用的300平均分子量一个仲脂族或脂环族胺6000和每分子平均1.5〜3.0个环氧基团和,任选地,C)。 它们适用于与交联剂作为涂布剂,尤其是用于阴极电沉积涂层组合。

    FLEXIBLE PRINTED MATERIAL
    375.
    发明申请

    公开(公告)号:WO2021011006A1

    公开(公告)日:2021-01-21

    申请号:PCT/US2019/042427

    申请日:2019-07-18

    Abstract: A method of forming a flexible printed material is described. The method comprises applying a layer of primer onto a flexible substrate; electrostatically printing onto the layer of primer a liquid electrostatic ink composition; applying a curable overprint varnish composition onto the printed electrostatic ink composition and curing the overprint varnish composition using electron beam irradiation. The curable overprint varnish composition comprises an ethylenically unsaturated monomer, an ethylenically unsaturated oligomer, or mixtures thereof, and less than 10 wt.% of a cross-linking additive based on the total weight of the curable overprint varnish composition. A flexible package comprising the flexible printed material is also described.

    有機EL表示装置
    376.
    发明申请

    公开(公告)号:WO2018123853A1

    公开(公告)日:2018-07-05

    申请号:PCT/JP2017/046098

    申请日:2017-12-22

    Abstract: 有機EL表示装置は、(A)アルカリ可溶性樹脂、(B)着色剤、(C)ラジカル重合性化合物、及び(D)光重合開始剤を含有する感光性樹脂組成物であり、(A)アルカリ可溶性樹脂が、(A-1)カルボキシル基を有するアルカリ可溶性樹脂であり、さらに、前記感光性樹脂組成物を硬化した硬化物の、飛行時間型二次イオン質量分析により測定される不揮発成分中の金属元素および/またはハロゲン元素の含有量の総和が1×10 17 atom/cm 3 以上1×10 22 atom/cm 3 以下であり、少なくとも基板、第一電極、第二電極、発光画素、平坦化層及び画素分割層で構成された有機EL素子のうち、平坦化層および/または画素分割層に配置された。

    水性塗料組成物
    377.
    发明申请
    水性塗料組成物 审中-公开
    含水涂料组合物

    公开(公告)号:WO2017131102A1

    公开(公告)日:2017-08-03

    申请号:PCT/JP2017/002779

    申请日:2017-01-26

    Abstract: 本発明は、低温硬化であっても優れた塗膜性能を有する塗膜を形成することができる、水性塗料組成物を提供することを課題とする。 本発明は、水酸基およびカルボキシル基を有する水性樹脂(A1)、ポリイソシアネート化合物(B)、親水化変性カルボジイミド化合物(C)、および水性ノボラック型エポキシ樹脂(D)を含む水性塗料組成物であって;上記水酸基およびカルボキシル基を有する水性樹脂(A1)は、樹脂固形分換算で、80~200mgKOH/gの水酸基価、および、10~40mgKOH/gの酸価を有し;上記水性塗料組成物中に含まれる水性ノボラック型エポキシ樹脂(D)の量は、水性樹脂(A1)、ポリイソシアネート化合物(B)および親水化変性カルボジイミド化合物(C)の樹脂固形分総量100質量部に対して、5~15質量部である;水性塗料組成物を提供する。

    Abstract translation:

    本发明可以形成具有涂膜性能的涂布膜具有优良即使在低温下固化,并提供一种水性涂料组合物。 本发明是具有羟基和羧基的(A1),聚异氰酸酯化合物(B),亲水性改性碳二亚胺化合物(C),和水性涂料组合物包括水性酚醛清漆型环氧树脂(d)的水性树脂 ;羟基和具有羧基的(A1)的水性树脂为树脂固体计,80〜200毫克KOH /克的羟基值,并具有10〜40毫克KOH / g的酸值;所述水性涂料组合物 包含在含水树脂(A1)的水性酚醛清漆型环氧树脂(d)的量,多异氰酸酯化合物(B)和按重量计的亲水性改性碳二亚胺化合物,每100份树脂固体成分(C),5〜 15质量份;提供水性涂料组合物。

    熱交換器用アルミニウムフィン材
    380.
    发明申请
    熱交換器用アルミニウムフィン材 审中-公开
    热交换器铝合金材料

    公开(公告)号:WO2013146388A1

    公开(公告)日:2013-10-03

    申请号:PCT/JP2013/057530

    申请日:2013-03-15

    Abstract:  親水持続性に優れるとともに、湿潤環境下においても良好な密着性を示す熱交換器用アルミニウムフィン材を提供することを課題とする。基板2と、前記基板2の表面に形成され、耐食性皮膜3a、および、疎水性塗膜層3bの少なくとも一層から構成される下地処理層3と、前記下地処理層3の表面に形成され、所定のシリカ系多孔体微粒子4aとカルボキシル基含有高分子4bと水酸基含有高分子4bとの混合物を含む塗膜で構成される親水処理層4と、を備え、前記シリカ系多孔体微粒子4aの付着量が所定量であり、前記カルボキシル基含有高分子4bと前記水酸基含有高分子4bとの合計の固形分重量に対する、前記シリカ系多孔体微粒子4aの固形分重量比率が1.0~3.5であり、前記水酸基含有高分子4bの固形分重量に対する、前記カルボキシル基含有高分子4bの固形分重量比率が0.1~10.0であることを特徴とする。

    Abstract translation: 本发明解决了提供一种具有优异的亲水性耐久性并且在湿润环境中表现出良好粘附性的热交换器的铝翅片材料的问题。 这种用于热交换器的铝翅片材料的特征在于:设置有:基底(2); 在所述基板(2)的表面上形成并由耐腐蚀膜(3a)和疏水性涂膜层(3b)中的至少一种构成的地下处理层(3)。 以及形成在地下处理层(3)的表面上的亲水处理层(4),其由含有规定的二氧化硅多孔微粒(4a),含羧基的聚合物(4b)和 含有羟基的聚合物(4b),其中二氧化硅多孔微粒(4a)的沉积量为规定量,二氧化硅多孔微粒(4a)的固体重量比相对于含羧基的总固体重量 聚合物(4b)和含羟基的聚合物(4b)的比例为1.0〜3.5,含羧基聚合物(4b)相对于含羟基的聚合物(4b)的固体重量比为0.1〜10.0 。