Abstract:
본 발명은 팽윤성과 흡착성이 우수한 이온교환수지에 관한 것이다. 이러한 이온교환수지는 술폰산기를 포함하는 비닐계 단량체와 가교제로서의 폴리에틸렌글리콜디아크렐레이트(PEGDA)를 현탁중합시키는 것을 포함한다. 본 발명에 따라 제조된 이온교환수지는 기공의 형성으로 비표면적이 상승하여 고흡착성의 성질을 가지며, 아크릴기를 함유하고 있어 우수한 팽윤성을 갖는다. 또한, 본 발명에 따라 제조된 이온교환수지는 해수에서 코발트의 흡착에 응용이 가능하다.
Abstract:
PURPOSE: An anion exchange membrane is provided to contain an excellent benzene structure with excellent dimensional stability and to have excellent durability in a redox flow battery. CONSTITUTION: A manufacturing method of an anion exchange membrane comprises 4-vinylbenzyl, styrene, and 2-hydroxyethyl acrylate as a monomer to synthesize a 4-vinylbenzyl chloride-styrene-2-hydroxyethyl acrylate copolymer; a step of aminatng the 4-vinylbenzyl chloride-styrene-2-hydroxyethyl acrylate copolymer; and a step of adding a crosslinking agent to the copolymer and manufacturing the anion exchange membrane by a crosslinking reaction. [Reference numerals] (AA) Hydroxyethyl acrylate(HEA); (BB) Aminated VBC-co-st-co-HEA; (CC) Anion exchange membrane; (DD) Vinylbenzyl chloride(VBC); (EE) Styrene(st); (FF) Glutaric dialdehyde(GA); (GG) Trimethyl amine(TMA)
Abstract:
본 발명은 발효주의 제조장치에 관한 것으로, 보다 상세하게는 두 종류의 전통주를 하나의 용기에서 동시에 제조하는 전통주 제조장치로서, 상기 본 발명에 따른 전통주 제조장치의 이용은 차별성 있는 전통주 용기로 소비자의 기호도에 따라 두 종류 이상의 전통주를 하나의 용기로 판매주점에서 소비자에게 직접 공급할 수 있는 장점이 있어 전통주의 대중화에 기여할 것이다.
Abstract:
본 발명은 강력한 살균력을 가진 강산성수를 필요 시 간단히 제조하여 사용하고자 개발한 것으로 일반적인 격막을 이용한 수도직결식 강전해수(강산성수,강알칼리수) 생성장치와는 상이한 구조로 원통형태의 착탈이 가능한 전해조와 음이온교환수지를 사용하여 장치의 소형화를 확보하였고 강산성수 발생효율을 제고시킨 것을 특징으로 한다. 침적식, 강산성수, 전기분해, 음이온교환수지, 포화소금물
Abstract:
PURPOSE: A manufacturing method of a porous deodorization filter is provided to efficiently remove chemical impurities including a fine dust, ammonia, or amine radical and improve the lifespan of a deodorizing agent by preventing an adhesive from covering the surface of the deodorizing agent. CONSTITUTION: A manufacturing method of a porous deodorization filter comprises next steps. An adhesive solution is infiltrated into a porous scaffold. The infiltrated porous scaffold is dried. The deodorant powder is decentralized into the dried porous scaffold and adhered. The porous scaffold, where the deodorant powder is adhered, is vibrated. After the vibration step, the porous scaffold is dried. The pore size of the porous scaffold is 5~120 ppi. The adhesive solution is coated in the surface of the porous scaffold to the thickness of 0.05~0.4mm.
Abstract:
PURPOSE: A composition for ion exchange liquid for electrode using polystyrene resin or derivates and a manufacturing method of an ion exchange film including the same are provided to reduce manufacturing costs of the ion exchange film and to replace the expensive ion exchange film. CONSTITUTION: A manufacturing method of an ion exchange film for CDI includes the following steps: manufacturing ion exchange liquid; coating the ion exchange liquid on a mesh net; post-processing the coated ion exchange film; and drying the ion exchange film. The ion exchange film adds a positive ion exchange group with mixed acid of sulfuric acid or chlorosulfonic acid / sulfuric acid on polysterene-based resin.